Friction stir welding of constrained groove pressed Al1050 using Al2O3 nanoparticles

被引:0
作者
Keshavarz, Hossein [1 ]
Moosavi, Seyyed Ezzatollah [1 ]
Kazeminezhad, Mohsen [1 ]
Movahedi, Mojtaba [1 ]
机构
[1] Sharif Univ Technol, Dept Mat Sci & Engn, Azadi Ave, Tehran, Iran
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 32卷
关键词
Friction stir welding; Constrained groove pressing; Aluminum; Mechanical properties; Al2O3; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; ALUMINUM; MICROSTRUCTURE; NANOCOMPOSITES; STRENGTH; BEHAVIOR; JOINT;
D O I
10.1016/j.jmrt.2024.07.198
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this investigation, two passes Constrained Groove Pressed (CGPed) Al1050 sheets went through Friction Stir Welding (FSW) by adding nano-sized Al2O3 particles. Then, the microstructure and mechanical properties of the welded joints, undergone various pass numbers and rotational to traverse speed (w/v) ratios, were presented. Findings showed all joints were fractured from the SZ, although HAZ softening happened due to grain growth in this region. The presence of the Al2O3 particles in the stir zone led to a fine and equiaxed grain structure, resulting from continuous dynamic recrystallization (CDRX) during the high-temperature welding process. This grain refinement contributed to an improvement in the mechanical properties of the joints, such as strength and microhardness. Employing two different w/v ratios resulted in a variety of thermal cycles during the welding procedure such that the peak temperature in the w/v of 70 and 25 r/mm reached 423 degrees C and 285 degrees C, respectively. Microstructure studies via optical observation and EBSD analysis illustrated that employing a higher w/v ratio and weld pass number resulted in more uniform particle distribution in the stir zone thanks to facilitating materials flow and incorporation during FSW. As a result, the three passes FSWed sample at the higher w/v ratio of 70 r/mm showed the most homogeneous particle distribution and finest grain structure in the SZ. This microstructure evolution was in reliable agreement with the mechanical performance of the joints. The three passes FSWed sample at the higher w/v ratio of 70 r/mm demonstrated the highest weld strength, microhardness, and %elongation compared to other FSWed joints. This sample showed an ultimate tensile strength (UTS) of 97 MPa and a %elongation of 16%, and its mean microhardness value had a 3.5% increase compared to the CGPed base metal. Conversely, the one pass FSWed sample at the lower w/v ratio of 25 r/mm represented the weakest mechanical properties due to cavities, defects, and agglomerated Al2O3 nanoparticles. The presence of nanoparticles was a decisive factor in microstructural evolution during the welding, thereby increasing the mechanical quality of the joints dependent upon their uniform dispersion, obtained by increasing the pass number and w/v ratio.
引用
收藏
页码:597 / 608
页数:12
相关论文
共 50 条
  • [31] Formation of Al/(Al13Fe4 + Al2O3) Nano-composites via Mechanical Alloying and Friction Stir Processing
    Azimi-Roeen, Ghasem
    Kashani-Bozorg, Seyed Farshid
    Nosko, Martin
    Nagy, Stefan
    Matko, Igor
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (02) : 471 - 482
  • [32] Effect of friction stir processing on the tribological performance of Steel/Al2O3 nanocomposites
    Ghasemi-Kahrizsangi, A.
    Kashani-Bozorg, S. F.
    Moshref-Javadi, M.
    SURFACE & COATINGS TECHNOLOGY, 2015, 276 : 507 - 515
  • [33] The Optimization of Gap Width Size During Friction Stir Welding of AA 6061-T6 with Al2O3 Particle Reinforcement
    Kesharwani, Rahul
    Jha, Kishor Kumar
    Imam, Murshid
    Sarkar, Chiranjit
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (13) : 6008 - 6027
  • [34] Enhanced structural integrity and tribological performance of Al6061–Al6082 alloys reinforced with TiB2 and Al2O3 via friction stir welding
    Ibrahim Sabry
    Mostafa S. S. El-Deeb
    The International Journal of Advanced Manufacturing Technology, 2025, 138 (7) : 2893 - 2910
  • [35] Laser butt joining of Al2O3 ceramic plates metallized by friction stir welding
    Sonomura, Hirosuke
    Katagiri, Kazuaki
    Yamaguchi, Takuto
    Tanaka, Keigo
    Ozaki, Tomoatsu
    Hasegawa, Yasunori
    Tanaka, Tsutomu
    Kakitsuji, Atsushi
    CERAMICS INTERNATIONAL, 2022, 48 (16) : 23381 - 23386
  • [36] Investigation of grain refinement in Al/Al2O3/B4C nano-composite produced by ARB
    Beni, Hossein Akbari
    Alizadeh, Morteza
    Ghaffari, Mohammad
    Amini, Rasool
    COMPOSITES PART B-ENGINEERING, 2014, 58 : 438 - 442
  • [37] Microstructure and mechanical properties of 7075 Al alloy based composites with Al2O3 nanoparticles
    Wu Ruirui
    Yuan Zheng
    Li Qiushu
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2017, 30 (06) : 337 - 340
  • [38] Texture analysis of a friction stir welded ultrafine grained Al-Al2O3 composite produced by accumulative roll-bonding
    Shamanian, Morteza
    Mohammadnezhad, Mahyar
    Szpunar, Jerzy
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 615 : 651 - 656
  • [39] Friction stir welding of an AA6061/Al2O3/20p reinforced alloy
    Marzoli, LM
    Strombeck, AV
    Dos Santos, JF
    Gambaro, C
    Volpone, LM
    COMPOSITES SCIENCE AND TECHNOLOGY, 2006, 66 (02) : 363 - 371
  • [40] Optimization of control factors on mechanical properties of friction stir processed AZ91B/Al2O3 nanocomposites
    Jusoh, Iberahin
    JOURNAL OF ENGINEERING RESEARCH, 2023, 11 (03): : 236 - 246