Influence mechanisms of ultraviolet irradiation aging on DC surface discharge properties of silicone rubber in dry and humid air

被引:1
|
作者
Li, Zhen [1 ,2 ,3 ]
Sun, Lei [1 ]
Liu, Songchen [1 ]
Li, Jinhao [1 ]
Ma, Zhiqin [3 ]
Cai, Linglong [3 ]
Wang, Zhongao [3 ]
Liu, Ji [1 ]
Li, Shengtao [2 ]
机构
[1] Harbin Univ Sci & Technol, Key Lab Engn Dielect & Its Applicat, Minist Educ, Harbin 150080, Heilongjiang, Peoples R China
[2] Xi An Jiao Tong Univ, State Key Lab Elect Insulat & Power Equipment, Xian 710049, Shaanxi, Peoples R China
[3] Elect Power Res Inst Guangdong Power Grid Co LTD, Guangdong Prov Key Lab Elect Power Equipment Relia, Guangzhou 510080, Guangdong, Peoples R China
基金
中国国家自然科学基金;
关键词
Surface discharge; Ultraviolet irradiation aging; Silicone rubber; Degradation and oxidization; Polarization; FLASHOVER PERFORMANCE; LEAKAGE CURRENT; WAVE-FUNCTION; INSULATORS;
D O I
10.1016/j.apsusc.2024.161107
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the modern DC electrical transmission system, high-energy photons interact with silicone rubber (SIR) chains during long-term ultraviolet (UV) irradiation, it degrades the surface properties and triggers surface discharge (flashover) along the SIR-air interface, threatening the secure operation of the advanced electrical equipment. To further comprehend how UV-aging influences the flashover performance, in this work, the chemical bonds, surface charge transport parameters, and flashover performance of UV-aged SIR samples are characterized, and the influence mechanisms of UV-aging on surface discharge in dry and humid air are comprehensively clarified through the investigation from "molecular-mesoscopic-macroscopic" scales. The results indicate both degradation and oxidization reactions occur during UV-aging. The degraded molecular chains dominate the discharge in dry air, while oxidization reactions determine the discharge in humid environment: The degradation reactions reduce the surface trap depth and increase surface conductivity, leading to large surface leakage current and surface charge dissipation rate, causing flashover voltage in dry air increases and decreases as UV-aging time increasing. The oxidization of the chains introduces -OH and -COOH groups into chains, enhancing permittivity and adsorbing H2O molecules, significantly increasing surface leakage current, causing surface discharge voltage in humid air to decrease as UV-aging time increases.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Influence of Ultraviolet Irradiation in Vacuum on DC Breakdown and Surface Flashover Characteristics of Silicone Rubber
    Li Z.
    Wang W.
    Li S.
    Min D.
    Chen L.
    Li X.
    Gaodianya Jishu/High Voltage Engineering, 2019, 45 (09): : 2919 - 2927
  • [2] Surface Degradation of Silicone Rubber Nanocomposites Due to DC Corona Discharge
    Vas, Joseph Vimal
    Thomas, M. Joy
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2014, 21 (03) : 1175 - 1182
  • [3] Research on Ultraviolet Aging Properties of Modified Silicone Rubber for Composite Insulator
    Peng Jing
    Liu Zhiqiang
    Wei Peng
    Jing Qian
    Wang Chunjie
    Liu Yuxin
    PROCEEDINGS OF 2020 INTERNATIONAL SYMPOSIUM ON ELECTRICAL INSULATING MATERIALS (ISEIM 2020), 2020, : 202 - 205
  • [4] Influence of Silicone Rubber Coating on the Characteristics of Surface Streamer Discharge
    Meng, Xiaobo
    Wang, Liming
    Mei, Hongwei
    Zhang, Chuyan
    POLYMERS, 2021, 13 (21)
  • [5] Influence of thermal aging on the properties of EPDM/silicone rubber blends
    Chung, YK
    Lee, SG
    Cho, BR
    Choi, KY
    POLYMER-KOREA, 2005, 29 (02) : 166 - 171
  • [6] Comparative Research on Aging Properties of HTV Silicone Rubber via Outdoor Electric Aging and Ultraviolet Accelerated Aging
    Qin, Yongxiong
    Fu, Jia
    Yu, Lan
    Yang, Zirong
    Guo, Wenyi
    BIOTECHNOLOGY, CHEMICAL AND MATERIALS ENGINEERING II, PTS 1 AND 2, 2013, 641-642 : 333 - +
  • [7] Electrical study of DC positive corona discharge in dry and humid air containing carbon dioxide
    Lachaud, S
    Loiseau, JF
    EUROPEAN PHYSICAL JOURNAL-APPLIED PHYSICS, 2003, 24 (01): : 67 - 74
  • [8] Influence of Precise Modification of Nano-TiO2 Surface on DC Insulation Properties of Silicone Rubber
    Zhou Y.
    Gao D.
    Zhu X.
    Zhang L.
    Huang X.
    Gaodianya Jishu/High Voltage Engineering, 2023, 49 (12): : 4879 - 4889
  • [9] Effect of DC Corona Aging on Properties of HTV Silicone Rubber and Alicyclic Epoxy Resin
    Huang X.
    Yang W.
    Tian Y.
    Yuan Z.
    Dianwang Jishu/Power System Technology, 2020, 44 (11): : 4454 - 4463
  • [10] Influence of thermal oxygen aging on dielectric and mechanical properties of liquid silicone rubber
    Chen Q.-G.
    Shang N.-Q.
    Wei X.-Z.
    Dianji yu Kongzhi Xuebao/Electric Machines and Control, 2020, 24 (04): : 141 - 148