Improving High-Temperature Wear Resistance of Ti-6Al-4V alloy via Si-B-Y Co-Deposited Coatings

被引:0
|
作者
Li, Xuan [1 ]
Zhang, Xu-yi [1 ]
Liu, Zhi-zhang [1 ]
Zhang, Li-jing [2 ]
Luo, Lei [1 ]
Lai, Sheng [1 ]
机构
[1] Sichuan Univ Sci & Engn, Coll Mech Engn, Zigong 643000, Peoples R China
[2] Xian Chang Feng Electromech Res Inst, Xian 710065, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-6Al-4V alloy; Si-B-Y co-deposition; Coating structure; High temperature; Friction and wear; Wear mechanisms; CODEPOSITION COATINGS; MECHANICAL-PROPERTIES; TI6AL4V ALLOY; BEHAVIOR; MICROSTRUCTURES; IMPROVEMENT; TITANIUM; AL;
D O I
10.1007/s12540-024-01787-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Si-deposited and Si-B-Y co-deposited coatings were prepared on the Ti-6Al-4V alloy using the pack cementation technique. The microstructures of the coatings, as well as their high-temperature wear performance and mechanisms, were comparatively investigated. The results illustrated that the Si-B-Y co-deposited coating had a similar structure with the Si-deposited coating, both of them possessed three-layer structures: an outer layer of TiSi2 matrix, a middle layer of TiSi, and an inner layer of Ti5Si4 and Ti5Si3 mixtures. However, numerous TiB2 and Y2O3 phases formed in the superficial zones of the Si-B-Y co-deposited coating. The micro-hardness of the Si-deposited and Si-B-Y co-deposited coatings was significantly higher than that of the Ti-6Al-4V substrate, and displayed a gradual decrease tendency from the coating surface to the interior. Compared to the Si-deposited coating, the Si-B-Y co-deposited coating possessed a more compact structure and higher surface hardness, and offered better anti-wear performance for the Ti-6Al-4V substrate at 600 degree celsius. Worn against the GCr15 ball, the average friction coefficient of the Si-B-Y co-deposited coating (similar to 0.449) were near equal to that of the Si-deposited coating (similar to 0.474), but lower than that of the Ti-6Al-4V substrate (similar to 0.685). The wear rate of the Si-B-Y co-deposited coating was approximately 4.1 x 10(-5) mm(3)/N center dot m, lower than that of the Ti-6Al-4V substrate by about 74.6%, and the Si-deposited coating by about 37.3%, respectively. When worn against the Al2O3 ball, the average friction coefficient of the Si-B-Y co-deposited coating (similar to 0.742) was lower than that of the Si-deposited coating (similar to 0.811), but higher than that of the Ti-6Al-4V substrate (similar to 0.551). The wear rate of the coating was approximately 1.22 x 10(-4) mm(3)/N center dot m, lower than that of the Ti-6Al-4V substrate by about 72.2%, and the Si-deposited coating by about 35%.
引用
收藏
页码:1009 / 1024
页数:16
相关论文
共 50 条
  • [1] Wear Resistance and Morphological Characterization of High power Laser Clad Coatings on Ti-6Al-4V Alloy
    Phala, M. F.
    Popoola, A. P., I
    2ND INTERNATIONAL CONFERENCE ON SUSTAINABLE MATERIALS PROCESSING AND MANUFACTURING (SMPM 2019), 2019, 35 : 769 - 774
  • [2] Improving corrosion resistance of Ti-6Al-4V alloy through plasma-assisted PVD deposited nitride coatings
    Oliveira, V. M. C. A.
    Aguiar, C.
    Vazquez, A. M.
    Robin, A.
    Barboza, M. J. R.
    CORROSION SCIENCE, 2014, 88 : 317 - 327
  • [3] Hybrid high-temperature wear mechanisms of additive manufactured Ti-6Al-4V alloy
    Xu, Ruiwen
    Zhu, Yi
    Wu, Jianxiong
    Huang, Pengfei
    Wu, Ming
    Wang, Wujun
    Zhang, Chao
    Yang, Huayong
    TRIBOLOGY INTERNATIONAL, 2025, 205
  • [4] Improvement in the high-temperature creep properties via heat treatment of Ti-6Al-4V alloy manufactured by selective laser melting
    Kim, Young-Kyun
    Park, Soon-Hong
    Yu, Ji-Hun
    AlMangour, Bandar
    Lee, Kee-Ahn
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 715 : 33 - 40
  • [5] Wear and Corrosion Resistance of Thick Ti-6Al-4V Coating Deposited on Ti-6Al-4V Substrate via High-Pressure Cold Spray
    Khun, N. W.
    Tan, A. W. Y.
    Sun, W.
    Liu, E.
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2017, 26 (06) : 1393 - 1407
  • [6] Wear and Corrosion Resistance of ZrN Coatings Deposited on Ti6Al4V Alloy for Biomedical Applications
    Rabadzhiyska, Stanislava
    Dechev, Dimitar
    Ivanov, Nikolay
    Ivanova, Tatyana
    Strijkova, Velichka
    Katrova, Vesela
    Rupetsov, Velko
    Dimcheva, Nina
    Valkov, Stefan
    COATINGS, 2024, 14 (11)
  • [7] Improving the wear resistance of Ti-6Al-4V/TiC composites through thermal oxidation (TO)
    Dalili, N.
    Edrisy, A.
    Farokhzadeh, K.
    Li, J.
    Lo, J.
    Riahi, A. R.
    WEAR, 2010, 269 (7-8) : 590 - 601
  • [8] Enhanced Strength and High-Temperature Wear Resistance of Ti6Al4V Alloy Fabricated by Laser Solid Forming
    Zhang, Zhinan
    Li, Zhen
    Pan, Shuaihang
    Chai, Xianghai
    JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2022, 144 (11):
  • [9] Microstructure and high-temperature oxidation resistance of Ti-Al-Nb coatings on a Ti-6Al-4V alloy fabricated by laser surface alloying
    Dai, Jingjie
    Li, Shouying
    Zhang, Hongxia
    Yu, Huijun
    Chen, Chuanzhong
    Li, Yang
    SURFACE & COATINGS TECHNOLOGY, 2018, 344 : 479 - 488
  • [10] Structural and High-Temperature Oxidation Performance of Al-Co-Y Co-deposited Coatings on a TiAl-Nb Alloy at Low Temperatures
    Li, Xuan
    Wei, Zekun
    Zhang, Lijing
    Lv, Wei
    Zhang, Xuyi
    Xie, Xiaoqing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 34 (4) : 2825 - 2834