Effects of the application protocol and bonding strategy of the universal adhesive on dentin previously impregnated with bioceramic sealer
被引:0
作者:
Barros, Antonia Patricia Oliveira
[1
]
Costa, Joatan Lucas de Sousa Gomes
Monteiro, Jardel Camilo do Carmo
[1
,2
]
Galvani, Lucas David
[3
]
de Andrade, Marcelo Ferrarezi
[1
]
Saad, Jose Roberto Cury
[1
]
Kuga, Milton Carlos
[1
]
机构:
[1] Sao Paulo State Univ, Araraquara Dent Sch, Dept Operat Dent, Araraquara, SP, Brazil
[2] Univ Fed Minas Gerais, Dept Restorat Dent, Belo Horizonte, MG, Brazil
[3] Sao Paulo State Univ, Araraquara Dent Sch, Dept Dent Mat & Prosthet, Araraquara, SP, Brazil
关键词:
Bond strength;
Failure modes;
Protocols;
Bioceramic Sealer;
Root canal filling material;
STRENGTH;
SYSTEMS;
IMPROVE;
D O I:
10.1016/j.ijadhadh.2024.103765
中图分类号:
TQ [化学工业];
学科分类号:
0817 ;
摘要:
Purpose: To evaluate the effects of the application of universal adhesive with manual brush (MB) or rotary brush (RB), in the etch-and-rinse (ER) or self-etching (SE) strategy, on the bond strength, adhesive layer thickness, and adhesive failure pattern to dentin impregnated with bioceramic sealer, at 24 h and 1 year. Materials and methods: Eighty-eight bovine incisor crowns were impregnated with bioceramic sealer was kept for 15 min and cleaned with cotton soaked in distilled water. They were then divided into four groups (n = 22): ERMB, ER-RB, SE-MB, SE-RB. Subsequently, the specimens were restored with Filtek Z-250 resin. The adhesive layer thickness was individually analyzed using laser confocal microscope. Bond strength was assessed through microtensile testing, and the failure pattern was examined using a stereomicroscope. Data were analyzed by oneway ANOVA/Tukey 's tests ( alpha = 0.05). Results: The adhesive layer thickness provided by ER-MB and SE-MB was greater than that provided by ER-RB and SE-RB (P < 0.05). ER-MB showed the lowest bond strength at 24 h (P < 0.05). At 1 year, SE-MB and SERB exhibited the highest bond strength values (P < 0.05). ER-MB demonstrated a higher incidence of adhesive failure at 24 h. At 1 year, SE-RB and SE-MB showed a higher incidence of mixed failure. Conclusion: The use of Scotchbond Universal (R) adhesive in the etch-and-rinse strategy applied with a MB negatively affects bond strength at 24 h, worsening after 1 year of control, regardless of the application protocol.