Metakaolin-Based Geopolymers Filled with Industrial Wastes: Improvement of Physicochemical Properties through Sustainable Waste Recycling

被引:7
作者
Viola, Veronica [1 ]
D'Angelo, Antonio [1 ]
Vertuccio, Luigi [1 ]
Catauro, Michelina [1 ]
机构
[1] Univ Campania Luigi Vanvitelli, Dept Engn, Via Roma 29, I-81031 Aversa, Italy
关键词
geopolymers; waste recycling; infrared spectroscopy; thermogravimetry analysis; mechanical properties; antimicrobial properties; CEMENT; ASH; COMPLEXES; PRECURSOR; SURFACE; GLASS;
D O I
10.3390/polym16152118
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The increasing global demand for cement significantly impacts greenhouse gas emissions and resource consumption, necessitating sustainable alternatives. This study investigates fresh geopolymer (GP) pastes incorporating 20 wt.% of five industrial wastes-suction dust, red mud from alumina production, electro-filter dust, and extraction sludges from food supplement production and from partially stabilized industrial waste-as potential replacements for traditional cement. Consistent synthesis methods are used to prepare the geopolymers, which are characterized for their physicochemical, mechanical, and biological properties. Ionic conductivity and pH measurements together with integrity tests, thermogravimetry analysis (TGA), and leaching analysis are used to confirm the stability of the synthesized geopolymers. Fourier-transform Infrared (FT-IR) spectroscopy is used to follow geopolymerization occurrences. Results for ionic conductivity, pH, and integrity revealed that the synthesized GPs were macroscopically stable. TGA revealed that the main mass losses were ascribable to water dehydration and to water entrapped in the geopolymer networks. Only the GP filled with the powder of the red mud coming from alumina production experienced a mass loss of 23% due to a partial waste degradation. FT-IR showed a red shift in the main Si-O-(Si or Al) absorption band, indicating successful geopolymer network formations. Additionally, most of the GPs filled with the wastes exhibited higher compressive strength (37.8-58.5 MPa) compared to the control (22 MPa). Only the GP filled with the partially stabilized industrial waste had a lower mechanical strength as its structure was highly porous because of gas formation during geopolymerization reactions. Despite the high compressive strength (58.5 MPa) of the GP filled with suction dust waste, the concentration of Sb leached was 25 ppm, which limits its use. Eventually, all samples also demonstrated effective antimicrobial activity against Escherichia coli and Staphylococcus aureus due to the alkaline environment and the presence of metal cations able to react with the bacterial membranes. The findings revealed the possibility of recycling these wastes within several application fields.
引用
收藏
页数:17
相关论文
共 90 条
[51]   Effect of Sn precursor on the synthesis of SnO2 and Sb-doped SnO2 particles via polymeric precursor method [J].
Lopez Morales, Francisco ;
Zayas, Teresa ;
Contreras, Oscar E. ;
Salgado, Leonardo .
FRONTIERS OF MATERIALS SCIENCE, 2013, 7 (04) :387-395
[52]   The pore structure and permeability of alkali activated fly ash [J].
Ma, Y. ;
Hu, J. ;
Ye, G. .
FUEL, 2013, 104 :771-780
[53]   Improvement of the reactivity of soda-lime-silica glass solution as a hardener for producing geopolymer materials [J].
Melele, Sorelle J. K. ;
Banenzoue, Charles ;
Fotio, Daniel ;
Tchakoute, Herve K. ;
Ruscher, Claus H. ;
Nanseu, Charles P. N. .
SN APPLIED SCIENCES, 2019, 1 (10)
[54]   Infrared spectra of surface nitrates: Revision of the current opinions based on the case study of ceria [J].
Mihaylov, M. Y. ;
Zdravkova, V. R. ;
Ivanova, E. Z. ;
Aleksandrov, H. A. ;
St Petkov, P. ;
Vayssilov, G. N. ;
Hadjiivanov, K., I .
JOURNAL OF CATALYSIS, 2021, 394 :245-258
[55]  
Nakamoto K., 2006, Handb. Vib. Spectrosc, DOI [DOI 10.1002/9780470027325.S4104, 10.1002/0470027320.s4104, DOI 10.1002/0470027320.S4104, 10.1002/]
[56]   Alkaline pH homeostasis in bacteria: New insights [J].
Padan, E ;
Bibi, E ;
Ito, M ;
Krulwich, TA .
BIOCHIMICA ET BIOPHYSICA ACTA-BIOMEMBRANES, 2005, 1717 (02) :67-88
[57]   The architecture of the Gram-positive bacterial cell wall [J].
Pasquina-Lemonche, L. ;
Burns, J. ;
Turner, R. D. ;
Kumar, S. ;
Tank, R. ;
Mullin, N. ;
Wilson, J. S. ;
Chakrabarti, B. ;
Bullough, P. A. ;
Foster, S. J. ;
Hobbs, J. K. .
NATURE, 2020, 582 (7811) :294-+
[58]   State of the art on the application of waste materials in geopolymer concrete [J].
Podolsky, Z. ;
Liu, J. ;
Dinh, H. ;
Doh, J. H. ;
Guerrieri, M. ;
Fragomeni, S. .
CASE STUDIES IN CONSTRUCTION MATERIALS, 2021, 15
[59]   Strength development of recycled concrete aggregate stabilized with fly ash-rice husk ash based geopolymer as pavement base material [J].
Poltue, Theerapruet ;
Suddeepong, Apichat ;
Horpibulsuk, Suksun ;
Samingthong, Wisanukhorn ;
Arulrajah, Arul ;
Rashid, Ahmad Safuan A. .
ROAD MATERIALS AND PAVEMENT DESIGN, 2020, 21 (08) :2344-2355
[60]  
Ricciotti L, 2017, ENVIRONMENTS, V4, DOI 10.3390/environments4040091