Effect of PA12 powder recycling on properties of SLS 3D printed parts including their hygroscopicity

被引:2
|
作者
Machotova, Jana [1 ]
Pagac, Marek [2 ]
Svoboda, Roman [3 ]
Jansa, Jan [2 ]
Podzimek, Stepan [1 ]
Cernoskova, Eva [4 ]
Palarcik, Jiri [5 ]
Koutova, Zuzana [6 ]
Kutalekg, Petr [7 ]
Zarybnicka, Lucie [8 ,9 ]
机构
[1] Univ Pardubice, Inst Chem & Technol Macromol Mat, Fac Chem Technol, Studentska 573, Pardubice 53210, Czech Republic
[2] VSB TU Ostrava, Fac Mech Engn, Dept Machining Assembly & Engn Technol, 17,Listopadu 2172-15, Ostrava 70800, Czech Republic
[3] Univ Pardubice, Fac Chem Technol, Dept Phys Chem, Studentska 573, Pardubice 53210, Czech Republic
[4] Univ Pardubice, Fac Chem Technol, Dept Gen & Inorgan Chem, Studentska 573, Pardubice 53210, Czech Republic
[5] Univ Pardubice, Inst Environm & Chem Engn, Fac Chem Technol, Studentska 573, Pardubice 53210, Czech Republic
[6] MemBrain Sro, Pod Vinici 87, Strazpod Ralskem 47127, Czech Republic
[7] Ctr Mat & Nanotechnol, Fac Chem Technol, Cs Legii 565, Pardubice 53002, Czech Republic
[8] Coll Polytech Jihlava, Dept Tech Studies, Tolsteho 16, Jihlava 58601, Czech Republic
[9] Czech Acad Sci, Inst Theoret & Appl Mechan, Ctr Telc, Prosecka 809-76, Prague 9, Czech Republic
关键词
Selective laser sintering; Print orientation; Polyamide; 12; Recycling; Hygroscopicity; MECHANICAL-PROPERTIES; LASER; BEHAVIOR; MICROSTRUCTURE; COALESCENCE; PERFORMANCE; COMPOSITES; PARAMETERS; MORPHOLOGY; WATER;
D O I
10.1016/j.eurpolymj.2024.113432
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The ageing and recycling of polyamide 12 (PA12) powder are key issues in selective laser sintering (SLS) processing, while hygroscopicity is an important defect of PA12 products during use. This paper aims to correlate PA12 powder recycling with changes in the hygroscopicity of printed parts, which is significant for a comprehensive understanding of the impact of ageing on the performance of PA12 parts. PA12 powder was utilized in different grades: virgin, post-industrial recycled, and virgin-post-industrial recycled mixture (virgin-to-post-industrial recycled powder weight ratio of 25/75). The mutual effects of the powder grade, print orientation used in the building process, and absorbed moisture on the properties of printed parts were evaluated. Molar mass increase and secondary crystallization have been demonstrated in the post-industrial recycled powder, being responsible for the worse sintering quality in the SLS process. Therefore, the printed parts made from the postindustrial recycled powder or the virgin-post-industrial recycled powder mixture exhibited worse mechanical strength, a higher porosity, and hence a higher level of hygroscopicity in terms of moisture absorption and wettability. On the contrary, the printed parts made from the virgin powder were found to be more moisture- sensitive in terms of the decline in mechanical strength in the wet state because of the higher content of the amorphous phase holding the plasticizing water.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] An investigation on mechanical properties of PA12 parts produced by a SLS 3D printer: An experimental approach
    Razaviye, Milad Khademe
    Tafti, Roohollah Azizi
    Khajehmohammadi, Mehran
    CIRP JOURNAL OF MANUFACTURING SCIENCE AND TECHNOLOGY, 2022, 38 : 760 - 768
  • [2] Effect of PA12 powder reuse on coalescence behaviour and microstructure of SLS parts
    Dadbakhsh, Sasan
    Verbelen, Leander
    Verkinderen, Olivier
    Strobbe, Dieter
    Van Puyvelde, Peter
    Kruth, Jean-Pierre
    EUROPEAN POLYMER JOURNAL, 2017, 92 : 250 - 262
  • [3] Optimizing the mechanical properties of TiO2/PA12 nano-composites fabricated by SLS 3D printing
    Afshari, Mahmoud
    Bakhshi, Soroush
    Samadi, Mohammad Reza
    Afshari, Hossein
    POLYMER ENGINEERING AND SCIENCE, 2023, 63 (01): : 267 - 280
  • [4] Multi-functional polyamide 12 (PA12)/multiwall carbon nanotube 3D printed nanocomposites with enhanced mechanical and electrical properties
    Vidakis, Nectarios
    Petousis, Markos
    Velidakis, Emmanouil
    Tzounis, Lazaros
    Mountakis, Nikolaos
    Boura, Orsa
    Grammatikos, Sotirios A.
    ADVANCED COMPOSITE MATERIALS, 2022, 31 (06) : 630 - 654
  • [5] Failure analysis of 3D printed glass fiber/PA12 composite lattice structures using DIC
    Hao, Wenfeng
    Liu, Ye
    Wang, Tao
    Gun, Guangping
    Chen, Haosen
    Fang, Daining
    COMPOSITE STRUCTURES, 2019, 225
  • [6] Mechanical and Tribological Properties of 3D Printed Polyamide 12 and SiC/PA12 Composite by Selective Laser Sintering
    Yu, Guoyan
    Ma, Jingdong
    Li, Jun
    Wu, Jingquan
    Yu, Jiang
    Wang, Xianzhang
    POLYMERS, 2022, 14 (11)
  • [7] Investigation of the effect of FDM process parameters on mechanical properties of 3D printed PA12 samples using Taguchi method
    Kam, Menderes
    Ipekci, Ahmet
    Sengul, Omer
    JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 2023, 36 (01) : 307 - 325
  • [8] Mechanical performance of non-reinforced, carbon fiber reinforced and glass bubbles reinforced 3D printed PA12 polyamide
    Pejkowski, Lukasz
    Seyda, Jan
    Nowicki, Krzysztof
    Mrozik, Dariusz
    POLYMER TESTING, 2023, 118
  • [9] Effect of build orientation on the green tribological properties of multi-jet fusion manufactured PA12 parts
    Gavcar, Beyza
    Sumer, Emir Halit
    Sagbas, Binnur
    Katiyar, Jitendra Kumar
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2023, 237 (12) : 2213 - 2223
  • [10] Chess-like Pieces Realized by Selective Laser Sintering of PA12 Powder: 3D Printing and Micro-Tomographic Assessment
    Colucci, Giovanna
    Fontana, Luca
    Barberi, Jacopo
    Brovarone, Chiara Vitale
    Messori, Massimo
    POLYMERS, 2024, 16 (24)