Effect of the application of surface treatments before and after sintering on the flexural strength, phase transformation and surface topography of zirconia

被引:23
作者
Kurtulmus-Yilmaz, Sevcan [1 ]
Aktore, Huseyin [1 ]
机构
[1] Near East Univ, Fac Dent, Dept Prosthodont, Mersin10, Lefkosa, Turkey
关键词
Er; Cr:YSGG laser; Airborne-particle abrasion; Pre-sintered zirconia; XRD analysis; FE-SEM analysis; SHEAR BOND STRENGTH; Y-TZP ZIRCONIA; PARTIALLY-STABILIZED ZIRCONIA; AIRBORNE-PARTICLE ABRASION; MECHANICAL-PROPERTIES; HEAT-TREATMENT; CERAMICS; LASER; CORE; ROUGHNESS;
D O I
10.1016/j.jdent.2018.02.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To evaluate the effects of airborne-particle abrasion (APA) and Er, Cr:YSGG laser irradiation on 4-point-flexural strength, phase transformation and morphologic changes of zirconia ceramics treated at pre-sintered or post-sintered stage. Methods: Three hundred and forty-two bar shaped zirconia specimens were milled with different sizes according to the flexural strength test (n = 10), X-ray diffraction (XRD) (n = 4) and field emission scanning electron microscope (FE-SEM) (n = 4) analyses. For each test protocol, specimens were divided into 4 main groups whether the surface treatments applied before or after sintering and whether the specimens received heat treatment or not as pre-sintered, post-sintered no-heat and post-sintered heat-treated groups, and a group was served as control. Main groups were further divided into 6 equal subgroups according to surface treatment method applied (2 W-, 3 W-, 4 W-, 5 W-, 6 W- laser irradiations and APA). Surface treatments were applied to pre-sintered groups before sintering and to post-sintered groups after sintering. Post-sintered heat-treated groups were subjected to veneer ceramic firing simulation after surface treatments. Flexural strength and flexural modulus values were statistically analysed and monoclinic phase content was calculated. Weibull analysis was used to evaluate strength reliability and fractographic analysis was conducted. Results: Highest flexural strength values were detected at post-sintered no-heat APA and 4W-laser groups (P < 0.05). Pre-sintered groups showed statistically lower flexural strength values. Heat treatment decreased the strength of the specimens. Monoclinic phase content was only detected at post-sintered no-heat groups and the highest amount was detected at APA group. Rougher surfaces and deeper irregularities were detected at FE-SEM images pre-sintered groups. Conclusions: Application of surface treatments at pre-sintered stage may be detrimental for zirconia ceramics in terms of flexural strength. Clinical significance: Treating the surface of zirconia ceramic before sintering process is not recommended due to significant decrease in flexural strength values. 2 W-4 W Er, Cr: YSGG laser irradiations can be regarded as alternative surface treatment methods when zirconia restoration would be subjected to veneer ceramic firing procedures.
引用
收藏
页码:29 / 38
页数:10
相关论文
共 50 条
[41]   The Shear Bond Strength of Resin-Based Luting Cement to Zirconia Ceramics after Different Surface Treatments [J].
Sokolowski, Grzegorz ;
Szczesio-Wlodarczyk, Agata ;
Szynkowska-Jozwik, Malgorzata Iwona ;
Stopa, Wioleta ;
Sokolowski, Jerzy ;
Kopacz, Karolina ;
Bociong, Kinga .
MATERIALS, 2023, 16 (15)
[42]   Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia [J].
Mohammadi-Bassir, Mahshid ;
Babasafari, Mansoure ;
Rezvani, Mohammad Bagher ;
Jamshidian, Mandieh .
JOURNAL OF PROSTHETIC DENTISTRY, 2017, 118 (05) :658-665
[43]   Mechanical properties of zirconia after different surface treatments and repeated firings [J].
Subasi, Meryem Gulce ;
Demir, Necla ;
Kara, Ozlem ;
Ozturk, A. Nilgun ;
Ozel, Faruk .
JOURNAL OF ADVANCED PROSTHODONTICS, 2014, 6 (06) :462-467
[44]   Investigation of Fracture Resistance of Zirconia Restorations After Different Surface Treatments [J].
Akar, Turker ;
Akin, Hakan .
CLINICAL AND EXPERIMENTAL HEALTH SCIENCES, 2021, 11 (02) :318-321
[45]   Influence of enzymatic and chemical degradation on zirconia resin bond strength after different surface treatments [J].
Mirmohammadi, Hesam ;
Aboushelib, Mostafa N. ;
Salameh, Ziad ;
Kleverlaan, Cornelis J. ;
Feilzer, Albert J. .
AMERICAN JOURNAL OF DENTISTRY, 2010, 23 (06) :327-330
[46]   Effect of Different Surface Treatments on Bond Strength of Resin Cement to a CAD/CAM Restorative Material [J].
Barutcigil, Kubilay ;
Barutcigil, Cagatay ;
Kul, Esra ;
Ozarslan, Mehmet Mustafa ;
Buyukkaplan, Ulviye Sebnem .
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (01) :71-78
[47]   Surface Roughness and Bond Strength of Zirconia Posts to a Resin Cement After Various Surface Pretreatments [J].
Akin, Gulsah E. ;
Kaval, Mehmet Emin ;
Turk, Tugba ;
Akin, Hakan .
PHOTOMEDICINE AND LASER SURGERY, 2015, 33 (05) :246-251
[48]   Evaluation of surface treatments of monolithic zirconia in different sintering stages [J].
Ebeid, Kamal ;
Wille, Sebastian ;
Salah, Tarek ;
Wahsh, Marwa ;
Zohdy, Maged ;
Kern, Matthias .
JOURNAL OF PROSTHODONTIC RESEARCH, 2018, 62 (02) :210-217
[49]   Nd:YAG Laser Treatment to Bioglass-coated Zirconia Surface and Its Effect on Bond Strength and Phase Transformation [J].
Soltaninejad, Fatemeh ;
Valian, Azam ;
Moezizadeh, Maryam ;
Khatiri, Mahdieh ;
Razaghi, Hossein ;
Nojehdehian, Hanieh .
JOURNAL OF ADHESIVE DENTISTRY, 2018, 20 (05) :379-387
[50]   Effect of sintering speed, aging processes, and different surface treatments on the optical and surface properties of monolithic zirconia restorations [J].
Hafezeqoran, Ali ;
Sabanik, Pouya ;
Koodaryan, Roodabeh ;
Ghalili, Kambiz M. .
JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (06) :917-926