Preparation and mechanical behavior of Yb2Si2O7 interphase in SiCf/SiC minicomposites

被引:0
作者
Mu, Shuang [1 ,2 ,3 ]
Ma, Qin [1 ,2 ,3 ]
Zhang, Yu [1 ,2 ,3 ]
Shen, Xu [1 ,2 ,3 ]
Liao, Chunjing [1 ,2 ]
Zhang, Xiangyu [1 ,2 ]
Ding, Yusheng [1 ,2 ]
Dong, Shaoming [1 ,2 ,4 ]
Yang, Jinshan [1 ,2 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, State Key Lab High Performance Ceram & Superfine M, Shanghai 200050, Peoples R China
[2] Chinese Acad Sci, Shanghai Inst Ceram, Struct Ceram & Composites Engn Res Ctr, Shanghai, Peoples R China
[3] Univ Chinese Acad Sci, Beijing, Peoples R China
[4] Univ Chinese Acad Sci, Ctr Mat Sci & Optoelect Engn, Beijing, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
interface; SiC fiber; SiCf/SiC composites; Yb2Si2O7; interphase; ENVIRONMENTAL BARRIER COATINGS; CERAMIC-MATRIX COMPOSITES; SIC/SIC COMPOSITES; MINI-COMPOSITES; OXIDATION; BETA-YB2SI2O7; RESISTANCE; EVOLUTION; CMCS; ART;
D O I
10.1111/jace.20153
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, the Yb2Si2O7 interphase was prepared on SiC fibers using the sol-gel method. The influence of sol concentration on the morphology of the interphase was discussed. After heat treatment in argon at 1200 degrees C for 1 h, the Yb2Si2O7 was grown in situ on the fiber surface, forming an interphase layer. Then, SiCf/Yb2Si2O7/SiC minicomposites were prepared by chemical vapor infiltration (CVI). The Yb2Si2O7 interphase exhibited no changes throughout the high-temperature preparation process and maintained stability and compatibility with the fiber and matrix. The tensile strength of SiCf/Yb2Si2O7/SiC minicomposites with Yb2Si2O7 interphase was significantly higher than SiCf/SiC minicomposites without interphase. The crack deflection, interfacial debonding, and fiber pullout were observed in the tensile fracture of the SiCf/Yb2Si2O7/SiC minicomposites.
引用
收藏
页数:10
相关论文
共 50 条
[41]   Water vapor corrosion behavior of SiC/Si/mixed Yb2Si2O7-Yb2SiO5 environmental barrier coating for C/C composites [J].
Chen, Guohui ;
Zhang, Yulei ;
Kong, Jing'an ;
Gai, Wenhan ;
Fu, Yanqin ;
Zhang, Pengfei .
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1002
[42]   Synthesis of Single-Phase β-Yb2Si2O7 and Properties of Its Sintered Bulk [J].
Wang, Shu-Bin ;
Lu, Yan-Ru ;
Chen, Yan-Xia .
INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2015, 12 (06) :1140-1147
[43]   Hot corrosion behaviour of Yb2Si2O7 environmental barrier coatings in molten NaVO3 salt [J].
Zhang, Yongqiu ;
Zou, Binglin ;
Chen, Xiaolong ;
Cai, Xiaolong ;
Wang, Ying ;
Huang, Pai ;
Yu, Ge ;
Gu, Zhengwei .
CERAMICS INTERNATIONAL, 2021, 47 (21) :30598-30609
[44]   Effects of suspension properties on the fabrication of Yb2Si2O7 coatings using electrophoretic deposition [J].
Yilmaz, Esma ;
Xiao, Ping .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (02) :638-648
[45]   Effect of deposition temperature on phase composition, morphology and mechanical properties of plasma-sprayed Yb2Si2O7 coating [J].
Huang, Jingqi ;
Liu, Ruoyu ;
Hu, Qing ;
Wang, Yuncheng ;
Guo, Xiaojun ;
Lu, Xiangrong ;
Xu, Mingyi ;
Tu, Yunwei ;
Yuan, Jieyan ;
Deng, Longhui ;
Jiang, Jianing ;
Dong, Shujuan ;
Liu, Li ;
Chen, Meizhu ;
Cao, Xueqiang .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (15) :7902-7909
[46]   Corrosion behavior and failure mechanism of SiC whisker and c-AIPO4 particle-modified novel tri-layer Yb2Si2O7/mullite/SiC coating in burner rig tests [J].
Chen, Pengju ;
Xiao, Peng ;
Tang, Xian ;
Li, Yang .
JOURNAL OF ADVANCED CERAMICS, 2022, 11 (12) :1901-1917
[47]   A novel strategy to improve the corrosion resistance of SiCf/SiC composites in high-temperature combustion environments by cooperation of self-healing SiBCN and high-stability Yb2Si2O7 [J].
Liang, Bin ;
Ji, Suya ;
Pang, Shengyang ;
Hu, Chenglong ;
Zhao, Rida ;
Tang, Sufang .
SURFACE & COATINGS TECHNOLOGY, 2024, 489
[48]   The effect of porosity, mixed molecular/Knudsen diffusion, and a surface barrier layer on steam corrosion of Yb2Si2O7 [J].
McCormack, Simon ;
Cao, Huatang ;
Martins, Joao P. ;
Withers, Philip J. ;
Xiao, Ping .
CORROSION SCIENCE, 2023, 219
[49]   Enhancing CMAS corrosion resistance of PS-PVD Si/Yb2Si2O7 EBCs via Al-modification [J].
Wu, Jian ;
Wang, Zifan ;
Zhuo, Xueshi ;
Zhan, Yongzhong ;
Liu, Min ;
Zhou, Kesong ;
Zhang, Xiaofeng .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (08) :3727-3736
[50]   Oxidation Behavior of SiCf/SiC Composites Modified by Layered-Y2Si2O7 in Wet Oxygen Environment [J].
Wang Peng ;
Wang Qing-Lei ;
Zhang Xiang-Yu ;
Yang Jin-Shan ;
Zhou Hai-Jun ;
Hu Jian-Bao ;
Ding Yu-Sheng ;
Dong Shao-Ming .
JOURNAL OF INORGANIC MATERIALS, 2019, 34 (08) :904-908