Friction stir welding of constrained groove pressed Al1050 using Al2O3 nanoparticles

被引:0
作者
Keshavarz, Hossein [1 ]
Moosavi, Seyyed Ezzatollah [1 ]
Kazeminezhad, Mohsen [1 ]
Movahedi, Mojtaba [1 ]
机构
[1] Sharif Univ Technol, Dept Mat Sci & Engn, Azadi Ave, Tehran, Iran
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 32卷
关键词
Friction stir welding; Constrained groove pressing; Aluminum; Mechanical properties; Al2O3; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; ALUMINUM; MICROSTRUCTURE; NANOCOMPOSITES; STRENGTH; BEHAVIOR; JOINT;
D O I
10.1016/j.jmrt.2024.07.198
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this investigation, two passes Constrained Groove Pressed (CGPed) Al1050 sheets went through Friction Stir Welding (FSW) by adding nano-sized Al2O3 particles. Then, the microstructure and mechanical properties of the welded joints, undergone various pass numbers and rotational to traverse speed (w/v) ratios, were presented. Findings showed all joints were fractured from the SZ, although HAZ softening happened due to grain growth in this region. The presence of the Al2O3 particles in the stir zone led to a fine and equiaxed grain structure, resulting from continuous dynamic recrystallization (CDRX) during the high-temperature welding process. This grain refinement contributed to an improvement in the mechanical properties of the joints, such as strength and microhardness. Employing two different w/v ratios resulted in a variety of thermal cycles during the welding procedure such that the peak temperature in the w/v of 70 and 25 r/mm reached 423 degrees C and 285 degrees C, respectively. Microstructure studies via optical observation and EBSD analysis illustrated that employing a higher w/v ratio and weld pass number resulted in more uniform particle distribution in the stir zone thanks to facilitating materials flow and incorporation during FSW. As a result, the three passes FSWed sample at the higher w/v ratio of 70 r/mm showed the most homogeneous particle distribution and finest grain structure in the SZ. This microstructure evolution was in reliable agreement with the mechanical performance of the joints. The three passes FSWed sample at the higher w/v ratio of 70 r/mm demonstrated the highest weld strength, microhardness, and %elongation compared to other FSWed joints. This sample showed an ultimate tensile strength (UTS) of 97 MPa and a %elongation of 16%, and its mean microhardness value had a 3.5% increase compared to the CGPed base metal. Conversely, the one pass FSWed sample at the lower w/v ratio of 25 r/mm represented the weakest mechanical properties due to cavities, defects, and agglomerated Al2O3 nanoparticles. The presence of nanoparticles was a decisive factor in microstructural evolution during the welding, thereby increasing the mechanical quality of the joints dependent upon their uniform dispersion, obtained by increasing the pass number and w/v ratio.
引用
收藏
页码:597 / 608
页数:12
相关论文
共 50 条
  • [41] Influence of hard inclusions on microstructural characteristics and textural components during dissimilar friction-stir welding of an PM Al-Al2O3-SiC hybrid nanocomposite with AA1050 alloy
    Khodabakhshi, F.
    Simchi, A.
    Kokabi, A. H.
    Gerlich, A. P.
    Nosko, M.
    Svec, P.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2017, 22 (05) : 412 - 427
  • [42] Fabrication and characterization of friction stir processed Al 6061 reinforced with TiB2-Al2O3
    Rao, Ch. Mohana
    Rao, K. Mallikarjuna
    INTERNATIONAL JOURNAL OF STRUCTURAL INTEGRITY, 2021, 12 (03) : 378 - 387
  • [43] Enhancing compressive response of Mg-6Al alloy using Al2O3 nanoparticles
    Mardi, K. Bimla
    Mallick, A.
    Dixit, A. Rai
    Gupta, M.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2018, 56 (03): : 183 - 190
  • [44] Cross accumulative roll bonding A novel mechanical technique for significant improvement of stir-cast Al/Al2O3 nanocomposite properties
    Ardakani, Mohammad Reza Kamali
    Amirkhanlou, Sajjad
    Khorsand, Shohreh
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 591 : 144 - 149
  • [45] Formations of AZ91/Al2O3 nano-composite layer by friction stir processing
    Ahmadkhaniha, D.
    Sohi, M. Heydarzadeh
    Salehi, A.
    Tahavvori, R.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2016, 4 (04) : 314 - 318
  • [46] Investigation of residual stress distribution of dissimilar Al-7075-T6 and Al-6061-T6 in the friction stir welding process strengthened with SiO2 nanoparticles
    Jafari, Hasan
    Mansouri, Hadi
    Honarpisheh, Mohammad
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 43 : 145 - 153
  • [47] SiC and Al2O3 Reinforced Friction Stir Welded Joint of Aluminium Alloy 6061
    Pasha, Md Aleem
    Reddy, P. Ravinder
    Laxminarayana, P.
    Khan, Ishtiaq Ahmed
    STRENGTHENING AND JOINING BY PLASTIC DEFORMATION, 2019, : 163 - 182
  • [48] Analysis of tensile strength on friction stir welded Al 6061 composite reinforced with B4C and Cr2O3 using RSM and ANN
    Uday, K. N.
    Rajamurugan, G.
    ENGINEERING RESEARCH EXPRESS, 2023, 5 (01):
  • [49] Impact of Al2O3 Particle Size on the Open Porosity of Ni/Al2O3 Composites Prepared by the Thermal Oxidation at Moderate Temperatures
    Opalek, Andrej
    Gaburjakova, Marta
    Svec, Peter
    Kudela, Stanislav
    Stepanek, Matej
    Stefanik, Pavol
    Izdinsky, Karol
    METALS, 2021, 11 (10)
  • [50] Pure Aluminum Structure and Mechanical Properties Modified by Al2O3 Nanoparticles and Ultrasonic Treatment
    Zhukov, Ilya A.
    Kozulin, Alexander A.
    Khrustalyov, Anton P.
    Kahidze, Nikolay, I
    Khmeleva, Marina G.
    Moskvichev, Evgeny N.
    Lychagin, Dmitry, V
    Vorozhtsov, Alexander B.
    METALS, 2019, 9 (11)