Microstructure and mechanical properties of Sc/Zr modified 1460 Al-Li alloy fabricated by laser powder bed fusion

被引:0
作者
Zhang, Siyu [1 ,2 ]
Sun, Chu [3 ]
Fan, Wei [4 ]
Zhang, Qiang [5 ]
Feng, Zhe [1 ,2 ]
Hao, Zhiwei [1 ,2 ]
Tan, Hua [1 ,2 ]
Zhang, Fengying [6 ]
Lin, Xin [1 ,2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Shaanxi, Peoples R China
[2] Northwestern Polytech Univ, Key Lab Met High Performance Addit Mfg & Innovat D, MIIT China, Xian 710072, Shaanxi, Peoples R China
[3] Beijing Inst Aeronaut Mat Co Ltd, Beijing 100094, Peoples R China
[4] Nanyang Technol Univ, Singapore Ctr Printing 3D, Sch Mech & Aerosp Engn, Singapore 639798, Singapore
[5] Suzhou Lab, Suzhou 215123, Jiangsu, Peoples R China
[6] Changan Univ, Sch Mat Sci & Engn, Xian 710064, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 903卷
基金
中国国家自然科学基金;
关键词
Laser powder bed fusion; Al-Li alloy; Microstructure; Crack; Mechanical property; DUCTILITY; EVOLUTION; CRACKING; METALS; TEMPERATURE; KINETICS;
D O I
10.1016/j.msea.2024.146673
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The preparation of Al-Li alloy by laser powder bed fusion (LPBF) technology, especially Al-Li alloy with high Li content, is of great significance for lightweight of aerospace equipment. However, the significant susceptibility of Al-Li alloys to hot cracking during the process limits their advancement. This study starts from the two aspects of process control and composition modification, to achieve the production of crack -free and high -quality 1460 Al-Li alloys. Crack -free 1460 specimens can only be prepared at extremely low scanning velocity. The process window is markedly expanded by Sc/Zr modification. The heterogeneous nucleation of Al3(Li,Sc,Zr) results in significant grain refinement and effectively suppresses crack initiation and propagation. The unique bimodal heterogeneous microstructure endows the alloy with notable mechanical properties. After the addition of 0.6Sc0.3Zr, the ultimate tensile strength (UTS), yield strength (YS), and elongation (delta) of 1460 alloy are increased by 104 %, 158 %, and 43.9 %, respectively. The strength -plasticity synergism is primarily attributed to grain refinement strengthening, precipitation strengthening, and hetero-deformation induced strain hardening resulting from its unique bimodal heterogeneous microstructure. The UTS and YS of 1.2Sc-0.6Zr modified 1460 alloy increased by 156 % and 279 %, respectively. However, this further increase in the Sc/Zr content significantly deteriorates the plasticity of the alloy. This work establishes a foundation for advancing the use of Al-Li alloys in high-performance, lightweight, and complex aerospace structures.
引用
收藏
页数:13
相关论文
共 51 条
  • [1] PRECIPITATION HARDENING
    ARDELL, AJ
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1985, 16 (12): : 2131 - 2165
  • [2] Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting
    Chauvet, Edouard
    Kontis, Paraskevas
    Jaegle, Eric A.
    Gault, Baptiste
    Raabe, Dierk
    Tassin, Catherine
    Blandin, Jean-Jacques
    Dendievel, Remy
    Vayre, Benjamin
    Abed, Stephane
    Martin, Guilhem
    [J]. ACTA MATERIALIA, 2018, 142 : 82 - 94
  • [3] Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting
    Croteau, Joseph R.
    Griffiths, Seth
    Rossell, Marta D.
    Leinenbach, Christian
    Kenel, Christoph
    Jansen, Vincent
    Seidman, David N.
    Dunand, David C.
    Vo, Nhon Q.
    [J]. ACTA MATERIALIA, 2018, 153 : 35 - 44
  • [4] Drezet JM, 2008, HOT CRACKING PHENOMENA IN WELDS II, P19
  • [5] Recent developments in advanced aircraft aluminium alloys
    Dursun, Tolga
    Soutis, Costas
    [J]. MATERIALS & DESIGN, 2014, 56 : 862 - 871
  • [6] Modern Al-Li alloys and prospects of their development
    Elagin, V. I.
    Zakharov, V. V.
    [J]. METAL SCIENCE AND HEAT TREATMENT, 2013, 55 (3-4) : 184 - 190
  • [7] Modeling the evolution of anisotropy in Al-Li alloys: application to Al-Li 2090-T8E41
    Garmestani, H
    Kalidindi, SR
    Williams, L
    Bacaltchuk, CM
    Fountain, C
    Lee, EW
    Es-Said, OS
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 2002, 18 (10) : 1373 - 1393
  • [8] Laser additive manufacturing of metallic components: materials, processes and mechanisms
    Gu, D. D.
    Meiners, W.
    Wissenbach, K.
    Poprawe, R.
    [J]. INTERNATIONAL MATERIALS REVIEWS, 2012, 57 (03) : 133 - 164
  • [9] Microstructure of Al3Sc with ternary transition-metal additions
    Harada, Y
    Dunand, DC
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 329 : 686 - 695
  • [10] Additive manufacturing of metals
    Herzog, Dirk
    Seyda, Vanessa
    Wycisk, Eric
    Emmelmann, Claus
    [J]. ACTA MATERIALIA, 2016, 117 : 371 - 392