Influence of cryogenic deformation and post-deform aging on microstructure and mechanical properties of Al-Cu alloy

被引:0
|
作者
Fan, Xiaobo [1 ,2 ]
Kang, Xin [1 ]
Zhang, Zhichao [3 ]
Zhang, Xuanming [3 ]
Yuan, Shijian [4 ]
机构
[1] Dalian Univ Technol, Sch Mech Engn, Dalian, Peoples R China
[2] Dalian Univ Technol, State Key Lab High performance precis Mfg, Dalian, Peoples R China
[3] Shanghai Aerosp Equipments Manufacturer Co Ltd, Shanghai, Peoples R China
[4] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Cu alloy; Cryogenic forming; Artificial aging; Mechanical properties; Strengthening mechanism; ALUMINUM-ALLOY; PRECIPITATION; STRENGTH; PHASE; BEHAVIOR;
D O I
10.1016/j.jallcom.2024.175894
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cryogenic forming has been developed as a new forming process for aluminum alloy components with ultra-thin thickness or complex shapes. But their mechanical properties are severely affected by cryogenic deformation and post-deform aging. The cooperative effects were thus studied under different cryogenic deformation and aging treatment conditions. The corresponding strengthening mechanisms were revealed through microstructure characterizations. The changements in dislocation and grain structure were evaluated through X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). Precipitation evolutions were reflected by differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). The strengthening effects were revealed through quantitative strengthening contribution analysis. It was found that excellent mechanical properties could be obtained under the combined contributions of cryogenic deformation and post-deform aging. Large cryogenic deformation can improve the strengths significantly without artificial aging, benefiting from the more produced dislocations and a few deformation-promoting theta '' phases. The highest yield strength reached 397.5 MPa after 30 % cryogenic deformation, which was 7.4 % higher than that of traditional T87. Cryogenic deformation could accelerate the precipitation obviously in artificial aging, which led to the continuous transformation of theta '' phase into dispersive theta ' phase in the peak aging condition. The peak aging time shortened gradually with the increasing cryogenic deformation. Excellent strength could be even obtained by aging 6 h at 175 degrees C for 2 % cryogenic deformation, which is just one-third of the traditional aging time. Moreover, the deformationproduced dislocations would recover in artificial aging, which is beneficial to the optimal combination of strength and toughness through large cryogenic deformation and short-time artificial aging. The processcontrolling window was established, which can provide huge potential to adjust the performance distribution in cryogenic forming for heat-treatable aluminum alloy.
引用
收藏
页数:17
相关论文
共 50 条
  • [21] Forming properties and microstructure of Al-Cu alloy prepared by liquid-die forging
    Zhang Xin
    Xu Hong
    Chen Tong
    Wang Chang-shun
    Wang Yan-long
    Xu Lan-jun
    Li Hong-wei
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2022, 29 (01) : 60 - 79
  • [22] Influence of Ti elements on the evolution of microstructure, mechanical properties and thermal stability of Al-Cu alloy
    Hu, Kuishen
    Zou, Chunming
    Wang, Hongwei
    Wei, Zunjie
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 952
  • [23] Influence of megaplastic deformation on the structure and hardness of Al-Cu-Mg alloy after aging
    Petrova, A. N.
    Radziszewska, H.
    Kaczmarek, L.
    Klih, M.
    Brodova, I. G.
    Steglinski, M.
    PHYSICS OF METALS AND METALLOGRAPHY, 2016, 117 (12): : 1237 - 1244
  • [24] Effects of the Rolling Temperature on the Microstructure Uniformities and Mechanical Properties of Large 2219 Al-Cu Alloy Rings
    Guo, Wanfu
    Chen, Dian
    Yi, Youping
    Ruan, Jinhua
    Liu, Changming
    METALS AND MATERIALS INTERNATIONAL, 2024, 30 (06) : 1505 - 1512
  • [25] Influence of cryogenic deformation on second-phase particles, grain structure, and mechanical properties of Al-Cu-Mn alloy
    Dong, Fei
    Yi, Youping
    Huang, Cheng
    Huang, Shiquan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 827 (827)
  • [26] Microstructure and mechanical properties stability of pre-hardening treatment in Al-Cu alloys for pre-hardening forming process
    Tang, Liping
    Wei, Pengfei
    Hu, Zhili
    Pang, Qiu
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2024, 31 (03) : 539 - 551
  • [27] Microstructure evolution and mechanical properties of Al-Cu alloys inoculated by FeBSi metallic glass
    Bai, Zhihao
    Qiu, Feng
    Chi, Jiaxuan
    Zhang, Tao
    Jiang, Qichuan
    MATERIALS & DESIGN, 2015, 67 : 130 - 135
  • [28] Age Hardening and Mechanical Properties of Cast Al-Cu Alloy Modified by La and Pr
    Bai, Zhihao
    Qiu, Feng
    Liu, Yingying
    Zhou, Wei
    Jiang, Qichuan
    ADVANCED ENGINEERING MATERIALS, 2015, 17 (02) : 143 - 147
  • [29] Microstructure Evolution and Mechanical Properties of 2219 Al Alloy During Aging Treatment
    Wang, Huimin
    Yi, Youping
    Huang, Shiquan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (04) : 1475 - 1482
  • [30] Synergetic Effect of Cryorolling and Postroll Aging on Simultaneous Increase in Wear Resistance and Mechanical Properties of an Al-Cu Alloy
    Jaseem, I
    Immanuel, R. J.
    Rao, P. N.
    Khan, F.
    Sahoo, B. N.
    Panigrahi, S. K.
    Kamaraj, M.
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2018, 140 (06):