Corrosion behavior of Ni-W coatings with and without macroscopic defects under different corrosion conditions

被引:2
|
作者
Li, Wenzhe [1 ,2 ]
Luo, Wei [1 ,2 ]
Wang, Du [1 ,2 ]
Wang, Chuanlei [1 ,2 ]
Liu, Yanming [3 ]
Wen, Lei [4 ]
机构
[1] PetroChina Southwest Oil & Gas Field Co, Engn Technol Res Inst, Chengdu 610017, Peoples R China
[2] PetroChina Southwest Oil & Gas Field Co, Well Integr Management Ctr, Chengdu 610017, Peoples R China
[3] Xian Shiyou Univ, Coll Mat Sci & Engn, Xian 710065, Peoples R China
[4] Univ Sci & Technol Beijing, Natl Ctr Mat Serv Safety, Beijing 100083, Peoples R China
来源
INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE | 2024年 / 19卷 / 07期
关键词
Ni-W coatings; Macroscopic defects; Live acid; Spent acid; Formation water; High- temperature CO2&H2S environment; STAINLESS-STEEL; HIGH-TEMPERATURE; CARBON-STEEL; IRON; CO2; PASSIVITY; OXIDE; H2S;
D O I
10.1016/j.ijoes.2024.100613
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
High pressure and high temperature corrosion performance of Ni-W coatings with and without macroscopic defects were investigated successively in live acid at 100 degree celsius, spent acid and formation water containing CO2&H2S at 160 degree celsius by using weight loss method, surface characterization and high temperature and high pressure electrochemical test. Additionally, the corrosion performance of C110 steels was comparatively studied. The results show that compared with C110 steels, Ni-W coatings have better resistance to each harsh corrosive environment with lower uniform corrosion rate, pit depth and decreased corrosion current density. The corrosion rate of Ni-W coatings in both live acid and spent acid are acceptable for oilfields, and its corrosion rate (0.0978 mm/y) in formation water is categorized as moderate-degree corrosion. The corrosion scale consisting of NiS, Ni3S2 or Ni3S4 and a small amount of Ni(OH)(2) is stable, compact and closely combined with the substrate, thus effectively slowing down the corrosion rate of Ni-W coatings during long-term immersion. However, the preferential dissolution of Ni causes a W-rich layer on the top layer of Ni-W coating, probably forming WO2, which tends to crack and aggravates the coating degradation. For Ni-W coatings with artificial defects, the galvanic effect and the catalytic role of Cl- synergistically accelerate the corrosion of the C110 substrate at the defect, and its pit depth is over 100 mu m after being corroded in formation water. Notably, the corrosion of the C110 substrate extends laterally and deeply along the coating/substrate interface, promoting the local corrosion disbonding of the coating. Therefore, macroscopic defects in Ni-W coatings should be avoided in their practical application.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Pulse electrodeposition and corrosion behavior of Ni-W/MWCNT nanocomposite coatings
    Li, Han
    He, Yi
    Fan, Yi
    Xu, Wei
    Yang, Qiangbin
    RSC ADVANCES, 2015, 5 (84): : 68890 - 68899
  • [2] Electrodeposition of laminar coatings of Ni-W alloy and their corrosion behaviour
    Elias, Liju
    Hegde, A. Chitharanjan
    SURFACE & COATINGS TECHNOLOGY, 2015, 283 : 61 - 69
  • [3] Corrosion behavior of Ni-W alloy in NaCl solution
    Yao, Ying-Wu
    Yao, Su-Wei
    Song, Zhen-Xing
    Cailiao Gongcheng/Journal of Materials Engineering, 2006, (09): : 42 - 44
  • [4] Effect of SiC on Corrosion and Wear Resistance of Ni-W Coatings
    Li Baosong
    Zhang Wen
    Huan Yuxing
    Zhang Weiwei
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (10) : 3129 - 3134
  • [5] Corrosion behaviour of compositionally modulated nanocrystalline Ni-W coatings
    Wasekar, Nitin P.
    Gowthami, S.
    Jyothirmayi, A.
    Joardar, J.
    Sundararajan, G.
    SURFACE ENGINEERING, 2020, 36 (09) : 952 - 959
  • [6] Investigation of corrosion resistance of electrodeposited Ni-W/SiC composite coatings
    Hosseini, M. G.
    Abdolmaleki, M.
    Ghahremani, J.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2014, 49 (04) : 247 - 253
  • [7] Corrosion Resistance of Heat-Treated Ni-W Alloy Coatings
    Popczyk, Magdalena
    Kubisztal, Julian
    Swinarew, Andrzej Szymon
    Waskiewicz, Zbigniew
    Stanula, Arkadiusz
    Knechtle, Beat
    MATERIALS, 2020, 13 (05)
  • [8] Effect of Amorphous Boron on the Microstructure and Corrosion Properties of Ni-W Coatings
    Kiatwisarnkij, Napat
    Mahattanatawee, Suchet
    Lothongkum, Gobboon
    Qin, Jiaqian
    COATINGS, 2023, 13 (02)
  • [9] Effect of heat treatment on the corrosion resistance of electrolytic Ni-W coatings
    Losiewicz, Bozena
    Popczyk, Magdalena
    OCHRONA PRZED KOROZJA, 2012, 55 (03): : 128 - +
  • [10] Pulse current electrodeposition and corrosion properties of Ni-W alloy coatings
    Zemanova, M.
    Krivosudska, M.
    Chovancova, M.
    Jorik, V.
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2011, 41 (09) : 1077 - 1085