Fermi level limitation in Na1/2Bi1/2TiO3-BaTiO3 piezoceramics by electrochemical reduction of Bi

被引:0
作者
Hu, Pengcheng [1 ]
Huang, Binxiang [1 ]
Bremecker, Daniel [2 ]
Koruza, Jurij [3 ]
Albe, Karsten [4 ]
Klein, Andreas [1 ]
机构
[1] Tech Univ Darmstadt, Inst Mat Sci, Elect Struct Mat, Otto Berndt Str 3, D-64283 Darmstadt, Germany
[2] Tech Univ Darmstadt, Inst Mat Sci, Nonmet Inorgan Mat, Peter Grunberg Str 2, D-64283 Darmstadt, Germany
[3] Graz Univ Technol, Inst Chem & Technol Mat, Stremayrgasse 9, A-8010 Graz, Austria
[4] Tech Univ Darmstadt, Inst Mat Sci, Mat Modelling, Otto Berndt Str 3, D-64283 Darmstadt, Germany
基金
奥地利科学基金会;
关键词
SODIUM BISMUTH TITANATE; LEAD-FREE PIEZOCERAMICS; SITE NONSTOICHIOMETRY; ELECTRICAL-PROPERTIES; OPTICAL-PROPERTIES; BAND-STRUCTURE; THIN-FILMS; HOLE TRAPS; CONDUCTIVITY; PERSPECTIVE;
D O I
10.1063/5.0227698
中图分类号
O59 [应用物理学];
学科分类号
摘要
The (electro)chemical stability of undoped and Zn-doped 0.94Na(1/2)Bi(1/2)TiO(3)-0.06BaTiO(3) lead-free piezoceramics (NBT-6BT) was studied. For this purpose, the Fermi level at the interface between NBT-6BT and Sn-doped In2O3 (ITO) electrode is varied by gradually reducing the ITO film either by annealing in vacuum or by applying a voltage across a Pt/NBT-6BT/ITO. The chemical and electronic changes are monitored in situ by x-ray photoelectron spectroscopy. The experiments reveal the formation of metallic Bi when the Fermi level is reaching a value of 2.23 +/- 0.10 eV above the valence band maximum, while no reduction of Ti is observed. The electrochemical reduction of Bi constitutes an upper limit of the Fermi level at approximate to 1 eV below the conduction band minimum. High electron concentrations in the conduction band and a contribution of free electrons to the electrical conductivity of NBT-6BT can, therefore, be excluded. The reduction occurs for an ITO work function of 4.2-4.3 eV. As typical electrode materials such as Ag, Cu, Ni, or Pt have higher work functions, an electrochemical instability of the electrode interfaces in ceramic capacitors is not expected. Under the given experimental conditions (350 degrees C, electric fields <40 V/mm), no degradation of resistance and no enrichment of Na at the interface are observed.
引用
收藏
页数:10
相关论文
共 50 条
[41]   Thermal stability of the electromechanical properties in acceptor-doped and composite-hardened (Na1/2Bi1/2)TiO3-BaTiO3 ferroelectrics [J].
Slabki, Mihail ;
Venkataraman, Lalitha Kodumudi ;
Rojac, Tadej ;
Roedel, Juergen ;
Koruza, Jurij .
JOURNAL OF APPLIED PHYSICS, 2021, 130 (01)
[42]   A transmission electron microscopy study of the atomic structure of Na1/2Bi1/2TiO3 (NBT) [J].
Zhang, Yingyi ;
Bourgeois, Laure ;
Withers, Ray ;
Etheridge, Joanne .
ACTA CRYSTALLOGRAPHICA A-FOUNDATION AND ADVANCES, 2011, 67 :C718-C718
[43]   Structural and Dielectric Properties of ZrO2 Added (Na1/2Bi1/2)TiO3 Ceramic [J].
Kumari, K. ;
Prasad, K. ;
Yadav, K. L. ;
Sen, S. .
BRAZILIAN JOURNAL OF PHYSICS, 2009, 39 (02) :297-300
[44]   Stress-modulated relaxor-to-ferroelectric transition in lead-free (Na1/2Bi1/2) TiO3-BaTiO3 ferroelectrics [J].
Schader, Florian H. ;
Wang, Zhiyang ;
Hinterstein, Manuel ;
Daniels, John E. ;
Webber, Kyle G. .
PHYSICAL REVIEW B, 2016, 93 (13)
[45]   Synthesis and characterisation of 1-x(Na1/2Bi1/2TiO3)-x(BiFeO3) ceramics [J].
Ramana, EV ;
Saradhi, BVB ;
Suryanarayana, SV ;
Sankaram, TB .
FERROELECTRICS, 2005, 324 :55-61
[46]   Dielectric relaxation and ac conductivity of WO3 added (Na1/2Bi1/2)TiO3 ceramic [J].
Prasad, K. ;
Kumari, K. ;
Chandra, K. P. ;
Yadav, K. L. ;
Sen, S. .
MATERIALS SCIENCE-POLAND, 2009, 27 (02) :373-384
[47]   Identifying phase transition behavior in Bi1/2Na1/2TiO3-BaTiO3 single crystals by piezoresponse force microscopy [J].
Lee, Hyun-Young ;
Wang, Ke ;
Yao, Fang-Zhou ;
Sun, Wei ;
Zhou, Zhen ;
Zhang, Mao-Hua ;
Li, Xiaobing ;
Luo, Haosu ;
Lee, Jae-Shin ;
Li, Jing-Feng .
JOURNAL OF APPLIED PHYSICS, 2017, 121 (17)
[48]   The enhanced piezoelectric performance of Bi1/2Na1/2TiO3-BaTiO3 ceramics by Ba0.77Ca0.23TiO3 substitution [J].
Luo, Laihui ;
Ni, Feng ;
Zhang, Huixin ;
Chen, Hongbing .
JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 536 :113-118
[49]   Preparation and photonic bandgap properties of Na1/2Bi1/2TiO3 inverse opal photonic crystals [J].
Yang, Zhengwen ;
Zhou, Ji ;
Huang, Xueguang ;
Xie, Qin ;
Fu, Ming ;
Li, Bo ;
Li, Longtu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 471 (1-2) :241-243
[50]   Relationship between structure and dielectric property in (1-x)(Na1/2Bi1/2)TiO3-xPbZrO3 ceramics [J].
Lee, JK ;
Yi, JY ;
Hong, KS .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 2001, 40 (10) :6003-6007