Effect of Ti/N Ratio on TiN Particles, Microstructures, and Toughness of Heat-Affected Zone After High Heat Input Welding of the Ca-Treated Steel Plates

被引:4
作者
Chen, Yanli [1 ]
Yang, Jian [1 ]
Zhang, Yinhui [1 ]
Li, Tingting [1 ]
Zhang, Yuqi [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, State Key Lab Adv Special Steel, Shanghai 200444, Peoples R China
基金
中国国家自然科学基金;
关键词
Ca-treated steel; heat affected zone; Ti/N ratio; TiN particles; AUSTENITE GRAIN-GROWTH; IMPACT TOUGHNESS; STATIC RECRYSTALLIZATION; NITROGEN-CONTENT; INCLUSIONS; PRECIPITATION; KINETICS; HAZ;
D O I
10.1002/srin.202400038
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The high heat input welding (HHIW) can greatly enhance the welding efficiency of the steel plates. However, coarse grains and brittle microstructures will be formed in the heat-affected zone (HAZ) during the HHIW process, which deteriorates the toughness of HAZ. In the present study, the effect of the Ti/N ratio on the size and distribution of titanium nitride (TiN) particles, microstructures, and toughness of HAZ after HHIW of 400 kJ cm-1 is investigated for the Ca-treated steels with different Ti/N ratios of 1.61, 3.79, and 5.00 for TN16, TN38, and TN50 steels. The TN38 steel has the highest number density of the TiN particles with the sizes between 20 and 25 nm and the highest pinning force of the particles in three steels, resulting the smallest grain sizes in its HAZ. In addition, in three steels, the TN38 steel has the main microstructure of intragranular aciculate ferrites with the highest high-angle grain boundaries density in its HAZ, thereby obtaining the highest value of low-temperature impact toughness of the HAZ. The effect of the Ti/N ratio on particles, microstructures, and toughness of the heat-affected zone after high heat input welding of 400 kJ cm-1 is investigated for Ca-treated steels with different Ti/N ratios. The steel with a Ti/N ratio of 3.79 exhibits the highest low-temperature impact toughness value in the heat-affected zone.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:13
相关论文
共 50 条
[21]   Inclusions and microstructures in coarse-grained heat-affected zone of Al-Ti-Ca deoxidized shipbuilding steels with different Al contents after high-heat input welding [J].
Li, Tingting ;
Yang, Jian ;
Zhang, Yinhui ;
Zhang, Yuqi ;
Chen, Yanli ;
Xu, Longyun ;
Li, Rongbin .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 :174-186
[22]   Effect of Heat Input During Welding on the Microstructure and Mechanical Properties of the Heat-Affected Zone of MIL-A-46100 Armour Steel [J].
Slyvins'kyy, O. A. ;
Kvasnyts'kyy, V. V. ;
Vladymyrskyi, I. A. ;
Bisyk, S. P. ;
Chvertko, Ye. P. ;
Kovalenko, V. L. .
METALLOPHYSICS AND ADVANCED TECHNOLOGIES, 2024, 46 (07) :663-677
[23]   Deterioration mechanism of impact toughness in the coarse-grained heat-affected zone of Ca-treated shipbuilding steel plate with high-Cr content [J].
Li, Tingting ;
Yang, Jian ;
Zhang, Yinhui ;
Sun, Han ;
Hu, Pengfei ;
Xu, Longyun .
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1024
[24]   Analysis of heat-affected zone microstructures of steel P92 after welding and after post-weld heat treatment [J].
Marko Dunđer ;
Tomaž Vuherer ;
Ivan Samardžić ;
Dejan Marić .
The International Journal of Advanced Manufacturing Technology, 2019, 102 :3801-3812
[25]   Effect of Heat Input on Impact Toughness of Coarse-grained Heat-affected Zone of a Nb-Ti Microalloyed Pipeline Steel [J].
Gao, Zhou ;
Wei, Ran ;
Wu, Kaiming .
MATERIALS PROCESSING TECHNOLOGY II, PTS 1-4, 2012, 538-541 :2026-2031
[26]   Effect of Ti/N Ratio on the Phase Transformation, Secondary Cracks, and Low-Temperature Toughness in Heat-Affected Zone of Shipbuilding Steel Plates with Mg Deoxidation [J].
Zhang, Yuqi ;
Zhang, Yinhui ;
Yang, Jian ;
Li, Tingting ;
Chen, Yanli ;
Wang, Liang .
JOM, 2025, 77 (02) :872-883
[27]   Enhancement of Heat-Affected Zone Toughness of a Low Carbon Steel by TiN Particle [J].
Yu Zhang ;
Xiaobao Li ;
Han Ma .
Metallurgical and Materials Transactions B, 2016, 47 :2148-2156
[28]   Effect of Mg addition on formation of intragranular acicular ferrite in heat-affected zone of steel plate after high-heat-input welding [J].
Xu, Long-yun ;
Yang, Jian ;
Wang, Rui-zhi ;
Wang, Wan-lin ;
Wang, Yu-nan .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2018, 25 (04) :433-441
[29]   Effect of Mg addition on formation of intragranular acicular ferrite in heat-affected zone of steel plate after high-heat-input welding [J].
Long-yun Xu ;
Jian Yang ;
Rui-zhi Wang ;
Wan-lin Wang ;
Yu-nan Wang .
Journal of Iron and Steel Research International, 2018, 25 :433-441
[30]   Micromechanism of Decrease of Impact Toughness in Coarse-Grain Heat-Affected Zone of HSLA Steel with Increasing Welding Heat Input [J].
R. Cao ;
J. Li ;
D. S. Liu ;
J. Y. Ma ;
J. H. Chen .
Metallurgical and Materials Transactions A, 2015, 46 :2999-3014