Galvanic corrosion behavior of micro-arc oxidation coated Al-Zn-Mg-Cu alloy coupled with 316 L stainless steel in the salt-spray atmosphere

被引:0
作者
Peng, Yiwen [1 ]
Zhao, Junwen [1 ]
Deng, Xiyue
Huang, Xingmin [1 ]
Han, Jing [1 ]
Zheng, Yunzhi [2 ]
机构
[1] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Key Lab Adv Technol Mat, Minist Educ, Chengdu 610031, Peoples R China
[2] Shandong Adv Aluminum Community Management & Opera, Binzhou 256603, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 39卷
关键词
Galvanic corrosion; Micro-arc oxidation (MAO); Al-Zn-Mg-Cu alloy; Stainless steel; EIS; ALUMINUM-ALLOY; MAGNESIUM ALLOYS; PLASMA; MICROSTRUCTURE; PEO; PERFORMANCE; COATINGS; LAYERS; DEPOSITION; RESISTANCE;
D O I
10.1016/j.mtcomm.2024.108864
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Micro -arc oxidation (MAO) coating with thickness, potential, current density, and impedance of 30 mu m, -0.62 V, 7.2x10 -8 A/cm 2 and 88,730 Omega & sdot; cm 2 was prepared on the surface of Al-Zn-Mg-Cu alloy to inhibit galvanic corrosion caused by its coupling with 316 L stainless steel. It was found that the MAO coating increased the potential of the galvanic corrosion zone (GCZ) from -0.67 V to -0.43 V, and decreased its current density from 3x10 -3 A/cm 2 to 4.4x10 -7 A/cm 2 , resulted in a much lower corrosion rate and longer failure time. Salt -spray erosion can cause the MAO coating to detach gradually and formed the stepped corrosion pits at the GCZ. The galvanic corrosion process of the MAO coated 7085 alloy could be divided into three stages: (1) the electrolyte passes through the interconnected defects in the coating, leading to pitting corrosion beneath the coating; (2) the corrosion products block the interconnected defect channels in the coating, reducing the rate of galvanic corrosion; (3) the Al alloy substrate becomes fully exposed and contacts with 316 L stainless steel through the electrolyte, accelerating the galvanic corrosion and corrosion detachment. These findings confirm the effectiveness of MAO coatings in inhibiting galvanic corrosion and clarify the complex corrosion mechanisms involved, providing valuable insights for enhancing the durability of Al-Zn-Mg-Cu alloy in coupled environments.
引用
收藏
页数:12
相关论文
共 41 条
  • [1] The effect of MAO processing time on surface properties and low temperature infrared emissivity of ceramic coating on aluminium 6061 alloy
    Al Bosta, Mohannad M. S.
    Ma, Keng-Jeng
    Chien, Hsi-Hsin
    [J]. INFRARED PHYSICS & TECHNOLOGY, 2013, 60 : 323 - 334
  • [2] Corrosion, erosion and erosion-corrosion performance of plasma electrolytic oxidation (PEO) deposited Al2O3 coatings
    Barik, RC
    Wharton, JA
    Wood, RJK
    Stokes, KR
    Jones, RL
    [J]. SURFACE & COATINGS TECHNOLOGY, 2005, 199 (2-3) : 158 - 167
  • [3] Surface Modification of 6xxx Series Aluminum Alloys
    Bhat, Kuruveri Udaya
    Panemangalore, Devadas Bhat
    Kuruveri, Spandana Bhat
    John, Merbin
    Menezes, Pradeep L.
    [J]. COATINGS, 2022, 12 (02)
  • [4] A method of atmospheric corrosion prediction for aircraft structure
    Chen, Yueliang
    Huang, Hailiang
    Zhang, Yong
    Wang, Chenguang
    Fan, Weijie
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (01): : 79 - 90
  • [5] The effects of anion deposition and negative pulse on the behaviours of plasma electrolytic oxidation (PEO)-A systematic study of the PEO of a Zirlo alloy in aluminate electrolytes
    Cheng, Yingliang
    Wang, Ting
    Li, Shaoxian
    Cheng, Yulin
    Cao, Jinhui
    Xie, Huanjun
    [J]. ELECTROCHIMICA ACTA, 2017, 225 : 47 - 68
  • [6] Effects of Cu content in Al-Cu alloys on microstructure, adhesive strength, and corrosion resistance of thick micro-arc oxidation coatings
    Dai, Weibing
    Zhang, Ce
    Zhao, Lijuan
    Li, Changyou
    [J]. MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [7] Corrosion characteristics of Al alloy/galvanized-steel Couple in NaCl solution
    Du, Pin
    Li, Jianzhong
    Zhao, Yanliang
    Dai, Yigang
    Yang, Zhongdong
    Tian, Yanwen
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2018, 13 (11): : 11164 - 11179
  • [8] Scatter and size effect in High Cycle Fatigue of cast aluminum-silicon alloys: A comprehensive experimental investigation
    El Khoukhi, Driss
    Morel, Franck
    Saintier, Nicolas
    Bellett, Daniel
    Osmond, Pierre
    Viet-Duc Le
    Adrien, Jerome
    [J]. 9TH EDITION OF THE INTERNATIONAL CONFERENCE ON FATIGUE DESIGN, FATIGUE DESIGN 2021, 2022, 38 : 611 - 620
  • [9] Effect of naturally formed oxide films and other variables in the early stages of Mg-alloy corrosion in NaCl solution
    Feliu, Sebastian, Jr.
    Maffiotte, C.
    Samaniego, Alejandro
    Carlos Galvan, Juan
    Barranco, Violeta
    [J]. ELECTROCHIMICA ACTA, 2011, 56 (12) : 4554 - 4565
  • [10] The role of corrosion product deposition in galvanic corrosion of aluminum/carbon systems
    Hakansson, Eva
    Hoffman, Joseph
    Predecki, Paul
    Kumosa, Maciej
    [J]. CORROSION SCIENCE, 2017, 114 : 10 - 16