Microstructure and Strength Parameters of Cement-Stabilized Loess

被引:10
|
作者
Axel, Mani [1 ]
Li, Xi'an [1 ]
Wen, Feng [1 ]
An, Ming-Xiao [1 ]
机构
[1] Changan Univ, Dept Geol Engn & Geomat, Xian 710064, Peoples R China
来源
GEOTECHNICS | 2023年 / 3卷 / 02期
基金
中国国家自然科学基金;
关键词
loess stabilization; cement; mechanical properties; landslide; microstructure; COMPRESSIVE STRENGTH; FLY-ASH; LANDSLIDE; PLATEAU; SOILS; LIME;
D O I
10.3390/geotechnics3020010
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
In this study, cement was used as a component to provide a stabilizing effect in order to evaluate the hardness and stability of loess soil. To evaluate the strength properties of loess soil reinforced with cement, samples with four distinct cement concentrations (3%, 5%, 7%, and 9%) and three distinct curing durations (7, 14, and 28 days) were generated. During a series of tests, the flexural strength, direct shear strength, indirect tensile strength, and unconfined compressive strength were determined. An appropriate cement dosage was found, in addition to a durability index that could be used to quantify the effect of water absorption investigations on cement-stabilized loess. Both of these discoveries were made simultaneously. Scanning electron microscopy (SEM) and energy dispersive X-ray fluorescence spectrometry (XRF) examinations were carried out so that the fundamental mechanics of the materials could be comprehended. The results show that the cohesion of cement-stabilized loess is much more sensitive to structure than the friction angle of the material. The increase in shear strength after remoulding is due to cohesion. The SEM study showed that the cement interacted with the loess particles to produce a thick cement network that successfully covered the voids and boosted the mixture's strength parameters. The 28-days UCS for the samples containing 7% cement was the greatest, at 3.5 MPa, while the UCS for those containing 9% cement was 4.78 MPa. The highest flexural tensile strength of 1.98 N/mm2 was determined after 28 days. The tensile strength after 7 days in samples containing 3%, 5%, 7%, and 9% cement reached a maximum force of 0.15 MPa, 0.23 MPa, 0.27 MPa, and 0.37 MPa, respectively, and increased with each passing day. To achieve the desired level of strength, it is necessary to adjust the proportion of cement. In addition, as the curing period progressed, we observed an increase in the resistance and stiffness of the cement-stabilized loess due to the interactions that take place between the structure and the mineral composition. It is believed that this event was caused by naturally occurring cementation. As a consequence of this reaction, the production of new cementitious materials takes place. The cation exchange that causes the hydration and pozzolanic reaction that leads to the creation of aggregates and interparticle flocculation is responsible for their production. These findings suggest that cement may be utilised as a simple and effective method of loess stabilization, ultimately resulting in improved performance of the loess. Therefore, this study revealed that cement may considerably enhance the microstructure and strength parameters of loess. This research provides important information on cement-stabilized loess that has ramifications for geotechnical investigation, construction, research, and testing to achieve a successful project.
引用
收藏
页码:161 / 178
页数:18
相关论文
共 50 条
  • [31] Bond Strength of Coir Fibers in Cement-Stabilized Rammed Earth Matrix
    Rathod, R. Sri Bhanupratap
    Reddy, B. V. Venkatarama
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2021, 33 (11)
  • [32] Strength and durability improvement of cement-stabilized Al-Qatif soil by the addition of sand
    Mohammad Sharif Zami
    Adeoluwa Oladapo Ewebajo
    Omar S. Baghabra Al-Amoudi
    Mohammed A. Al-Osta
    Yassir Mubarak Hussein Mustafa
    Arabian Journal of Geosciences, 2022, 15 (15)
  • [33] Comparison of Mechanical Properties of Cement-Stabilized Loess Produced Using Different Compaction Methods
    Jiang, Yingjun
    Yuan, Kejia
    Li, Qilong
    Deng, Changqing
    Yi, Yong
    Zhang, Yu
    Xue, Jinshun
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2020, 2020 (2020)
  • [34] Strength, durability and cost effectiveness of cement-stabilized laterite hollow blocks
    Alutu, OE
    Oghenejobo, AE
    QUARTERLY JOURNAL OF ENGINEERING GEOLOGY AND HYDROGEOLOGY, 2006, 39 : 65 - 72
  • [35] Evaluation on Strength Properties of Lime-Slag Stabilized Loess as Pavement Base Material
    Jia, Liang
    Zhang, Li
    Guo, Jian
    Yao, Kai
    Lim, Sin Mei
    Li, Bin
    Xu, Hui
    SUSTAINABILITY, 2019, 11 (15)
  • [36] Performance of cement-stabilized sand subjected to freeze-thaw cycles
    Jumassultan, Assel
    Sagidullina, Nazerke
    Kim, Jong
    Ku, Taeseo
    Moon, Sung-Woo
    GEOMECHANICS AND ENGINEERING, 2021, 25 (01) : 41 - 48
  • [37] Microscopic Properties and Splitting Tensile Strength of Fiber-Modified Cement-Stabilized Aeolian Sand
    Zhang, Xiangdong
    Geng, Jie
    Pang, Shuai
    Su, Lijuan
    Cai, Guanjun
    Zhou, Zhongchao
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2023, 35 (06)
  • [38] Influence of Silica Fume and Additives on Unconfined Compressive Strength of Cement-Stabilized Marine Soft Clay
    Yang, Qing
    Du, Chuanxin
    Zhang, Jinli
    Yang, Gang
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2020, 32 (02)
  • [39] STRENGTH PROPERTIES OF CEMENT-STABILIZED MUNICIPAL SOLID-WASTE INCINERATOR ASH MASONRY BRICKS
    ALI, MT
    CHANG, WF
    ACI MATERIALS JOURNAL, 1994, 91 (03) : 256 - 263
  • [40] The effect of water content and cement content on the strength of portland cement-stabilized compacted fly ash
    Kalinski, ME
    Hippley, BT
    FUEL, 2005, 84 (14-15) : 1812 - 1819