Effect of calcification roasting process on vanadium oxidation and extraction from vanadium titanomagnetite pellets via sulfuric acid Leaching: Mechanism and enhancement

被引:4
作者
Zheng, Yu [1 ]
Chen, Jianli [2 ]
Chen, Shuzhong [2 ]
Chen, Feng [1 ]
Wang, Shuai [1 ]
Guo, Yufeng [1 ]
Li, Hao [1 ]
Xu, Fuchun [1 ]
Zhang, Jinlai [1 ]
Yang, Lingzhi [1 ]
机构
[1] Cent South Univ, Sch Minerals Proc & Bioengn, Changsha 410083, Peoples R China
[2] LB Grp Co Ltd, Jiaozuo 454000, Peoples R China
关键词
Vanadium Extracting; Vanadium titanomagnetite pellet; Calcification roasting; Sulfuric acid leaching; Core-shell structure; MAGNETITE; TITANIUM; REDUCTION; RECOVERY; CONCENTRATE; BEHAVIOR;
D O I
10.1016/j.seppur.2024.128859
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Calcification roasting-sulfuric acid leaching is widely regarded as a clean and efficient alternative to sodium roasting-water leaching for directly vanadium extraction, and has been used industrially for vanadium extraction from vanadium slag. Nevertheless, limited research has been conducted on vanadium extraction from vanadium titanomagnetite (VTM). This knowledge gap contributes to suboptimal vanadium leaching rate and elevated iron leaching rate in the extraction process. This article systematically studied the effect of calcification roasting on vanadium oxidation and sulfuric acid leaching extraction vanadium from VTM pellets. The results reveal that the diminished vanadium leaching rate primarily stems from the dense pore structure of the roasted pellets and inadequate vanadium oxidation during calcification roasting process. Additionally, the formation of the core-- shell structure during the preheating stage directly contributes to insufficient vanadium oxidation. Lastly, a thorough analysis of the core-shell structure formation mechanism was conducted, leading to the identification of the optimal calcification roasting regime. With the conditions of preheating at 900 degrees C for 25 min followed by roasting at 1150 degrees C for 15 min, the complete elimination of the core-shell structure was achieved, and the average valence of vanadium was 4.77 in roasted pellets. Finally, the vanadium leaching rate reached 72.78 % by sulfuric acid leaching.
引用
收藏
页数:13
相关论文
共 50 条
[31]   Application of response surface methodology for roasting optimization in composite roasting-Acid leaching vanadium extraction process [J].
Wang, Xin ;
Xiang, Junyi ;
Pei, Guishang ;
Li, Lanjie ;
Huang, Qingyun ;
Lv, Xuewei .
CHEMICAL ENGINEERING RESEARCH & DESIGN, 2021, 172 :254-263
[32]   Efficient separation of vanadium, titanium, and iron from vanadium-bearing titanomagnetite by pressurized pyrolysis of ammonium chloride-acid leaching-solvent extraction process [J].
Bian, Zhenzhong ;
Feng, Yali ;
Li, Haoran ;
Wu, Hao .
SEPARATION AND PURIFICATION TECHNOLOGY, 2021, 255
[33]   Kinetics of Leaching Vanadium with Sulfuric Acid from carbonaceous shale containing vanadium [J].
Liu, Yan ;
Sun, Cong ;
Zhong, Weijun ;
Zhai, Yuchun .
ADVANCES IN METALLURGICAL AND MINING ENGINEERING, 2012, 402 :7-11
[34]   Selective extraction of vanadium from vanadium-titanium magnetite concentrates by non-salt roasting of pellets-H2SO4 leaching process [J].
Luo, Yi ;
Che, Xiaokui ;
Wang, Haixia ;
Zheng, Qi ;
Wang, Lei .
PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING, 2021, 57 (04) :36-47
[35]   Effective Extraction of Vanadium from Bauxite-Type Vanadium Ore Using Roasting and Leaching [J].
Zou, Kai ;
Xiao, Junhui ;
Liang, Guanjie ;
Huang, Wenxiao ;
Xiong, Wenliang .
METALS, 2021, 11 (09)
[36]   Effect of microwave irradiation and conventional calcification roasting with calcium hydroxide on the extraction of vanadium and chromium from high-chromium vanadium slag [J].
Gao, Huiyang ;
Jiang, Tao ;
Zhou, Mi ;
Wen, Jing ;
Li, Xi ;
Wang, Ying ;
Xue, Xiangxin .
MINERALS ENGINEERING, 2020, 145 (145)
[37]   Extraction of vanadium from sulfuric acid leaching solution of stone coal by ion exchange [J].
Yang, Xiao ;
Zhang, Yi-min ;
Bao, Shen-xu .
BULGARIAN CHEMICAL COMMUNICATIONS, 2015, 47 :99-104
[38]   Competitive extraction behaviors of vanadium and chromium in the sodium roasting - Water leaching process [J].
Xiang, Junyi ;
Lu, Xi ;
Rao, Hongru ;
Bai, Luwei ;
Huang, Qingyun ;
Lv, Xuewei .
SEPARATION AND PURIFICATION TECHNOLOGY, 2025, 363
[39]   Preparation of titanium mineral from vanadium titanomagnetite concentrates by hydrogen reduction and acid leaching [J].
Yan, Zheng-pei ;
Zhang, Ying ;
Zheng, Shi-li ;
Zhang, Yang ;
Sun, Pei ;
Song, Zi-wei ;
Safdar, Faiza ;
Qi, Tao .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2022, 32 (09) :3099-3109
[40]   The kinetics of vanadium extraction from spent hydroprocessing catalyst by leaching with sulfuric acid at atmospheric pressure [J].
Wang, Hongjun ;
Feng, Yali ;
Li, Haoran ;
Deng, Xiangyi ;
Kang, Jinxing .
METALLURGICAL RESEARCH & TECHNOLOGY, 2019, 116 (02)