Structure, mechanical, and tribological properties of Ag2CrO4 high-temperature oxide coatings

被引:0
|
作者
Zeng, Zhong [1 ,6 ]
Zhang, Lei [1 ,6 ]
Pelenovich, Vasiliy [2 ,3 ,6 ]
Wan, Qiang [4 ,6 ]
Zhan, Xinggang [5 ,6 ]
Xu, Tao [5 ,6 ]
Hu, Longwei [5 ,6 ]
Liu, Yan [6 ,7 ]
Li, Zhenggang [1 ,6 ]
Yang, Bing [1 ,6 ]
Chen, Yanming [1 ,6 ]
机构
[1] Wuhan Univ, Sch Power & Mech Engn, Wuhan 430072, Peoples R China
[2] Wuhan Univ, Inst Technol Sci, Wuhan 430072, Peoples R China
[3] Wuhan Univ, Hubei Key Lab Elect Mfg & Packaging Integrat, Wuhan 430072, Peoples R China
[4] Huazhong Agr Univ, Coll Engn, Wuhan 430072, Peoples R China
[5] Guizhou Aerosp Precis Prod Co Ltd Guizhou, Zunyi 563099, Peoples R China
[6] Aerosp Precis Prod Inc Ltd, Tianjin 300000, Peoples R China
[7] Hubei JiuFengShan Future Sci & Technol Lab, Wuhan 420000, Peoples R China
基金
中国国家自然科学基金;
关键词
High temperature self-lubrication; Silver chromate; Coating; Oxygen flow ratio; Mechanical properties; Tribological properties; LUBRICATING PROPERTIES; COMPOSITES; BEHAVIOR; AG;
D O I
10.1016/j.tsf.2024.140533
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, a series of Ag2CrO4 high-temperature self-lubricating oxide coatings were prepared by reactive radio frequency magnetron sputtering under different argon-oxygen flow ratio (Ar:O-2 ratio) conditions. Effects of the gas flow ratio on phase composition, coating morphology, high temperature treatment in air atmosphere, mechanical and tribological properties are studied. A low Ar:O-2 flow ratio is beneficial for the formation of Ag2CrO4 phase. At high temperature treatment, formation of surface Ag particle and volatility and decomposition of the Ag2CrO4 phase are observed, and the volatility and decomposition of the coating are slight at temperatures below 500 degrees C. When the Ar:O-2 ratio is 1:1, the coating shows exceptional comprehensive performance, it is dense with a smooth surface, excellent toughness and bond strength, and the lowest wear rate and coefficient of friction, which is 0.14 mm(3)/10(-3)N center dot m and 0.35 respectively. The coating can function as a lubricant in temperature environments of 500 degree celsius and below, demonstrating practical application value.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] Fabrication of new Ag2CrO4/Ag2MoO4 and Ag2CrO4/Ag2WO4 heterostructures with enhanced degradation of the mixture of dyes by photocatalysis
    Silva, J. M. P.
    Neto, N. F. Andrade
    Teodoro, M. D.
    Paiva, A. E. M.
    Bomio, M. R. D.
    Motta, F. V.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 928
  • [2] Ag2CrO4 nanostructures: Characterization and catalytic properties
    Shanthi, B.
    Saravanan, K.
    Ravichandran, C.
    Venkatachalapathy, B.
    Sathiyanarayanan, K.
    Karthikeyan, N. S.
    Suresh, R.
    MATERIALS LETTERS, 2023, 351
  • [3] Preparation and high-temperature tribological properties of CrAlVYN-Ag nanocomposite coatings
    Fu, Yingying
    Li, Hongxuan
    Ji, Li
    Liu, Xiaohong
    He, Nairu
    Zhou, Huidi
    Chen, Jianmin
    MATERIALS AND MANUFACTURING PROCESSES, 2017, 32 (04) : 409 - 415
  • [4] High-temperature tribological properties of CrAlN, CrAlSiN and AlCrSiN coatings
    Polcar, Tomas
    Cavaleiro, Albano
    SURFACE & COATINGS TECHNOLOGY, 2011, 206 (06): : 1244 - 1251
  • [5] Ag2CrO4 for photocatalytic applications: High performance of crystals designed by autogenous pressure
    Miclau, Marinela
    Kumar, Sanjay
    Ursu, Daniel
    Orha, Corina
    Miclau, Nicolae
    Rueff, Jean-Michel
    Malo, Sylvie
    Martin, Christine
    MATERIALS CHARACTERIZATION, 2019, 158
  • [6] MXene/Ag2CrO4 Nanocomposite as Supercapacitors Electrode
    Yaqoob, Tahira
    Rani, Malika
    Mahmood, Arshad
    Shafique, Rubia
    Khan, Safia
    Janjua, Naveed Kausar
    Shah, Aqeel Ahmad
    Ahmad, Awais
    Al-Kahtani, Abdullah A.
    MATERIALS, 2021, 14 (20)
  • [7] Microstructure, mechanical and high-temperature tribological properties of MoS2-Cr-Ag composite films
    Chen, Yanjun
    Sun, Jianfang
    Liu, Yong
    Li, Qiang
    Xiao, Shu
    Su, Fenghua
    SURFACE & COATINGS TECHNOLOGY, 2023, 452
  • [8] CrN-Ag nanocomposite coatings: High-temperature tribological response
    Mulligan, C. P.
    Blanchet, T. A.
    Gall, D.
    WEAR, 2010, 269 (1-2) : 125 - 131
  • [9] Microstructure, mechanical properties and tribological properties of NiCrAlY-Ag-SrF2 self-lubricating coatings by detonation spraying
    Liu, Jiangxia
    Chen, Wenyuan
    Chen, Juanjuan
    Tan, Hui
    Cheng, Jun
    Zhu, Shengyu
    Yang, Jun
    TRIBOLOGY INTERNATIONAL, 2024, 199
  • [10] Thermostability, oxidation, and high-temperature tribological properties of nano-multilayered AlCrSiN/VN coatings
    Wang, Rui
    Li, Hai Qing
    Li, Ren Suo
    Mei, Hai Juan
    Zou, Chag Wei
    Zhang, Teng Fei
    Wang, Qi Min
    Kim, Kwang Ho
    CERAMICS INTERNATIONAL, 2022, 48 (09) : 11915 - 11923