A 3D Nanoscale View of Electrocatalyst Degradation in Hydrogen Fuel Cells

被引:9
作者
Amichi, Lynda [1 ]
Yu, Haoran [1 ]
Ziabari, Amirkoushyar [2 ]
Rahman, Obaidullah [2 ]
Arregui-Mena, David [3 ]
Hu, Leiming [4 ]
Neyerlin, K. C. [4 ]
Cullen, David A. [1 ]
机构
[1] Oak Ridge Natl Lab, Ctr Nanophase Mat Sci, Oak Ridge, TN 37930 USA
[2] Oak Ridge Natl Lab, Electrificat & Energy Infrastruct Div, Oak Ridge, TN 37830 USA
[3] Oak Ridge Natl Lab, Mat Sci & Technol Div, Oak Ridge, TN 37930 USA
[4] Natl Renewable Energy Lab, Chem & Nanosci Ctr, Golden, CO 80401 USA
关键词
carbon pores; ECSA; electron tomography; fuel cell; nanoparticles; NANOPARTICLES; DISTRIBUTIONS; TOMOGRAPHY; TOOL;
D O I
10.1002/aenm.202402310
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The loss of platinum (Pt) electrochemically active surface area (ECSA) is a critical degradation mode that often becomes a limiting factor for heavy-duty proton exchange membrane fuel cell vehicles. High surface area carbon supports have been shown to improve Pt dispersion and limit detrimental ionomer-electrocatalyst interactions due to their large interior pore volume. In this work, using automated scanning transmission electron tomography, the degradation of nanoparticles located on the interior versus exterior surfaces of the carbon support is compared following a catalyst-specific accelerated stress test (AST) of 90,000 voltage cycles between 0.6 V to 0.95 V. The results reveal a notable increase in median particle size for both interior and exterior Pt catalyst particles, with a slightly higher increase in particle size distribution and loss of specific surface area for the particles located on the exterior carbon surface. The fraction of Pt nanoparticles that reside within the interior of the carbon support also increased following the AST test, accompanied by evidence of an increase in average carbon mesopore size. The results shed light on the degradation mechanisms affecting electrochemical properties and the enhanced particle accessibility at lower relative humidity. This study investigates the nanoscale degradation of platinum nanoparticles supported on high surface area carbon. Utilizing electron tomography, the relative distribution of platinum within versus on the carbon support is compared before and after an accelerated stress test. Results show exterior particles degrade more quickly, as well as an increase in average pore size arising from minor carbon corrosion. image
引用
收藏
页数:8
相关论文
共 35 条
[1]  
[Anonymous], Fuel Cell Technologies
[2]  
[Anonymous], ELYST PT50 0550
[3]  
[Anonymous], AVIZO SOFTWARE MAT C
[4]   New roads and challenges for fuel cells in heavy-duty transportation [J].
Cullen, David A. ;
Neyerlin, K. C. ;
Ahluwalia, Rajesh K. ;
Mukundan, Rangachary ;
More, Karren L. ;
Borup, Rodney L. ;
Weber, Adam Z. ;
Myers, Deborah J. ;
Kusoglu, Ahmet .
NATURE ENERGY, 2021, 6 (05) :462-474
[5]  
DEFINITIONS TERMINOLOGY AND SYMBOLS IN COLLOID AND SURF ACE CHEMISTRY, 1976, PURE APPL CHEM, V46, P71
[6]   Electron Tomography: A Three-Dimensional Analytic Tool for Hard and Soft Materials Research [J].
Ercius, Peter ;
Alaidi, Osama ;
Rames, Matthew J. ;
Ren, Gang .
ADVANCED MATERIALS, 2015, 27 (38) :5638-5663
[7]   Instability of Pt/C electrocatalysts in proton exchange membrane fuel cells - A mechanistic investigation [J].
Ferreira, PJ ;
la O', GJ ;
Shao-Horn, Y ;
Morgan, D ;
Makharia, R ;
Kocha, S ;
Gasteiger, HA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (11) :A2256-A2271
[8]  
Girod R. P. A., 2023, MULTIDIMENSIONAL ELE
[9]   Three-dimensional nanoimaging of fuel cell catalyst layers [J].
Girod, Robin ;
Lazaridis, Timon ;
Gasteiger, Hubert A. ;
Tileli, Vasiliki .
NATURE CATALYSIS, 2023, 6 (05) :383-+
[10]   Proton conductors for heavy-duty vehicle fuel cells [J].
Gittleman, Craig S. ;
Jia, Hongfei ;
De Castro, Emory S. ;
Chisholm, Calum R., I ;
Kim, Yu Seung .
JOULE, 2021, 5 (07) :1660-1677