Role of Quenching Temperature Selection in the Improvement of the Abrasive (Al2O3) Wear Resistance of Hybrid Multi-Component Cast Irons

被引:1
作者
Chabak, Yuliia [1 ,2 ]
Efremenko, Vasily [1 ,2 ]
Petryshynets, Ivan [2 ]
Golinskyi, Michail [1 ]
Shimizu, Kazumichi [3 ]
Efremenko, Bohdan [1 ,4 ]
Kudin, Vadim [5 ]
Azarkhov, Alexander [4 ]
机构
[1] Pryazovskyi State Tech Univ, Phys Dept, UA-49044 Dnipro, Ukraine
[2] Slovak Acad Sci, Inst Mat Res, Div Met Syst, Kosice 04001, Slovakia
[3] Muroran Inst Technol, Grad Sch Engn, 27-1 Mizumoto, Muroran, Hokkaido 0508585, Japan
[4] Pryazovskyi State Tech Univ, Biomed Engn Dept, UA-49044 Dnipro, Ukraine
[5] Natl Univ Zaporizhzhia Polytech, Dept Machines & Technol Foundry Prod, UA-69063 Zaporizhzhia, Ukraine
关键词
multi-component cast iron; high boron content; quenching; carboborides; matrix; hardness; abrasive wear resistance; HEAT-TREATMENT; MECHANICAL-PROPERTIES; CURIE-TEMPERATURE; HARDNESS; CARBIDES; BEHAVIOR; CR; MN; NI; MICROSTRUCTURE;
D O I
10.3390/ma17153742
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, enhancing the tribological characteristics of novel cast metallic materials-hybrid multi-component cast irons-by applying a strengthening heat treatment is described. The experimental materials were the cast alloys of a nominal composition (5 wt.% W, 5 wt.% Mo, 5 wt.% V, 10 wt.% Cr, 2.5 wt.% Ti, Fe is a balance) supplemented with 0.3-1.1 wt.% C and 1.5-2.5 wt.% B (total of nine alloys). The heat treatment was oil-quenching followed by 200 degrees C tempering. The quench temperature (QT) varied in the range of 900-1200 degrees C, with a step of 50 degrees C (with a 2-h holding at QT). The correlation of the QT with microstructure and properties was estimated using microstructure/worn surface characterization, differential scanning calorimetry, hardness measurement, and three-body-abrasive wear testing (using Al2O3 particles). The as-cast alloys had a multi-phase structure consisting of primary and/or eutectic borocarbide M-2(B,C)(5), carboborides M(C,B), M-7(C,B)(3), M-3(C,B), and the matrix (ferrite, martensite, pearlite/bainite) in different combinations and volume fractions. Generally, the increase in the quenching temperature resulted in a gradual increase in hardness (maximally to 66-67 HRC) and a decrease in the wear rate in most alloys. This was due to the change in the phase-structure state of the alloys under quenching, namely, the secondary carboboride precipitation, and replacing ferrite and pearlite/bainite with martensite. The wear rate was found to be inversely proportional to bulk hardness. The maximum wear resistance was attributed to QT = 1150-1200 degrees C, when the wear rate of the alloys was lowered by three to six times as compared to the as-cast state. With the QT increase, the difference in the wear rate of the alloys decreased by three times. The highest abrasive resistance was attributed to the alloys with 1.1 wt.% C, which had a 2.36-3.20 times lower wear rate as compared with that of the reference alloy (13 wt.% Cr cast iron, hardness of 66 HRC). The effects of carbon and boron on hardness and wear behavior are analyzed using the regression models developed according to the factorial design procedure. The wear mechanisms are discussed based on worn surface characterization.
引用
收藏
页数:26
相关论文
共 50 条
[31]   Preparation and Wear Resistance of Aluminum Composites Reinforced with In Situ Formed TiO/Al2O3 [J].
Qin, Q. D. ;
Huang, B. W. ;
Li, W. ;
Zeng, Z. Y. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (05) :2029-2036
[32]   Al2O3/(W,Ti)C/CaF2 multi-component graded self-lubricating ceramic cutting tool material [J].
Xu, C. H. ;
Wu, G. Y. ;
Xiao, G. C. ;
Fang, B. .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 45 :125-129
[33]   Relationship between microstructure and abrasive wear resistance of Al2O3-FeAl2O4 nanocomposites produced via solid-state precipitation [J].
Mukhopadhyay, Amartya ;
Todd, Richard I. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (03) :339-350
[34]   Impact-abrasive wear property of ZrO2 toughened Al2O3 ceramic particles reinforced high manganese steel matrix composites [J].
Wang, Zhijie ;
Zhou, Mojin ;
Jiang, Yehua ;
Sui, Yudong ;
Li, Zulai .
TRIBOLOGY INTERNATIONAL, 2024, 194
[35]   Effect of Y2O3-stabilized ZrO2 whiskers on the microstructure, mechanical and wear resistance properties of Al2O3 based ceramic composites [J].
Fang, Yihang ;
Chen, Nan ;
Du, Guoping ;
Zhang, Mengxian ;
Zhao, Xianrui ;
Wu, Jianbo .
CERAMICS INTERNATIONAL, 2019, 45 (13) :16504-16511
[36]   Microstructure and Wear Study of Al 7075-T6/Eggshell/SiC/Al2O3 Hybrid Composites [J].
Moona, Girija ;
Rastogi, Vikas ;
Walia, R. S. ;
Sharma, Rina .
RECENT ADVANCES IN MECHANICAL ENGINEERING, NCAME 2019, 2020, :471-481
[37]   Abrasive Wear Model for Al2O3 Particle Reinforced MMCs Using Genetic Expression Programming [J].
Koek, Metin ;
Kanca, Erdogan .
CMC-COMPUTERS MATERIALS & CONTINUA, 2010, 18 (03) :213-235
[38]   Mechanical Properties and Abrasive Wear Behaviour of Functionally Graded Al-Si12Cu/Al2O3 Metal Matrix Composite [J].
Radhika, N. .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (01) :145-157
[39]   Effect of Al2O3 Nanoparticles and Heat Treatment on the Wear Resistance of Electrodeposited Ni-W/Al2O3 Composite Coatings [J].
Xinyang Shi ;
Zhongquan Zhang ;
Leyu Dai ;
Yin Lv ;
Zhao Xu ;
Yibiao Yin ;
Zhiqun Liao ;
Guoying Wei .
Journal of Materials Engineering and Performance, 2022, 31 :3094-3106
[40]   Effect of Si content on impact-abrasive wear resistance of Al2O3p/steel composites prepared by squeeze casting [J].
Lu, De-hong ;
Li, Hai-zhou ;
Ren, Bo .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2018, 25 (09) :984-994