Comparative Evaluation of Two Different Preparation Designs and Materials on the Fracture Resistance of Laminate Veneers: An In Vitro Study

被引:0
|
作者
Soni, Pranjal S. [1 ]
Sanyal, Pronob [1 ]
机构
[1] Krishna Vishwa Vidyapeeth Deemed Univ, Sch Dent Sci, Dept Prosthodont & Crown & Bridge, Karad, India
关键词
instron universal testing machine; tooth preparation for laminate veneer; fracture resistance; upcera; BITE FORCE; PORCELAIN;
D O I
10.7759/cureus.66811
中图分类号
R5 [内科学];
学科分类号
1002 ; 100201 ;
摘要
Introduction Laminate veneers are thin porcelain or composite resin shells bonded to the front of teeth for cosmetic enhancement. The design of the tooth preparation is crucial; it involves minimal enamel removal to ensure a proper fit and strong bond. This careful preparation increases the veneers' fracture resistance by preserving tooth structure and evenly distributing stress, ensuring durability and natural appearance. Aim Our aim was to determine the fracture resistance of two preparation designs with two different materials for the fabrication of laminate veneers. Materials and methods An in vitro study was conducted on 40 laminate veneers divided into two groups based on the material used: Group 1 (Cerec Tessera (Dentsply Sirona, Charlotte, NC, USA)) and Group 2 (Upcera, Shenzhen, China). Each group was further divided into two sub-groups based on tooth preparation designs: butt joint and feather edge. The fracture resistance of these veneers following thermocycling was determined, and the mode of fracture was evaluated using a stereomicroscope. Results Feather edge preparation with Cerec Tessera laminate veneer restoration demonstrated the highest fracture resistance at 111.5 N, followed by butt joint preparation with Cerec Tessera laminate veneer restoration, which showed a fracture resistance of 90.8 N. The study identified laminate fractures as the most common type of fracture observed in the veneer restorations, followed by cement interface fractures. Conclusion The study suggests that the feather edge preparation design contributed to higher fracture resistance compared to the butt joint design. This finding aligns with the idea that modifying the preparation design can have a significant impact on the overall strength and durability of veneer restorations. The use of Cerec Tessera, especially in combination with the feather edge design, yielded the maximum fracture resistance.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] Fracture Resistance of Ceramic Veneers with Different Preparation Designs
    Akoglu, Burcin
    Gemalmaz, Deniz
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (05): : 380 - 384
  • [2] Ceramic laminate veneers: effect of preparation design and ceramic thickness on fracture resistance and marginal quality in vitro
    Uwe Blunck
    Sabine Fischer
    Jan Hajtó
    Stefan Frei
    Roland Frankenberger
    Clinical Oral Investigations, 2020, 24 : 2745 - 2754
  • [3] Effect of preparation design on fracture resistance of molars restored with occlusal veneers of different CAD-CAM materials: an in vitro study
    Taha, Ahmed Ismail
    Hafez, Mona Elshirbini
    BMC ORAL HEALTH, 2024, 24 (01):
  • [4] Ceramic laminate veneers: effect of preparation design and ceramic thickness on fracture resistance and marginal quality in vitro
    Blunck, Uwe
    Fischer, Sabine
    Hajto, Jan
    Frei, Stefan
    Frankenberger, Roland
    CLINICAL ORAL INVESTIGATIONS, 2020, 24 (08) : 2745 - 2754
  • [5] Fracture resistance and marginal discrepancy of porcelain laminate veneers influenced by preparation design and restorative material in vitro
    Lin, Tai-Min
    Liu, Perng-Ru
    Ramp, Lance C.
    Essig, Milton E.
    Givan, Daniel A.
    Pan, Yu-Hwa
    JOURNAL OF DENTISTRY, 2012, 40 (03) : 202 - 209
  • [6] Laboratory study of fracture resistance and failure mode of porcelain laminate veneers with different preparation depths in endodontically treated teeth
    Dehpagaee, Amirhossein Samiee
    Tavakol, Omid
    AMERICAN JOURNAL OF DENTISTRY, 2024, 37 (02): : 106 - 112
  • [7] Long-term survival of porcelain laminate veneers using two preparation designs: A retrospective study
    Smales, RJ
    Etemadi, S
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2004, 17 (03) : 323 - 326
  • [8] An in vitro comparative evaluation of fracture resistance of endodontically treated teeth obturated with different materials
    Chadha, Rupali
    Taneja, Sonali
    Kumar, Mohit
    Sharma, Mohit
    CONTEMPORARY CLINICAL DENTISTRY, 2010, 1 (02) : 70 - 72
  • [9] Evaluation of Fracture Resistance of Occlusal Veneers Made of Different Types of Materials Depending on Their Thickness
    Czechowski, Lukasz
    Dejak, Beata
    Konieczny, Bartlomiej
    Krasowski, Michal
    MATERIALS, 2023, 16 (17)
  • [10] Comparative Evaluation of Fracture Resistance of Composite Core Buildup Materials: An In Vitro Study
    Pande, Deepmala
    Benjamin, Niharika
    Rani, Vishakha
    Hina, Malik
    Haldar, Shreya
    Nirmal, Harni
    Gole, Shivani
    Ali, Md Sadique
    CUREUS JOURNAL OF MEDICAL SCIENCE, 2024, 16 (06)