Chloride Corrosion Process of Concrete with Different Water-Binder Ratios under Variable Temperature Drying-Wetting Cycles

被引:0
|
作者
Wang, Lei [1 ]
Chen, Chunhong [1 ,2 ]
Liu, Ronggui [2 ]
Zhu, Pinghua [1 ]
Liu, Hui [1 ,3 ]
Jiang, Hongwei [1 ]
Yu, Jiang [1 ]
机构
[1] Changzhou Univ, Sch Urban Construct, Changzhou 213164, Peoples R China
[2] Jiangsu Univ, Fac Civil Engn & Mech, Zhenjiang 212013, Peoples R China
[3] Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China
基金
中国国家自然科学基金;
关键词
water-binder ratio; variable temperature; drying-wetting cycles; mechanical properties; free chloride content; erosion depth; REINFORCED-CONCRETE; BINDING-CAPACITY; HYDRATION PRODUCTS; SERVICE LIFE; DIFFUSION; DURABILITY; SALT; PENETRATION; COEFFICIENTS; TRANSPORT;
D O I
10.3390/ma17102263
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, four water-binder ratios (w/b) of 0.29, 0.33, 0.39, and 0.46 were designed. A variable test temperature was implemented in the drying-wetting cycle test according to the temperature fluctuations in the actual service environment, and the constant temperature test was established as the control group. The mechanical properties and chloride corrosion resistance of concrete with different w/b ratios under variable temperature drying-wetting cycles, as well as the microstructure changes, phase composition, and damage mechanism inside the concrete, were investigated. The results showed that the mechanical properties of concrete increased first and then decreased with drying-wetting cycles increasing, whereas the chloride corrosion resistance continued to decline. A higher w/b exacerbated the deterioration of the concrete performance. A higher w/b increased the porosity, chloride diffusion depth, and chloride content, thus reducing the resistance of chloride corrosion. Compared with w/b = 0.29, the compressive strength, splitting tensile strength, mass, and relative dynamic elasticity modulus of w/b = 0.46 exposed to 60 drying-wetting cycles decreased by 54.50%, 52.44%, 0.96%, and 6.50%, respectively, while the porosity, peak chloride content, and erosion depth increased by 45.12%, 70.45%, and 45.00%. Compared with the drying-wetting cycle with a constant temperature, the cumulative damage caused by the drying-wetting cycle with a variable temperature was greater, resulting in more severe deterioration of concrete performance. The increase in the test temperature significantly accelerated the diffusion rate, penetration depth, and chemical binding capacity of chloride ions. After 60 drying-wetting cycles, the peak chlorine content and erosion depth of w/b = 0.46 under variable temperature cycles were 15.38% and 10.32% higher than those under a constant temperature, while the compressive strength, splitting tensile strength, mass, and relative dynamic elastic modulus were reduced by 7.76%, 14.81%, 0.33%, and 2.40%, respectively. Microscopic analysis confirmed that higher w/b and variable temperature cycles accelerated the decay of mechanical properties and the decline of chloride corrosion resistance. According to the numerical fitting analysis, the w/b should be 0.29 similar to 0.39 under the condition that the mechanical properties and chloride corrosion resistance of concrete are met.
引用
收藏
页数:19
相关论文
共 50 条
  • [1] Experimental Studies on Chloride Penetration and Steel Corrosion in Cracked Concrete Beams under Drying-Wetting Cycles
    Lu, Chunhua
    Yang, Jinmu
    Li, Hui
    Liu, Ronggui
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2017, 29 (09)
  • [2] Chloride Penetration of Recycled Fine Aggregate Concrete under Drying-Wetting Cycles
    Chen, Chunhong
    Wang, Lei
    Liu, Ronggui
    Yu, Jiang
    Liu, Hui
    Wu, Jinlong
    MATERIALS, 2023, 16 (03)
  • [3] Chloride transport in concrete subjected to multiple cracks under drying-wetting cycles
    Peng, Jianxin
    Cheng, Xiaokang
    Yang, Yiming
    Xiao, Junyi
    CONSTRUCTION AND BUILDING MATERIALS, 2025, 470
  • [4] Chloride diffusion behavior of coral aggregate concrete under drying-wetting cycles
    Huang, Daguan
    Niu, Ditao
    Su, Li
    Fu, Qiang
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 270
  • [5] Chloride Ingress into Alkali-Activated Concrete Under Drying-Wetting Cycles
    Bao J.
    Zhang X.
    Zhang P.
    Cui Y.
    Wei J.
    Zhuang Z.
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2022, 50 (06): : 1607 - 1615
  • [6] Transport model of chloride ions in concrete under loads and drying-wetting cycles
    Wu, Jin
    Li, Hongming
    Wang, Zhe
    Liu, Jingjing
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 112 : 733 - 738
  • [7] Resistance of concrete against combined attack of chloride and sulfate under drying-wetting cycles
    Chen, Yanjuan
    Gao, Jianming
    Tang, Luping
    Li, Xuehong
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 106 : 650 - 658
  • [8] Water transport in concrete cover under different drying-wetting conditions
    Liu, Peng
    Song, Li
    Yu, Zhiwu
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2014, 45 (08): : 2830 - 2838
  • [9] Experimental Analysis of Chloride Penetration into Concrete Subjected to Drying-Wetting Cycles
    Lu, Chunhua
    Gao, Yuan
    Cui, Zhaowei
    Liu, Ronggui
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2015, 27 (12)
  • [10] Model of chloride penetration into cracked concrete subject to drying-wetting cycles
    Ye, Hailong
    Jin, Nanguo
    Jin, Xianyu
    Fu, Chuanqing
    CONSTRUCTION AND BUILDING MATERIALS, 2012, 36 : 259 - 269