Impact of Surface Pretreatment on the Corrosion Resistance and Adhesion of Thin Film Coating on SS316L Bipolar Plates for Proton-Exchange Membrane Fuel Cell Applications

被引:8
作者
Chellehbari, Yasin Mehdizadeh [1 ]
Gupta, Abhay [1 ]
Li, Xianguo [2 ]
Shahgaldi, Samaneh [1 ]
机构
[1] Univ Quebec Trois Rivieres, Hydrogen Res Inst, Trois Rivieres, PQ G8Z 4M3, Canada
[2] Univ Waterloo, Mech & Mechatron Engn, Waterloo, ON N2L 3G1, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
PEM fuel cell; bipolar plates; stainless steel; pretreatment; thin films; chemical etching; PERFORMANCE; PROTECTION; BEHAVIOR;
D O I
10.3390/molecules29184319
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Coated SS316L is a potential alternative to the graphite bipolar plates (BPPs) used in proton-exchange membrane fuel cells (PEMFCs) owing to their low manufacturing cost and machinability. Due to their susceptibility to corrosion and passivation, which increases PEMFC ohmic resistance, protective and conductive coatings on SS316L have been developed. However, coating adhesion is one of the challenges in the harsh acidic environment of PEMFCs, affecting the performance and durability of BPPs. This study compares mechanical polishing and the frequently adopted chemical etchants for SS316L: Adler's, V2A, and Carpenter's etchant with different etching durations and their impact on the wettability, adhesion, and corrosion resistance of a Nb-coated SS316L substrate. Contact angle measurements and laser microscopy revealed that all etching treatments increased the hydrophobicity and surface roughness of SS316L substrates. Ex situ potentiodynamic and potentiostatic polarization tests and interfacial contact resistance analysis revealed high corrosion resistance, interfacial conductivity, and adhesion of the Nb-coated SS316L substrate pretreated with V2A (7 min) and Adler's (3 min) etchant. Increased hydrophobicity (contact angle = 101 degrees) and surface roughness (Ra = 74 nm) achieved using V2A etchant led to the lowest corrosion rate (3.3 mu A.cm-2) and interfacial resistance (15.4 m Omega.cm2). This study established pretreatment with V2A etchant (a solution of HNO3, HCl, and DI water (1:9:23 mole ratio)) as a promising approach for improving the longevity, electrochemical stability, and efficiency of the coated SS316L BPPs for PEMFC application.
引用
收藏
页数:12
相关论文
共 50 条
[31]   Molybdenum carbide coated 316L stainless steel for bipolar plates of proton exchange membrane fuel cells [J].
Wang, Lun ;
Tao, Youkun ;
Zhang, Zhen ;
Wang, Yajun ;
Feng, Qi ;
Wang, Haijiang ;
Li, Hui .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (10) :4940-4950
[32]   Corrosion Resistance and Conductivity of Ta-Nb-N-Coated 316L Stainless Steel as Bipolar Plates for Proton Exchange Membrane Fuel Cells [J].
Li, Qizhong ;
Ding, Chuan ;
Yang, Mai ;
Yang, Meijun ;
Gao, Tenghua ;
Zhang, Song ;
Ji, Baifeng ;
Goto, Takashi ;
Tu, Rong .
COATINGS, 2024, 14 (05)
[33]   Multilayered Zr-C/a-C film on stainless steel 316L as bipolar plates for proton exchange membrane fuel cells [J].
Bi, Feifei ;
Peng, Linfa ;
Yi, Peiyun ;
Lai, Xinmin .
JOURNAL OF POWER SOURCES, 2016, 314 :58-65
[34]   Corrosion Resistance and Surface Conductivity of 446 Stainless Steel with Electrochemical Cr-Enrichment and Nitridation for Proton Exchange Membrane Fuel Cell (PEMFC) Bipolar Plates [J].
Xu, Ronghai ;
Zhu, Yangyue ;
Zhu, Ruigang ;
Li, Moucheng .
METALS, 2025, 15 (05)
[35]   Corrosion and interfacial contact resistance of 316L stainless steel coated with magnetron sputtered ZrN and TiN in the simulated cathodic environment of a proton-exchange membrane fuel cell [J].
Yi, Pan ;
Zhu, Lijie ;
Dong, Chaofang ;
Xiao, Kui .
SURFACE & COATINGS TECHNOLOGY, 2019, 363 :198-202
[36]   Effect of bipolar-plates design on corrosion, mass and heat transfer in proton-exchange membrane fuel cells and water electrolyzers: A review [J].
Zhang, Jiuhong ;
Luo, Xiejing ;
Ding, Yingyu ;
Chang, Luqi ;
Dong, Chaofang .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2024, 31 (07) :1599-1616
[37]   TiZrC-coated 316 L stainless steel bipolar plates for proton exchange membrane fuel cells [J].
Ma, Tiancai ;
Guo, Huijin ;
Tian, Yan ;
Qi, Jinxuan ;
Yao, Naiyuan .
MATERIALS TODAY COMMUNICATIONS, 2025, 42
[38]   Carbon coating for corrosion protection of SS-316L and AA-6061 as bipolar plates of PEM fuel cells [J].
Sisan, M. Mirzaee ;
Sereshki, M. Abdolahi ;
Khorsand, H. ;
Siadati, M. H. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 613 :288-291
[39]   Mechanical properties, corrosion resistance, and rubber pad forming of cold differential speed-rolled pure titanium for bipolar plates of proton-exchange membrane fuel cells [J].
Liu, Qian ;
Wang, Xiubin ;
Yin, Deliang ;
Zhang, Xinping .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (40) :17737-17748
[40]   A review of bipolar plates materials and graphene coating degradation mechanism in proton exchange membrane fuel cell [J].
Okonkwo, Paul C. ;
Emori, Wilfred ;
Uzoma, Paul C. ;
Mansir, Ibrahim B. ;
Radwan, Ahmed Bahgat ;
Ige, Oladeji O. ;
Abdullah, Aboubakr M. .
INTERNATIONAL JOURNAL OF ENERGY RESEARCH, 2022, 46 (04) :3766-3781