Effect of laser shock peening on stress corrosion cracking of TC4/2A14 dissimilar metal friction stir welding joints

被引:25
作者
Gong, Ziying [1 ]
Zhang, Timing [1 ]
Chen, Yuhua [1 ]
Lu, Jinzhong [2 ]
Ding, Xiangyu [3 ]
Zhang, Shiyi [1 ]
Lan, Ming [1 ]
Shen, Yang [1 ]
Wang, Shanlin [1 ]
机构
[1] Nanchang Hangkong Univ, Sch Aeronaut Mfg Engn, Nanchang 330063, Peoples R China
[2] Jiangsu Univ, Sch Mech Engn, Zhenjiang 212013, Peoples R China
[3] Nanchang Hangkong Univ, Sch Aerosp Mfg Engn, Nanchang 330063, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
基金
中国国家自然科学基金;
关键词
Laser shock peening; Friction stir welding; Microstructure; Residual stress; Stress corrosion cracking; VECTOR FUNCTIONAL-LINK; ALLOY; BEHAVIOR; RESISTANCE; FATIGUE; SCC;
D O I
10.1016/j.jmrt.2024.03.216
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stress corrosion cracking (SCC) of welded joints is a significant issue that affects the widespread application of multimetal welded structures in aerospace, transportation, and other fields. This paper investigates the effect of laser shock peening (LSP) on the SCC of TC4/2A14 friction stir welded (FSW) joints with dissimilar metals. The microstructural evolution, mechanical properties, and corrosion behavior with and without LSP treatment were investigated using optical microscopy, transmission electron microscopy, X-ray analysis, electrochemical testing, and slow strain rate tensile testing (SSRT). The results showed that the LSP significantly refined the grains and induced work-hardening on the near-surface of the material. After LSP, the compressive residual stresses on the surface of the titanium and aluminium sides were -817.6 MPa and -153.6 MPa for the joint, respectively. Corrosion resistance was also improved, with the self-corrosion current density on the Al side of the joints reduced by 77% and the SCC susceptibility index ( I ssrt ) reduced from 0.140 to 0.121. The enhanced SCC resistance of the LSP-treated TC4/2A14 dissimilar metal FSW joints is primarily due to grain refinement, workhardening effect, and high-level compressive residual stress. These factors not only enhance the material strength and improve the pitting resistance of the joints but also prevent the initiation and propagation of SCC.
引用
收藏
页码:1716 / 1725
页数:10
相关论文
共 50 条
  • [31] Effect of the Surface State of Steel on the Microstructure and Mechanical Properties of Dissimilar Metal Lap Joints of Aluminum and Steel by Friction Stir Welding
    Y.C. Chen
    K. Nakata
    Metallurgical and Materials Transactions A, 2008, 39 : 1985 - 1992
  • [32] Stress corrosion crack sensitivity of ultra-thick TC4 titanium alloy electron beam welding joints
    Fang W.
    Xiao T.
    Zhang Y.
    Xu W.
    Yi Y.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 121 - 128
  • [33] The effect of laser shock peening on the microstructure and wear resistance of micro-arc oxidation coatings on TC4 alloy
    Luo, Junming
    Tang, Weiqing
    Cui, Shiyu
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 5851 - 5859
  • [34] Impact of friction stir welding parameters and Al2TiO5 reinforcement on the mechanical, wear, and corrosion performance of dissimilar welded aluminium composite joints
    Senthilraj, K.
    Rajamurugan, G.
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2024,
  • [35] Effect of friction stir welding parameters on the material flow, mechanical properties and corrosion behavior of dissimilar AA5083-AA6061 joints
    Kumar, Kethavath Kranthi
    Kumar, Adepu
    Satyanarayana, M. V. N. V.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2022, 236 (06) : 2901 - 2917
  • [36] Effect of Post Weld Heat Treatment on Microstructure and Properties of Linear Friction Welded Joints for Hyperoxic TC4/TC17 Dissimilar Titanium Alloys
    Chang C.
    Li J.
    Zhang T.
    Guo D.
    Cailiao Daobao/Materials Reports, 2021, 35 (10): : 10109 - 10113
  • [37] Interfacial microstructure and corrosion behaviors of TC4/DP780 steel joints by laser welding with H62 interlayer
    Li, Taotao
    Shi, Jiaxing
    Li, Ruifeng
    Qi, Kai
    Liu, Zhenguang
    Zhang, Xiaoqiang
    Qiao, Lei
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 : 4470 - 4479
  • [38] Optimizing the shoulder diameter for double side friction stir welding of medium-thick TC4/AA2024 dissimilar alloys by Taguchi optimization technique
    Chen, Yang
    Li, Yang
    Shi, Lei
    Wu, Chuansong
    Li, Shengli
    Gao, Song
    WELDING IN THE WORLD, 2023, 67 (08) : 1887 - 1899
  • [39] Microstructures of dissimilar friction stir welded joints between 2024-T4 aluminum alloy and Al/Mg2Si metal matrix cast composite
    Sharifitabar, M.
    Nami, H.
    COMPOSITES PART B-ENGINEERING, 2011, 42 (07) : 2004 - 2012
  • [40] Effect of welding parameters on mechanical properties of friction stir welded T-lap dissimilar metal joints between 7075 and 5083 aluminum alloys
    Hao Dinh Duong
    Okazaki, Masakazu
    Tra Hung Tran
    MECHANICAL ENGINEERING JOURNAL, 2019, 6 (04):