Numerical and experimental investigation on flexural properties of selective laser melting (SLM) manufactured strut lattices structures from Ti-6Al-4V and Inconel 625

被引:3
作者
Condruz, Mihaela Raluca [1 ]
Badea, Teodor Adrian [1 ]
Paraschiv, Alexandru [1 ]
机构
[1] Romanian Res & Dev Inst Gas Turbines COMOTI, 220D Iuliu Maniu Ave, Bucharest 061126, Romania
关键词
Lattice structures; Three-point bending; Finite element analysis; Microstructure; Selective laser melting; MICROSTRUCTURE EVOLUTION; HEAT-TREATMENTS; ALLOY; BEHAVIOR;
D O I
10.1016/j.mtcomm.2024.110150
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Lattice structures hold a significant importance in the aerospace industry due to their ability to tailor the physical, thermal, and mechanical properties of complex components for optimal performance. This study is focused on evaluating the flexural properties of four lattice configurations - re-entrant, truncated octahedron, Kelvin, and octet cells - through static finite element analysis (FEA) and experimental three-point bending tests, as well as examining their microstructural features (as they affect the materials' mechanical properties). Highperformance alloys used for gas turbines components manufacturing, Ti-6Al-4 V and Inconel 625, were fabricated using selective laser melting (SLM) process. The necessity of this research resulted from the lack of information in the scientific literature regarding flexural properties of various additive manufactured cell types and metallic materials. The aim was to compile data that could be used to create a comprehensive database for various industrial applications. Findings from both simulations and experimental analyses indicated that the octet cell had the highest performance, with experimentally measured flexural strengths of 878 MPa for Ti-6Al4V, respective 674 MPa for Inconel 625. Contrarily, the re-entrant cell exhibited the lowest performance, with flexural strengths of 125 MPa for Ti-6Al-4V and 116 MPa for Inconel 625. Failure in the re-entrant cells was attributed to the bending fracture of vertical rods at the connecting nodes or lattice struts, while other cell types experienced damage through a combination of bending and shear mechanisms. Dimensional deviations observed in all specimens were attributed to defects such as surface roughness, the stair-stepping effect, and internal stresses.
引用
收藏
页数:16
相关论文
共 50 条
[41]   Microstructure and inclusion of Ti-6Al-4V fabricated by selective laser melting [J].
Huang, Qianli ;
Hu, Ningmin ;
Yang, Xing ;
Zhang, Ranran ;
Feng, Qingling .
FRONTIERS OF MATERIALS SCIENCE, 2016, 10 (04) :428-431
[42]   Achieving high strength and ductility in selective laser melting Ti-6Al-4V alloy by laser shock peening [J].
Lv, Jiming ;
Luo, Kaiyu ;
Lu, Haifei ;
Wang, Zhao ;
Liu, Jiajun ;
Lu, Jinzhong .
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 899
[43]   Quasi-static analysis of mechanical properties of Ti6Al4V lattice structures manufactured using selective laser melting [J].
Feng, Qixiang ;
Tang, Qian ;
Liu, Ying ;
Setchi, Rossi ;
Soe, Shwe ;
Ma, Shuai ;
Bai, Long .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 94 (5-8) :2301-2313
[44]   Microstructure and Mechanical Properties of Ti-6Al-4V Fabricated by Selective Laser Melting [J].
Simonelli, Marco ;
Tse, Yau Yau ;
Tuck, Christopher .
TMS 2012 141ST ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND INTERFACES, 2012, :863-870
[45]   Evaluation of fatigue crack propagation behaviour in Ti-6Al-4V manufactured by selective laser melting [J].
Walker, K. F. ;
Liu, Q. ;
Brandt, M. .
INTERNATIONAL JOURNAL OF FATIGUE, 2017, 104 :302-308
[46]   The effect of oxygen pickup during selective laser melting on the microstructure and mechanical properties of Ti-6Al-4V lattices [J].
Velasco-Castro, M. ;
Hernandez-Nava, E. ;
Figueroa, I. A. ;
Todd, I. ;
Goodall, R. .
HELIYON, 2019, 5 (12)
[47]   A processing diagram for high-density Ti-6Al-4V by selective laser melting [J].
Wang, Yinmin ;
Kamath, Chandrika ;
Voisin, Thomas ;
Li, Zan .
RAPID PROTOTYPING JOURNAL, 2018, 24 (09) :1469-1478
[48]   Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting [J].
Yang, Jingjing ;
Yu, Hanchen ;
Yin, Jie ;
Gao, Ming ;
Wang, Zemin ;
Zeng, Xiaoyan .
MATERIALS & DESIGN, 2016, 108 :308-318
[49]   Experimental analysis of Selective Laser Melting process for Ti-6Al-4V turbine blade manufacturing [J].
Caiazzo, Fabrizia ;
Cardaropoli, Francesco ;
Alfieri, Vittorio ;
Sergi, Vincenzo ;
Cuccaro, Luigi .
XIX INTERNATIONAL SYMPOSIUM ON HIGH-POWER LASER SYSTEMS AND APPLICATIONS 2012, 2013, 8677
[50]   Mechanical and Electrochemical Properties Comparison of Additively Manufactured Ti-6Al-4V Alloys by Electron Beam Melting and Selective Laser Melting [J].
Romero Resendiz, Liliana ;
Sanchez Cano, Tonantzin ;
Naeem, Muhammad ;
Rehman, Asif Ur ;
Salamci, Elmas ;
Torres Mendoza, Vianey ;
Degalez Duran, Eduardo ;
Bazan Diaz, Lourdes ;
Salamci, Metin U. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (17) :9028-9038