Flexural behavior of ribbed CFRP bars in ultra-high-performance fiber-reinforced concrete (UHPFRC) beams with lap-splice connection

被引:0
作者
Yoo, Sun-Jae [1 ]
Yoo, Doo-Yeol [2 ]
Lee, Jin-Young [3 ]
Lee, Joo-Ha [4 ]
Yoon, Young-Soo [1 ]
机构
[1] Korea Univ, Sch Civil Environm & Architectural Engn, 145 Anam Ro, Seoul 02841, South Korea
[2] Yonsei Univ, Dept Architecture & Architectural Engn, 50 Yonsei Ro, Seoul 03722, South Korea
[3] Kyungpook Natl Univ, Dept Agr Civil Engn, 80 Daehak Ro, Daegu 41566, South Korea
[4] Univ Suwon, Dept Civil & Environm Engn, 17 Wauan Gil, Hwaseong Si 18323, Gyeonggi Do, South Korea
基金
新加坡国家研究基金会;
关键词
Ribbed CFRP bar; UHPFRC; Lap-spliced beam; Bond strength; Minimum lap-splice length; BOND BEHAVIOR; POLYMER BARS; GFRP BARS; STRENGTH; STEEL;
D O I
10.1016/j.cemconcomp.2024.105700
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Due to transport limitations, lap-splice of CFRP bars is imperative, lap-spliced CFRP bars in ultra-high strength concrete can be an innovative solution by reducing the lap-splice length. This study investigated lap-splice behavior of CFRP bars in UHPFRC and required lap-splice length of CFRP bars by comparing design guidelines. For these purposes, a total of 8 beam specimens were fabricated and subjected to four-point loading. Two beams are control variables, one of which consists of a continuous ribbed CFRP bar, and the other of a mechanical connection by coupler. The main parameters are different lap-splice lengths (20d, 40d, and 60d), and concrete strength (normal strength concrete (NC), high strength concrete (HC), ultra-high-performance fiberreinforced concrete (UHPFRC)), including one beam with traverse reinforcement in the lap-spliced region. Test results showed that the coupler connection was disadvantageous, with the ultimate load reducing by approximately 76 % compared to the un-spliced beam. A lap-splice length of 60d was determined to be the critical length, resulting in 1.0 % and 6.3 % higher ultimate load and developed tensile strength compared to the unspliced beam. The ultimate load was increased by about 14 % due to the contribution of transverse reinforcement in the lap-spliced region. Unlike NC and HC, lap-spliced ribbed CFRP bars in UHPFRC can prevent splitting failure with crack localization around the loading points. Current design guideline for lap-splice length of FRP bars does not predict well ribbed CFRP bars in UHPFRC, and the predicted lap-splice length of ribbed CFRP bars in UHPFRC was shown to be about 42d.
引用
收藏
页数:15
相关论文
共 67 条
  • [1] Effect of confining stirrups and bar gap in improving bond behavior of glass fiber reinforced polymer (GFRP) bar lap splices in RC beams
    Abbas, Husain
    Elsanadedy, Hussein
    Alaoud, Louai
    Almusallam, Tarek
    Al-Salloum, Yousef
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2023, 365
  • [2] ACI, 2019, ACI 318-14
  • [3] Bond Performance of GFRP Bar-Splicing in Reinforced Concrete Beams
    Al-Salloum, Yousef
    Alaoud, Louai
    Elsanadedy, Hussein
    Albidah, Abdulrahman
    Almusallam, Tarek
    Abbas, Husain
    [J]. JOURNAL OF COMPOSITES FOR CONSTRUCTION, 2022, 26 (02)
  • [4] [Anonymous], 2012, ASTM C. 1609
  • [5] [Anonymous], 2012, CSA S806-12
  • [6] [Anonymous], 2015, ACI 440.1R-15
  • [7] [Anonymous], 2021, ASTM Standard D7205/D7205M-06, V633
  • [8] [Anonymous], 2015, STANDARD TEST METHOD, DOI DOI 10.1520/C0127-15
  • [9] [Anonymous], 2014, S614 CANCSA
  • [10] [Anonymous], 2015, Standard test method for relative density (specific gravity) and absorption of fine aggregate