Degradation of the protective layer on stainless steel by chlorine variation under high-temperature conditions

被引:2
|
作者
Karuana, Feri [1 ,2 ]
Prismantoko, Adi [1 ,2 ]
Jatisukamto, Gaguk [3 ]
Tambunan, Barman [2 ,4 ]
Suhendra, Nandang [2 ]
Syahril, Muhammad [2 ]
Rahayu, Sri [2 ]
Darmawan, Arif [2 ]
Darmadi, Djarot B. [5 ]
Aziz, Muhammad [6 ]
Muflikhun, Muhammad Akhsin [1 ]
Hariana, Hariana [2 ]
机构
[1] Gadjah Mada Univ, Dept Mech & Ind Engn, Yogyakarta 55281, Indonesia
[2] Natl Res & Innovat Agcy, South Tangerang 15314, Indonesia
[3] Jember Univ, Fac Engn, Dept Mech Engn, Jember 68121, Indonesia
[4] Deakin Univ, Melbourne, Vic, Australia
[5] Brawijaya Univ, Dept Mech Engn, Malang, Indonesia
[6] Univ Tokyo, Inst Ind Sci, Tokyo 1538505, Japan
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 40卷
关键词
Chromium; Chlorine; Corrosion; Stainless steel; Oxide layer; ZHUNDONG COAL; CORROSION; ASH; BEHAVIOR; SCALE; COMBUSTION; FIRESIDE; BIOMASS;
D O I
10.1016/j.mtcomm.2024.109981
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigates the impact of various chlorine (Cl) content ratios on the degradation of 304 stainless steel during co-combustion of coal with solid recovered fuel (SRF) at a combustion temperature of 1250 degrees C. The research specifically focuses on the corrosion potential at 550 degrees C, which represents the temperature in the superheater area of a power plant. High-temperature corrosion experiments are conducted in a laboratory-scale drop tube furnace to observe initial corrosion during combustion. Analyses include visual examination, mineral analysis, microstructure-based metal analysis, and corrosion rate determination. The results show significant degradation at Cl contents higher than 0.09 wt%. The usual carbide formation at the grain boundaries in 304 stainless-steel does not occur in the short-term tests, as indicated by Cr content remaining above 12 % and Cl content less than 0.06 wt%. In addition, material degradation is due to the Cl reacting with alkali content, damaging the oxide layer and causing pits in the cross-section area of the probe material. This research provides insights into the critical role of Cl in metal degradation and identifies the optimum Cl amount suitable for coal blending in power plants.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] STAINLESS-STEEL FIBERS IN HIGH-TEMPERATURE SUPERCONDUCTOR COMPOSITE
    VIPULANANDAN, C
    SALIB, S
    MATERIALS RESEARCH BULLETIN, 1991, 26 (09) : 951 - 958
  • [22] HIGH-TEMPERATURE TRANSGRANULAR FRACTURE IN AN AUSTENITIC STAINLESS-STEEL
    HASEGAWA, T
    ILSCHNER, B
    SCRIPTA METALLURGICA, 1983, 17 (04): : 523 - 527
  • [23] TRANSFORMATION AND HIGH-TEMPERATURE DEFORMATION OF DUPLEX STAINLESS-STEEL
    KAGAMI, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1395 - 1395
  • [24] Effect of Nb on high-temperature properties for ferritic stainless steel
    Nippon Steel Corp, Futtsu, Japan
    Scripta Mater, 6 (705-710):
  • [25] OXIDATION OF STAINLESS-STEEL TUBINGS IN HIGH-TEMPERATURE STEAM
    KINOSHITA, K
    MIMINO, T
    SHIBATA, M
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1975, 15 (06) : 334 - 340
  • [26] Effect of Nb on high-temperature properties for ferritic stainless steel
    Fujita, N
    Ohmura, K
    Kikuchi, M
    Suzuki, T
    Funaki, S
    Hiroshige, I
    SCRIPTA MATERIALIA, 1996, 35 (06) : 705 - 710
  • [27] High-temperature stress and strain partitioning in duplex stainless steel
    Duprez, L
    De Cooman, BC
    Akdut, N
    ZEITSCHRIFT FUR METALLKUNDE, 2002, 93 (03): : 236 - 243
  • [28] HIGH-TEMPERATURE EMBRITTLEMENT OF STAINLESS STEEL IRRADIATED IN FAST FLUXES
    FRASER, AS
    BIRSS, IR
    CAWTHORN.C
    NATURE, 1966, 211 (5046) : 291 - &
  • [29] High-temperature oxidation resistance in yttrium implanted stainless steel
    Barlak, Marek
    Piekoszewski, Jerzy
    Werner, Zbigniew
    Sartowska, Bozena
    Walis, Lech
    Starosta, Wojciech
    Kierzek, Joachim
    Kowalska, Ewa
    Wilhelm, Richard A.
    Pochrybniak, Cezary
    Woznica, Magdalena
    NUKLEONIKA, 2012, 57 (04) : 473 - 476
  • [30] DEVELOPMENT OF HIGH-TEMPERATURE STAINLESS STEEL SOLID LUBRICANT COMPOSITES
    AMATO, I
    MARTINEN.P
    ASLE TRANSACTIONS, 1974, 17 (03): : 201 - 205