Effect of calcification roasting process on vanadium oxidation and extraction from vanadium titanomagnetite pellets via sulfuric acid Leaching: Mechanism and enhancement

被引:4
作者
Zheng, Yu [1 ]
Chen, Jianli [2 ]
Chen, Shuzhong [2 ]
Chen, Feng [1 ]
Wang, Shuai [1 ]
Guo, Yufeng [1 ]
Li, Hao [1 ]
Xu, Fuchun [1 ]
Zhang, Jinlai [1 ]
Yang, Lingzhi [1 ]
机构
[1] Cent South Univ, Sch Minerals Proc & Bioengn, Changsha 410083, Peoples R China
[2] LB Grp Co Ltd, Jiaozuo 454000, Peoples R China
关键词
Vanadium Extracting; Vanadium titanomagnetite pellet; Calcification roasting; Sulfuric acid leaching; Core-shell structure; MAGNETITE; TITANIUM; REDUCTION; RECOVERY; CONCENTRATE; BEHAVIOR;
D O I
10.1016/j.seppur.2024.128859
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Calcification roasting-sulfuric acid leaching is widely regarded as a clean and efficient alternative to sodium roasting-water leaching for directly vanadium extraction, and has been used industrially for vanadium extraction from vanadium slag. Nevertheless, limited research has been conducted on vanadium extraction from vanadium titanomagnetite (VTM). This knowledge gap contributes to suboptimal vanadium leaching rate and elevated iron leaching rate in the extraction process. This article systematically studied the effect of calcification roasting on vanadium oxidation and sulfuric acid leaching extraction vanadium from VTM pellets. The results reveal that the diminished vanadium leaching rate primarily stems from the dense pore structure of the roasted pellets and inadequate vanadium oxidation during calcification roasting process. Additionally, the formation of the core-- shell structure during the preheating stage directly contributes to insufficient vanadium oxidation. Lastly, a thorough analysis of the core-shell structure formation mechanism was conducted, leading to the identification of the optimal calcification roasting regime. With the conditions of preheating at 900 degrees C for 25 min followed by roasting at 1150 degrees C for 15 min, the complete elimination of the core-shell structure was achieved, and the average valence of vanadium was 4.77 in roasted pellets. Finally, the vanadium leaching rate reached 72.78 % by sulfuric acid leaching.
引用
收藏
页数:13
相关论文
共 50 条
[21]   Effect of pretreatment on the extraction of valuable metal from vanadium-bearing titanomagnetite by ammonium sulfate roasting [J].
Bian, Zhenzhong ;
Feng, Yali ;
Li, Haoran ;
Zhang, Qian ;
Xu, Chenglong ;
Li, Haosheng ;
Li, Zhengyao .
METALLURGICAL RESEARCH & TECHNOLOGY, 2021, 118 (06)
[22]   Research on the Removal of Sodium from Vanadium Tailings by Calcification Roasting and NaOH Leaching [J].
Guo, Yufeng ;
Wang, Chao ;
Wang, Shuai ;
Chen, Feng ;
Wang, Xueyuan ;
An, Zhiwei ;
Yang, Lingzhi .
SUSTAINABILITY, 2022, 14 (15)
[23]   A sustainable chromium and vanadium extraction and separation process from high-chromium vanadium slag via synchronous roasting and asynchronous leaching [J].
Zhao, Weiduo ;
Zhao, Zhongwei ;
Xu, Yingpeng ;
Cao, Ziming ;
Li, Weilun ;
Zhao, Tianyu .
SEPARATION AND PURIFICATION TECHNOLOGY, 2025, 368
[24]   Effect of Cr2O3 addition on the oxidation induration mechanism of Hongge vanadium titanomagnetite pellets [J].
Li, Wei ;
Wang, Nan ;
Fu, Gui-qin ;
Chu, Man-sheng ;
Zhu, Miao-yong .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2018, 25 (04) :391-398
[25]   Simultaneous extraction of vanadium and titanium from vanadium slag using ammonium sulfate roasting-leaching process [J].
Zhang, Guoquan ;
Luo, Dongmei ;
Deng, Chenhui ;
Lv, Li ;
Liang, Bin ;
Li, Chun .
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 742 :504-511
[26]   Influence Mechanism of SiO2 on the Oxidation Behavior and Induration Process of Hongge Vanadium Titanomagnetite Pellets [J].
Fu, Guiqin ;
Li, Wei ;
Chu, Mansheng ;
Zhu, Miaoyong .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2020, 51 (01) :114-123
[27]   Leaching Kinetics of Vanadium and Chromium During Sulfuric Acid Leaching With Microwave and Conventional Calcification-Roasted High Chromium Vanadium Slag [J].
Gao, Huiyang ;
Jiang, Tao ;
Xu, Yingzhe ;
Wen, Jing ;
Xue, Xiangxin .
MINERAL PROCESSING AND EXTRACTIVE METALLURGY REVIEW, 2020, 41 (01) :22-31
[28]   Extraction Behavior of Vanadium and Chromium by Calcification Roasting-Acid Leaching from High Chromium Vanadium Slag: Optimization Using Response Surface Methodology [J].
Wen, Jing ;
Jiang, Tao ;
Liu, Yajing ;
Xue, Xiangxin .
MINERAL PROCESSING AND EXTRACTIVE METALLURGY REVIEW, 2019, 40 (01) :56-66
[29]   Extraction of Vanadium from High Calcium and High Phosphorus Vanadium Slag by Magnesiation Roasting-Acid Leaching [J].
Chen, Xin-Mian ;
Li, Hong-Yi ;
Tan, Jing ;
Cheng, Jie ;
Diao, Jiang ;
Xie, Bing .
RARE METAL TECHNOLOGY 2024, 2024, :453-461
[30]   Asynchronous extraction of vanadium and chromium from vanadium slag by stepwise sodium roasting-water leaching [J].
Li, Hong-Yi ;
Fang, Hai-Xing ;
Wang, Kang ;
Zhou, Wang ;
Yang, Zhao ;
Yan, Xiao-Man ;
Ge, Wen-Sun ;
Li, Qian-Wen ;
Xie, Bing .
HYDROMETALLURGY, 2015, 156 :124-135