Analysis of the influence of girth weld strength matching on pipe deformation mode and failure pattern

被引:0
作者
Wu, Mingchang [1 ]
Wang, Hankui [2 ]
Wang, Leilei [1 ]
Guo, Lei [1 ]
Song, Ming [2 ]
He, Renyang [2 ]
机构
[1] PipeChina West East Gas Pipeline Co, Shanghai, Peoples R China
[2] China Special Equipment Inspect & Res Inst, Beijing 100013, Peoples R China
来源
JOURNAL OF PIPELINE SCIENCE AND ENGINEERING | 2024年 / 4卷 / 03期
关键词
Pipeline; Girth weld; Tensile strain capacity; Strength matching;
D O I
10.1016/j.jpse.2024.100183
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
A theory model with two kinds of material, which are used to describe the axis stress strain relationship of the pipe segment and girth weld joints, is proposed for the pipeline axial deformation analysis, and a pipeline deformation diagram is composed for the axis deformation combination within the pipeline design limit. According to the pipeline deformation diagram, it is found that the strength of the pipe segment at the design limit sigma(A)(b) plays a key role in the strength matching discussion. The pipeline axis deformation could be classified as three categories based on the yield strength sigma wY, ultimate tensile strength sigma wcritof the weld joints and the pipe design strength sigma(A)(b), which are sigma(Y )(w)> sigma(A)(b), sigma(crit)(w) >= sigma(A )(b)>= sigma(Y)(w) and sigma(A )(b)> sigma(crit)(w). For sigma(Y )(w)> sigma(A)(b), the axis plastic deformation will distribute along the pipe segment and this is the ideal states for the pipeline. For sigma(A )(b)> sigma(crit)(w), the girth weld may fail as stress rupture with tensile strain as low as 0.003. For sigma(crit)(w) >= sigma(A )(b)>= sigma(Y)(w), the weld joint may endure the plastic deformation, and the material properties of the weld joint may change, such as the toughness may decrease. Charpy-V impact test have shown that the toughness decreases 35 % for 2 % deformation for the weld joints welded by FCAW-S. In this scenario, the girth weld may break up as brittle fracture due to the toughness decrease. This model could be used to explain the girth weld failures, optimize the strength matching and control the risk, especially for the buried high strength pipeline of the high stress locations.
引用
收藏
页数:8
相关论文
共 17 条
  • [1] Anderson TL, 2005, FRACTURE MECH FUNDAM
  • [2] [Anonymous], 2001, Guidelines for the Design of Buried Steel Pipe
  • [3] API, 2023, Specification for Line Pipe
  • [4] Boniszewski T., 1992, Self Shielded Arc Welding, P80
  • [5] Canada Energy Regulator, 2020, SA 2020-01
  • [6] DISLOCATION THEORY OF YIELDING AND STRAIN AGEING OF IRON
    COTTRELL, AH
    BILBY, BA
    [J]. PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON SECTION A, 1949, 62 (349): : 49 - 62
  • [7] Glover A., 2002, PIP DREAM C APPL EV, P33
  • [8] Gray J.M., 2016, Evolution of microalloyed steels since microalloying '75 with specific emphasis on linepipe and plate, P53
  • [9] Strain ageing embrittlement behaviour of X80 self-shielded flux-cored girth weld metal
    Guo, Lei
    Su, Xin
    Dai, Lianshuang
    Wang, Leilei
    Sun, Qiaofei
    Fan, Chaohai
    Wang, Yalei
    Li, Xueda
    [J]. MATERIALS TECHNOLOGY, 2023, 38 (01)