Is additional silane application necessary for a new silane-containing universal adhesive to bond to glass ceramics?

被引:0
作者
da Silva, Priscila Luciane [1 ]
Bittencourt, Helio Radke [2 ]
Burnett Jr, Luiz Henrique [1 ]
Spohr, Ana Maria [1 ]
机构
[1] Pontificia Univ Catolica Rio Grande do Sul, Sch Dent, Dept Restorat Dent, Ave Piranga 6681,Block 6, BR-90619900 Porto Alegre, Brazil
[2] Pontificia Univ Catolica Rio Grande do Sul, Polytech Sch, Dept Stat, Porto Alegre, Brazil
关键词
adhesive; bond strength; ceramic; failure; in vitro; silane; SURFACE TREATMENTS; COMPOSITE RESIN; COUPLING AGENT; STRENGTH; PERFORMANCE;
D O I
10.1111/jerd.13283
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective To evaluate the in vitro influence of prior silane application on the microshear bond strength (mu SBS) of Scotchbond Universal Plus to glass ceramic. Materials and Methods Thirty blocks of lithium disilicate ceramic were etched with hydrofluoric acid for 20 s and distributed into Group 1 (no silane and no adhesive), Group 2 (adhesive), Group 3 (silane + adhesive). Three cylinders of resin cement were made on each ceramic block. Five blocks (n = 15 cylinders) were subjected to the mu SBS test after 24 h, and the other five blocks (n = 15 cylinders) were tested after 6 months of water storage. Results According to two-way ANOVA, followed by Tukey's test, the means of mu SBS (MPa), denoted by different letters, show significant differences (p < 0.05): after 24 h-Group 1 (31.7)(B), Group 2 (43.3)(A), and Group 3 (31.3)(B); after 6 months-Group 1 (14.8)(B), Group 2 (33.6)(A), and Group 3 (30.3)(A). After 6 months of storage, there was a significant decrease in mu SBS for Groups 1 and 2, along with an increase in adhesive failures across all groups. Conclusions Prior application of silane did not increase the mu SBS between Scotchbond Universal Plus and ceramic, and there was degradation at the bond interface over time. Clinical SignificancePrior application of a silane agent is not necessary when using Scotchbond Universal Plus for bonding to glass ceramics. Regardless of the prior application of silane, there is degradation at the bond interface over time.
引用
收藏
页码:1452 / 1458
页数:7
相关论文
共 41 条
[11]  
Moura DMD, 2020, BRAZ ORAL RES, V34, DOI [10.1590/1807.3107bor-2020.vol34.0018, 10.1590/1807-3107bor-2020.vol34.0018]
[12]   A technique to facilitate ceramic veneer cementation [J].
Farah, Ra'fat, I ;
Aldhafeeri, Abdullah Fahad ;
Alogaili, Rakan Saud .
JOURNAL OF PROSTHETIC DENTISTRY, 2018, 120 (02) :194-197
[13]  
Garboza Celso Sebastião, 2016, Braz. Dent. J., V27, P458, DOI 10.1590/0103-6440201600624
[14]  
Ghodsi Safoura, 2021, J Clin Exp Dent, V13, pe1154, DOI 10.4317/jced.58671
[15]   Optimization and characterization of biomolecule immobilization on silicon substrates using (3-aminopropyl)triethoxysilane (APTES) and glutaraldehyde linker [J].
Gunda, Naga Siva Kumar ;
Singh, Minashree ;
Norman, Lana ;
Kaur, Kamaljit ;
Mitra, Sushanta K. .
APPLIED SURFACE SCIENCE, 2014, 305 :522-530
[16]   THE STRUCTURE OF AN AMINOSILANE COUPLING AGENT IN AQUEOUS-SOLUTIONS AND PARTIALLY CURED SOLIDS [J].
ISHIDA, H ;
NAVIROJ, S ;
TRIPATHY, SK ;
FITZGERALD, JJ ;
KOENIG, JL .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1982, 20 (04) :701-718
[17]  
IvoclarVivadent, 2014, IPS EMAX PRESS TECHN
[18]  
Jardel V, 1999, INT J PROSTHODONT, V12, P59
[19]   Performance of universal adhesives on bonding to leucite-reinforced ceramic [J].
Kim R.J.-Y. ;
Woo J.-S. ;
Lee I.-B. ;
Yi Y.-A. ;
Hwang J.-Y. ;
Seo D.-G. .
Biomaterials Research, 19 (1)
[20]  
Lee HY., 2016, RESTOR DENT ENDOD, V42, P95