Plastic Deformation Behavior of Ti5Si3 Single Crystals

被引:0
作者
Kishida, Kyosuke [1 ]
Fujiwara, Masakazu [1 ]
Okamoto, Norihiko L. [1 ]
Tanaka, Katsushi [1 ]
Inui, Haruyuki [1 ]
机构
[1] Kyoto Univ, Dept Mat Sci & Engn, Sakyo Ku, Kyoto 6068501, Japan
来源
ADVANCED INTERMETALLIC-BASED ALLOYS FOR EXTREME ENVIRONMENT AND ENERGY APPLICATIONS | 2009年 / 1128卷
关键词
TIAL ALLOYS; MICROSTRUCTURE; COMPOSITE;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Deformation behavior of binary stoichiometric Ti(5)Si(3) single crystals was examined as a function of the loading axis orientation and temperature. Two different types of deformation modes, namely {1100}[0001] prism slip, {2112}1/3 < 2113 > pyramidal slip were newly identified to be activated above 1300 C depending on the loading axis orientation. Critical resolved shear stresses (CRSS) for the {1100} [0001] prism slip and {2112}1/3 < 2113 > pyramidal slip were estimated to be about 130 MPa and 330 MPa at 1400 degrees C, respectively. The values of the CRSS for these two slip systems decrease monotonously with increasing the temperature.
引用
收藏
页码:537 / 542
页数:6
相关论文
共 11 条
[1]  
Alexander H., 1968, SOLID STATE PHYS, V22, P28
[2]  
FROMMEYER G, 1990, Z METALLKD, V81, P307
[3]   Plastic deformation of single crystals of TiSi2 with the C54 structure [J].
Inui, H ;
Moriwaki, M ;
Okamoto, N ;
Yamaguchi, M .
ACTA MATERIALIA, 2003, 51 (05) :1409-1420
[4]  
Inui H, 1998, PHILOS MAG A, V77, P375, DOI 10.1080/01418619808223759
[5]   Formation of a TiN/Ti5Si3 nano-grain composite by a non-equilibrium PM process [J].
Suehiro, Y ;
Ameyama, K .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 111 (1-3) :118-121
[6]   Solidification behavior of Ti5Si3 whiskers in TiAl alloys [J].
Sun, FS ;
Froes, FH .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 345 (1-2) :262-269
[7]   Ti5Si3 whisker in-situ reinforced TiAl alloys [J].
Sun, FS ;
Cao, CX ;
Kim, SE ;
Lee, YT ;
Yan, MG .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (05) :1233-1244
[8]   HIGH-TEMPERATURE DEFORMATION OF TI5SI3 SINGLE-CRYSTALS WITH D8(8) STRUCTURE [J].
UMAKOSHI, Y ;
NAKASHIMA, T .
SCRIPTA METALLURGICA ET MATERIALIA, 1994, 30 (11) :1431-1436
[9]   Unidirectional crystallization and high-temperature oxidation of in situ Ti3(Al,Si)-Ti5(Si,Al)3 composite [J].
Vojtech, D. ;
Novak, M. ;
Novak, P. ;
Lejcek, P. ;
Kopecek, J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 489 (1-2) :1-10
[10]   THE TI3(AL,SI) + TI5(SI,AL)3 EUTECTIC REACTION IN THE TI-AL-SI SYSTEM [J].
WU, JS ;
BEAVEN, PA ;
WAGNER, R .
SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (01) :207-212