Effect of fly ash and gypsum on drying shrinkage and mechanical properties of one-part alkali-activated slag mortar

被引:0
作者
Chen, Haiming [1 ,2 ]
Zhang, Yadong [1 ]
Chen, Jie [1 ]
Qin, Ziguang [1 ]
Wu, Peng [1 ]
机构
[1] Anhui Univ Sci & Technol, Sch Civil Engn & Architecture, Huainan 232001, Peoples R China
[2] Anhui Univ Sci & Technol, Minist Educ, Engn Res Ctr Underground Mine Construct, Huainan, Peoples R China
基金
中国国家自然科学基金;
关键词
compressive strength; drying shrinkage; fly ash; gypsum; one-part alkali-activated slag; STRENGTH DEVELOPMENT; GEOPOLYMER MIXES; WORKABILITY LOSS; SODIUM-SILICATE; EARLY HYDRATION; CONCRETE; DURABILITY; SIZE; DOSAGE; HEAT;
D O I
10.1002/suco.202400006
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
One-part alkali-activated materials can be processed into semi-finished products by mixing a solid activator with the powder. They only require the addition of water, which greatly improves their commercial feasibility. So, we used one-part alkali-activated slag mortar to investigate the effects of the dosages of the activator (sodium metasilicate), fly ash (FA), and gypsum on its fluidity, flexural strength, compressive strength, and drying shrinkage. The microscopic mechanisms of the mortar were analyzed using scanning electron microscopy and x-ray diffraction. The below conclusions were drawn. First, the drying shrinkage and compressive strength of the mortar gradually increased with the increase of the activator dosage. Second, the drying shrinkage of the mortar initially decreased and then increased as increasing FA substitution, while the compressive strength decreased gradually in the early stage and then increased and decreased in the later stage. Lastly, by increasing the gypsum dosage, the drying shrinkage of the mortar was significantly reduced. However, the compressive strength gradually decreased. Besides, when adding 20% of FA and 2.4% of gypsum, it was found that ettringite, which underwent expansion, formed in the system. This not only reduced the drying shrinkage by 25.3% but also increased the compressive strength by 1.3%. Furthermore, our investigation has led to the development of a low-shrinkage one-part alkali-activated slag and FA mortar, which not only facilitates the recycling of solid waste materials but also presents commendable environmental and economic advantages.
引用
收藏
页码:1275 / 1288
页数:14
相关论文
共 72 条
[21]   Effect of pore size distribution on drying shrinkage of alkali-activated slag concrete [J].
Collins, F ;
Sanjayan, JG .
CEMENT AND CONCRETE RESEARCH, 2000, 30 (09) :1401-1406
[22]   One part alkali activated materials: A state-of-the-art review [J].
Elzeadani, M. ;
Bompa, D. V. ;
Elghazouli, A. Y. .
JOURNAL OF BUILDING ENGINEERING, 2022, 57
[23]   The effect of silica availability on the mechanism of geopolymerisation [J].
Hajimohammadi, Ailar ;
Provis, John L. ;
van Deventer, Jannie S. J. .
CEMENT AND CONCRETE RESEARCH, 2011, 41 (03) :210-216
[24]   One-Part Geopolymer Mixes from Geothermal Silica and Sodium Aluminate [J].
Hajimohammadi, Ailar ;
Provis, John L. ;
van Deventer, Jannie S. J. .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2008, 47 (23) :9396-9405
[25]   Effect of paste aggregate ratio and curing methods on the performance of one-part alkali-activated concrete [J].
Haruna, Sani ;
Mohammed, Bashar S. ;
Wahab, M. M. A. ;
Liew, M. S. .
CONSTRUCTION AND BUILDING MATERIALS, 2020, 261
[26]   Insulating and fire-resistant performance of slag and brick powder based one-part alkali-activated lightweight mortars [J].
Koksal, Fuat ;
Bayraktar, Oguzhan Yavuz ;
Bodur, Burak ;
Benli, Ahmet ;
Kaplan, Gokhan .
STRUCTURAL CONCRETE, 2023, 24 (03) :3128-3146
[27]   Effects of dosage and modulus of water glass on early hydration of alkali-slag cements [J].
Krizan, D ;
Zivanovic, B .
CEMENT AND CONCRETE RESEARCH, 2002, 32 (08) :1181-1188
[28]   Robustness to water and temperature, and activation energies of metakaolin-based geopolymer and alkali-activated slag binders [J].
Lahalle, Hugo ;
Benavent, Virginie ;
Trincal, Vincent ;
Wattez, Thomas ;
Bucher, Raphael ;
Cyr, Martin .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 300 (300)
[29]   Setting and mechanical properties of alkali-activated fly ash/slag concrete manufactured at room temperature [J].
Lee, N. K. ;
Lee, H. K. .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 47 :1201-1209
[30]   Influence of fly ash and its mean particle size on certain engineering properties of cement composite mortars [J].
Li, GY ;
Wu, XZ .
CEMENT AND CONCRETE RESEARCH, 2005, 35 (06) :1128-1134