Influence of cryogenic deformation and post-deform aging on microstructure and mechanical properties of Al-Cu alloy

被引:0
|
作者
Fan, Xiaobo [1 ,2 ]
Kang, Xin [1 ]
Zhang, Zhichao [3 ]
Zhang, Xuanming [3 ]
Yuan, Shijian [4 ]
机构
[1] Dalian Univ Technol, Sch Mech Engn, Dalian, Peoples R China
[2] Dalian Univ Technol, State Key Lab High performance precis Mfg, Dalian, Peoples R China
[3] Shanghai Aerosp Equipments Manufacturer Co Ltd, Shanghai, Peoples R China
[4] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Cu alloy; Cryogenic forming; Artificial aging; Mechanical properties; Strengthening mechanism; ALUMINUM-ALLOY; PRECIPITATION; STRENGTH; PHASE; BEHAVIOR;
D O I
10.1016/j.jallcom.2024.175894
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cryogenic forming has been developed as a new forming process for aluminum alloy components with ultra-thin thickness or complex shapes. But their mechanical properties are severely affected by cryogenic deformation and post-deform aging. The cooperative effects were thus studied under different cryogenic deformation and aging treatment conditions. The corresponding strengthening mechanisms were revealed through microstructure characterizations. The changements in dislocation and grain structure were evaluated through X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). Precipitation evolutions were reflected by differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). The strengthening effects were revealed through quantitative strengthening contribution analysis. It was found that excellent mechanical properties could be obtained under the combined contributions of cryogenic deformation and post-deform aging. Large cryogenic deformation can improve the strengths significantly without artificial aging, benefiting from the more produced dislocations and a few deformation-promoting theta '' phases. The highest yield strength reached 397.5 MPa after 30 % cryogenic deformation, which was 7.4 % higher than that of traditional T87. Cryogenic deformation could accelerate the precipitation obviously in artificial aging, which led to the continuous transformation of theta '' phase into dispersive theta ' phase in the peak aging condition. The peak aging time shortened gradually with the increasing cryogenic deformation. Excellent strength could be even obtained by aging 6 h at 175 degrees C for 2 % cryogenic deformation, which is just one-third of the traditional aging time. Moreover, the deformationproduced dislocations would recover in artificial aging, which is beneficial to the optimal combination of strength and toughness through large cryogenic deformation and short-time artificial aging. The processcontrolling window was established, which can provide huge potential to adjust the performance distribution in cryogenic forming for heat-treatable aluminum alloy.
引用
收藏
页数:17
相关论文
共 50 条
  • [11] Enhanced mechanical properties in 7075 Al alloy fasteners processed by post ECAP-CU aging
    Zhang, Junjie
    He, Tao
    Du, Xiangyang
    Alexey, Vereschaka
    Song, Miao
    Chen, Xilin
    MATERIALS TODAY COMMUNICATIONS, 2025, 45
  • [12] Microstructure analysis of high-temperature deformation of Al-Cu alloy
    Yuan, Xia
    Hui, Jun
    Feng, Zaixin
    Fan, Wenxin
    Gao, Weifeng
    Xue, Chen
    MATERIALS RESEARCH EXPRESS, 2018, 5 (06):
  • [13] Mechanical Properties and Microstructure of Thin-Walled Al-Cu Alloy Casting
    L. Xiang
    J. Q. Tao
    Q. Chen
    G. Z. Zhao
    F. Y. Zhang
    S. X. Chai
    Z. H. Xing
    M. Li
    E. C. Yang
    F. Li
    Strength of Materials, 2022, 54 : 302 - 308
  • [14] Effects of deformation temperature on the evolution of second mechanical phase and properties of large 2219 Al-Cu alloy rings
    Guo, Wanfu
    Yi, Youping
    Huang, Shiquan
    Mao, Xianchang
    Fang, Jie
    He, Hailin
    Hu, Bin
    MATERIALS CHARACTERIZATION, 2020, 160 (160)
  • [15] Microstructure and Mechanical Properties of Friction Stir Repaired Al-Cu Casting Alloy
    Ji, Shude
    Huang, Ruofei
    Zhang, Liguo
    Meng, Xiangchen
    Lv, Zan
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (08) : 2057 - 2065
  • [16] Effects of cold deformation modes on microstructure uniformity and mechanical properties of large 2219 Al-Cu alloy rings
    Guo, Wanfu
    Yi, Youping
    Ruan, Jinhua
    Liu, Changming
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2023, 62 (01)
  • [17] Effect of thermo-mechanical treatment on microstructure and mechanical properties of wire-arc additively manufactured Al-Cu alloy
    Zhang, Tao
    Qin, Zhen-yang
    Gong, Hai
    Wu, Yun-xin
    Chen, Xin
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2024, 31 (07) : 2181 - 2193
  • [19] Influence of heat treatment on microstructure and mechanical properties of Al/Al-Cu graded materials
    Cong, Qian
    Xu, Fumin
    Tan, Yi
    Shi, Xiaolei
    Dong, Wei
    Li, Jiayan
    Zhang, Junshan
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2011, 24 (02) : 118 - 124
  • [20] Effect of Aging Regime on Microstructure and Mechanical Properties of 2195 Al-Li Alloy
    Wang Yun
    Xu Yong
    Xia Liangliang
    Chen Shuaifeng
    Yin Kuo
    Men Xiangnan
    Deng Tao
    Shi-Hong Zhang
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (10) : 3884 - 3891