The Effect of Detonation Frequency on the Linear Reciprocating Wear Behavior of Detonation Sprayed Ni-20%Cr Coatings at Elevated Temperatures

被引:0
|
作者
Prasad, Rahul [1 ]
Purushotham, N. [1 ]
Kumar, G. V. Preetham [1 ]
Babu, P. Suresh [2 ]
Sivakumar, G. [2 ]
Rajasekaran, B. [1 ]
机构
[1] Natl Inst Technol, Dept Met & Mat Engn, Karnataka NITK, Surathkal 575025, India
[2] Int Adv Res Ctr Powder Met & New Mat, Hyderabad 500005, India
关键词
counter material; linear reciprocating; residual stress; spray frequency; worn surface; OXIDATION BEHAVIOR; RESIDUAL-STRESSES; TRIBOLOGICAL PERFORMANCE; MECHANICAL-PROPERTIES; COMPOSITE COATINGS; NICKEL; STEEL; CONTACT;
D O I
10.1007/s11665-024-10043-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The study explores the impact of detonation frequency (3 and 6 Hz) on the temperature-dependent linear reciprocating wear behavior of Ni-20%Cr coatings deposited by detonation spraying on a nickel-based superalloy (IN718). Dry sliding experiments were carried out at both ambient (25 degrees C) and high (420 degrees C) temperatures, using an alumina (Al2O3) ball as the counter material and different loads (5, 10, and 20 N). HV0.2 microhardness indentations were used to test material hardness variations attributed to heat exposure. X-ray diffraction (XRD), Raman spectroscopy, and field emission scanning electron microscopy with energy-dispersive spectroscopy (FESEM with EDS) were used to investigate the wear characteristics and mechanisms. Furthermore, surface roughness and profiles of worn surfaces (including track depth, breadth, and wear volume) enabled the calculation of wear rates using confocal optical 3D profilometry. The results showed the 6 Hz Ni-20%Cr coating showed better wear resistance than the 3 Hz coating. However, a higher wear rate and low friction coefficient at 420 degrees C were observed due to partial oxide particles, which were insufficient to restrict direct ball-to-metal contact. The research delves into wear maps, tribolayer formation, wear mechanisms, and sub-mechanisms.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] EFFECT OF LASER SURFACE MELTING ON MICROSTRUCTURE OF COLD SPRAYED Ni20Cr COATINGS
    Sobon, D.
    ARCHIVES OF METALLURGY AND MATERIALS, 2021, 66 (03) : 853 - 860
  • [32] Effect of heat treatment on wear performance of nanostructured WC-Ni/Cr HVOF sprayed coatings
    Ben Mahmud T.
    Farrokhzad M.A.
    Khan T.I.
    Tribology Online, 2017, 12 (01) : 18 - 28
  • [33] Wear resistance of Fe66Cr10Nb5B19 detonation coatings under dry linearly reciprocating conditions and nanoscratch test
    Kuchumova, I. D.
    Shikalov, V. S.
    Batraev, I. S.
    Filippov, A. A.
    Koga, G. Yu.
    LETTERS ON MATERIALS, 2023, 13 (02): : 138 - 142
  • [34] Elevated temperatures erosion wear behavior of HVOF sprayed WC-Co-Cr/Mo coatings on Ti6Al4V substrate
    Behera, Netrananda
    Medabalimi, Subba Rao
    Ramesh, M. R.
    SURFACE & COATINGS TECHNOLOGY, 2023, 470
  • [35] Hot Corrosion Studies on Detonation-Gun-Sprayed NiCrAlY and 80Ni-20Cr Coatings on Alloy X22CrMoV12-1 at 600°C
    Subramani, P.
    Padgelwar, Nirmal
    Shetty, Sanket
    Pandit, Anirudha
    Sreenivasulu, V.
    Arivazhagan, N.
    Duoli, W. U.
    Manikandan, M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (06) : 1639 - 1642
  • [36] A Study on the Cyclic Oxidation Behavior of Detonation-Gun-Sprayed Ni-5Al Coatings on Inconel-718 at 900 A°C
    Saladi, Sekar
    Menghani, Jyoti
    Prakash, Satya
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (12) : 4394 - 4403
  • [37] A Study on the Cyclic Oxidation Behavior of Detonation-Gun-Sprayed Ni-5Al Coatings on Inconel-718 at 900 °C
    Sekar Saladi
    Jyoti Menghani
    Satya Prakash
    Journal of Materials Engineering and Performance, 2014, 23 : 4394 - 4403
  • [38] Hot Corrosion Studies on Detonation-Gun-Sprayed NiCrAlY and 80Ni–20Cr Coatings on Alloy X22CrMoV12-1 at 600 °C
    P. Subramani
    Nirmal Padgelwar
    Sanket Shetty
    Anirudha Pandit
    V. Sreenivasulu
    N. Arivazhagan
    W. U. Duoli
    M. Manikandan
    Transactions of the Indian Institute of Metals, 2019, 72 : 1639 - 1642
  • [39] DETONATION DEPOSITED Fe-Al COATINGS PART I: MORPHOLOGY OF Ni(Al) AND Cr(Ni) TRANSITION LAYERS AND COATINGS OF Fe-Al TYPE SPRAYED ONTO CARBON STEEL SUBSTRATE
    Pawlowski, A.
    Senderowski, C.
    Bojar, Z.
    Faryna, M.
    ARCHIVES OF METALLURGY AND MATERIALS, 2010, 55 (04) : 1061 - 1071
  • [40] Sliding wear behaviour of nanocrystalline Cr3C2-25(Ni20Cr) coatings at elevated temperature
    Roy, M
    Pauschitz, A
    Franek, F
    TRIBOLOGICAL RESEARCH AND DESIGN FOR ENGINEERING SYSTEMS, 2003, : 141 - 149