Investigation of Basicity on Compressive Strength and Oxidation Induration Mechanism of Vanadium-Titanium Magnetite Pellets

被引:0
|
作者
Zhang, Song [1 ,2 ]
Zong, Yanbing [1 ]
Huang, Yun [3 ]
Gui, Xiangyou [4 ]
Lei, Dian [3 ]
Zhang, Jianliang [1 ,5 ]
Gan, Xian [3 ]
Wang, Zhenyang [1 ]
Zhang, Shushi [1 ]
Lu, Peiyuan [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Bijie Big Data Ind Dev Ctr, Bijie 551700, Guizhou, Peoples R China
[3] Pangang Grp Xichang Steel&Vanadium Co Ltd, Xichang 615032, Sichuan, Peoples R China
[4] Bijie Vocat & Tech Coll, Bijie 551700, Guizhou, Peoples R China
[5] Univ Queensland, Sch Chem Engn, St Lucia, Qld 4072, Australia
基金
中国国家自然科学基金;
关键词
iron and steel industries; oxidation induration; pellets; vanadium-titanium magnetites; HIGH-CHROMIUM VANADIUM; CONSOLIDATION MECHANISM; BEHAVIORS;
D O I
10.1002/srin.202400461
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Currently, the typical charge structure for blast furnace smelting of vanadium-titanium magnetite (VTM) is the addition of acidic pellets, high-basicity sinters, and lumps. To increase the percentage of pellets entering the blast furnace, it is necessary to transfer the basicity burden to the pellets. In this study, the effect of basicity on the phase transition and oxidation hardening mechanism of VTM pellets is investigated. In the results, it is indicated that when the preheating temperature is 950 degrees C, the preheating time is 15 min, the roasting temperature is 1260 degrees C, and the roasting time is 15 min, with the basicity (CaO/SiO2) increasing from 0.08 to 1.3, the compressive strength of pellets shows a trend of "increasing first and then decreasing," with the highest value reaching 3159 N pellet-1 at basicity of 0.5. As the basicity increases, calcium ferrate can be generated by CaO in the liquid phase with Fe2O3 in addition to silicate with SiO2, which will increase the amount of the liquid phase. With the increase of basicity, the oxide-bonded induration is gradually weakened, and the slag-bonded induration is gradually enhanced. A moderate amount of liquid phase can play the role of bonding and filling, thereby improving compressive strength. With the increase of basicity, the content of recrystallized hematite decreases, and the oxide-bonded induration is gradually weakened; while with the larger amount of CaO added, it will generate low-melting-point silicate and calcium ferrate with SiO2 and Fe2O3 and transform into the liquid phase at high temperature, and the slag-bonded induration is gradually enhanced.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:11
相关论文
共 37 条
  • [1] Effect of diboron trioxide on the crushing strength and smelting mechanism of high-chromium vanadium-titanium magnetite pellets
    Cheng, Gong-jin
    Gao, Zi-xian
    Yang, He
    Xue, Xiang-xin
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2017, 24 (11) : 1228 - 1240
  • [2] Influence and Mechanism of CaO on the Oxidation Induration of Hongge Vanadium Titanomagnetite Pellets
    Zeng, Ruiqi
    Li, Wei
    Wang, Nan
    Fu, Guiqin
    Chu, Mansheng
    Zhu, Miaoyong
    ISIJ INTERNATIONAL, 2020, 60 (10) : 2199 - 2205
  • [3] Process mechanism research on direct vortex melting reduction of vanadium-titanium magnetite
    Han, Yong-chao
    Dou, Zhi-he
    Yang, Zhan-ning
    Xie, Wei
    Zhang, Ting-an
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2025, 32 (03) : 536 - 549
  • [4] Effects of basicity and temperature on mineralogy and reduction behaviors of high-chromium vanadium-titanium magnetite sinters
    Tang Wei-dong
    Yang Song-tao
    Zhang Li-heng
    Huang Zhuang
    Yang He
    Xue Xiang-xin
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2019, 26 (01) : 132 - 145
  • [5] Effect of high-pressure grinding rolls pretreatment on the preparation of vanadium-titanium magnetite pellets
    Guo, Yufeng
    Liu, Kuo
    Chen, Feng
    Wang, Shuai
    Yang, Lingzhi
    Li, Dongyue
    Zheng, Yu
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 23 : 2479 - 2490
  • [6] Phase transformation and slag evolution of vanadium-titanium magnetite pellets during softening-melting process
    Hu, Qingqing
    Ma, Donglai
    Zhou, Kai
    Liu, Yongjie
    You, Yang
    You, Zhixiong
    Lv, Xuewei
    POWDER TECHNOLOGY, 2022, 396 : 710 - 717
  • [7] Investigation of the oxidation induration mechanism of Hongge vanadium titanomagnetite pellets with different Al2O3 additions
    Li, Wei
    Fu, Guiqin
    Chu, Mansheng
    Zhu, Miaoyong
    POWDER TECHNOLOGY, 2020, 360 (555-561) : 555 - 561
  • [8] Effect of diboron trioxide on the crushing strength and smelting mechanism of high-chromium vanadium–titanium magnetite pellets
    Gong-jin Cheng
    Zi-xian Gao
    He Yang
    Xiang-xin Xue
    InternationalJournalofMineralsMetallurgyandMaterials, 2017, 24 (11) : 1228 - 1240
  • [9] Effect of diboron trioxide on the crushing strength and smelting mechanism of high-chromium vanadium–titanium magnetite pellets
    Gong-jin Cheng
    Zi-xian Gao
    He Yang
    Xiang-xin Xue
    International Journal of Minerals, Metallurgy, and Materials, 2017, 24 : 1228 - 1240
  • [10] Effect of Cr2O3 addition on the oxidation induration mechanism of Hongge vanadium titanomagnetite pellets
    Li, Wei
    Wang, Nan
    Fu, Gui-qin
    Chu, Man-sheng
    Zhu, Miao-yong
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2018, 25 (04) : 391 - 398