Experimental determination of equivalent hydrogen gas pressure from electrochemical hydrogen charging

被引:3
|
作者
Hagen, Anette B. [1 ]
Nyhus, Bard [1 ]
Gerhardt, Michael R. [2 ]
Hagen, Catalina H. Musinoi [1 ]
Stenerud, Gaute [1 ]
Alvaro, Antonio [1 ]
Maincon, Philippe [3 ]
Olden, Vigdis [1 ]
机构
[1] SINTEF Ind, Dept Mat & Nanotechnol, POB 4760, NO-7465 Trondheim, Norway
[2] SINTEF Ind, Dept Sustainable Energy Technol, POB 4760, NO-7465 Trondheim, Norway
[3] SINTEF Ocean, Dept Energy & Transport, POB 4762, N-7465 Trondheim, Norway
关键词
Hydrogen embrittlement; Equivalent hydrogen pressure; Hydrogen diffusion; Electrochemical hydrogen charging; Gaseous hydrogen charging; EMBRITTLEMENT; PERMEATION; DIFFUSION; ENTRY; TRANSPORT; EVOLUTION; SPECIMEN; FUGACITY; METALS; STEELS;
D O I
10.1016/j.ijhydene.2024.02.117
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study describes a novel approach for determining the electrochemical charging conditions corresponding to the hydrogen gas pressures associated with transportation of hydrogen in X65 pipeline steel, using a custommade setup. Electrochemical charging conditions representing cathodic protection at -1050 mV vs. Ag/AgCl are found to be equivalent to a hydrogen pressure of 15-20 bar. Additions of recombination poisons increase the equivalent pressure up to 200 bar, which is the desired pressure for transportation of hydrogen gas in existing pipelines. The results are compared with data from fracture mechanical testing of a X65 steel under equivalent charging conditions, thereby verifying the reliability of the new custom-made setup. The electrochemical production of hydrogen on the outer wall and its diffusion into the sample is simulated with a transient, 1-D diffusion model. The model predicts the evolution of hydrogen pressure, elucidating the impact of varying operational and material parameters, such as increased pressure with more negative potentials and increased time to reach steady state with larger internal volume. The model is validated with experimental pressure measurements.
引用
收藏
页码:1146 / 1156
页数:11
相关论文
共 50 条
  • [31] Determination of Hydrogen Diffusion Parameters of Ferritic Steel from Electrochemical Permeation Measurement under Tensile Loads
    Kim, Sung Jin
    Yun, Dae Won
    Jung, Hwan Gyo
    Kim, Kyoo Young
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2014, 161 (12) : E173 - E181
  • [32] Surface coating with a high resistance to hydrogen entry under high-pressure hydrogen-gas environment
    Yamabe, Junichiro
    Matsuoka, Saburo
    Murakami, Yukitaka
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (24) : 10141 - 10154
  • [33] Effect of electrochemical hydrogen charging on the mechanical property and corrosion behavior of Ti-3Mo alloy
    Pan, Zhimin
    Wei, Ya
    Fu, Yu
    Luo, Hong
    Li, Xiaogang
    CORROSION SCIENCE, 2022, 200
  • [34] Effects of Hydrogen Charging Time and Pressure on the Hydrogen Embrittlement Susceptibility of X52 Pipeline Steel Material
    Wan, Hong-Jiang
    Wu, Xiao-Qi
    Ming, Hong-Liang
    Wang, Jian-Qiu
    Han, En-Hou
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2024, 37 (02) : 293 - 307
  • [35] Effects of Prior Cold Work on Hydrogen Trapping and Diffusion in API X-70 Line Pipe Steel During Electrochemical Charging
    Ha, Hung M.
    Ai, Jia-He
    Scully, John R.
    CORROSION, 2014, 70 (02) : 166 - 184
  • [36] Review and Assessment of the Effect of Hydrogen Gas Pressure on the Embrittlement of Steels in Gaseous Hydrogen Environment
    Michler, Thorsten
    Wackermann, Ken
    Schweizer, Frank
    METALS, 2021, 11 (04)
  • [37] Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures
    Shang, Juan
    Hua, Zhengli
    Xing, Baihui
    Wei, Haotian
    Zheng, Jinyang
    ACTA MATERIALIA, 2023, 259
  • [38] Hydrogen charging of carbon and low alloy steel by electrochemical methods
    Bolzoni, Fabio
    Paterlini, Luca
    Casanova, Luca
    Ormellese, Marco
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2024, 54 (01) : 103 - 114
  • [39] Effect of electrochemical charging on the hydrogen embrittlement susceptibility of a low-alloyed tempered martensitic steel submitted to high internal pressure
    Peral, L. B.
    Diaz, A.
    Colombo, C.
    Alegre, J.
    Cuesta, I. I.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 63 : 657 - 667
  • [40] Effect of deformation and charging conditions on crack and blister formation during electrochemical hydrogen charging
    Laureys, A.
    Van den Eeckhout, E.
    Petrov, R.
    Verbeken, K.
    ACTA MATERIALIA, 2017, 127 : 192 - 202