Surface Enhancement of Titanium-Based Coatings on Commercial Hard Steel Cutting Tools

被引:4
作者
Dang, Minh Nhat [1 ,2 ]
Singh, Surinder [1 ]
King, Hannah J. [1 ]
Navarro-Devia, John H. [3 ]
Le, Hoang [4 ]
Pattison, Thomas G. [1 ]
Hocking, Rosalie K. [1 ]
Wade, Scott A. [1 ]
Stephens, Guy [3 ]
Papageorgiou, Angelo [3 ]
Manzano, Armando [2 ]
Wang, James [1 ]
机构
[1] Swinburne Univ Technol, Sch Engn, Australian Res Council ARC Training Ctr Surface En, POB 218, Hawthorn, Vic 3122, Australia
[2] ANCA Pty Ltd, 25 Gatwick Rd, Bayswater, Vic 3153, Australia
[3] Sutton Tools, 378 Settlement Rd, Thomastown, Vic 3074, Australia
[4] Univ Huddersfield, Sch Comp & Engn, Electron Microscopy & Mat Anal Res Grp, Queensgate, Huddersfield HD13DH, England
关键词
thin film coating; cutting tools; titanium nitride; aluminium nitride; surface finish; high speed steel; PVD; RAMAN-SPECTROSCOPY; THERMAL-STABILITY; PITTING CORROSION; NITRIDE; TIN; DEPOSITION; PERFORMANCE; OXIDATION; HAFNIUM; WEAR;
D O I
10.3390/cryst14050470
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This study investigates the mechanical properties, surface integrity, and chemical configuration of PVD-coated high-speed steel (HSS) cutting tools, with a particular focus on titanium nitride (TiN) and titanium aluminium nitride (TiAlN) coatings. A range of characterisation methodologies were employed to examine the impact of pre-coating surface conditions on the resulting coatings. This impact includes the effects of gas bubble production and unequal distribution of elements, which are two unwanted occurrences. Notwithstanding these difficulties, coatings applied on surfaces that were highly polished exhibited more consistency in their mechanical and elemental characteristics, with a thickness ranging from 2 to 4 mu m. The study of mechanical characteristics confirms a significant increase in hardness, from an initial value of roughly 1000 HV0.5 for untreated tools to 1300 HV0.5 for tools with physical vapour deposition (PVD) coatings. Although PVD coatings produced on an industrial scale might not exceed the quality of coatings manufactured in a laboratory, they do offer substantial enhancements in terms of hardness. This study highlights the significant importance of thorough surface preparation in achieving enhanced coating performance, hence contributing to the efforts to prolong the lifespan of tools and enhance their performance even under demanding operational circumstances.
引用
收藏
页数:14
相关论文
共 61 条
[1]   Raman spectroscopy studies on the thermal stability of TiN, CrN, TiAlN coatings and nanolayered TiN/CrN, TiAlN/CrN multilayer coatings [J].
Barshilia, HC ;
Rajam, KS .
JOURNAL OF MATERIALS RESEARCH, 2004, 19 (11) :3196-3205
[2]   Fracture toughness and structural evolution in the TiAlN system upon annealing [J].
Bartosik, M. ;
Rumeau, C. ;
Hahn, R. ;
Zhang, Z. L. ;
Mayrhofer, P. H. .
SCIENTIFIC REPORTS, 2017, 7
[3]   High-performance coatings for cutting tools [J].
Bobzin, Kirsten .
CIRP JOURNAL OF MANUFACTURING SCIENCE AND TECHNOLOGY, 2017, 18 :1-9
[4]   Solid particle erosion and corrosion resistance performance of nanolayered multilayered Ti/TiN and TiAl/TiAlN coatings deposited on Ti6Al4V substrates [J].
Bonu, Venkataramana ;
Jeevitha, M. ;
Kumar, V. Praveen ;
Srinivas, G. ;
Siju ;
Barshilia, Harish C. .
SURFACE & COATINGS TECHNOLOGY, 2020, 387
[5]   Structure, Mechanical and Tribological Properties of Me-Doped Diamond-Like Carbon (DLC) (Me = Al, Ti, or Nb) Hydrogenated Amorphous Carbon Coatings [J].
Bouabibsa, Imane ;
Lamri, Salim ;
Sanchette, Frederic .
COATINGS, 2018, 8 (10)
[6]   INFLUENCE OF NI, MO, AND CR ON PITTING CORROSION OF STEELS STUDIED BY RAMAN-SPECTROSCOPY [J].
BOUCHERIT, N ;
HUGOTLEGOFF, A ;
JOIRET, S .
CORROSION, 1992, 48 (07) :569-579
[7]  
Carbonari M.J., 2001, Mat. Res, V4, P163, DOI [10.1590/S1516-14392001000300004, DOI 10.1590/S1516-14392001000300004]
[8]   High temperature oxidation and cutting performance of AlCrN, TiVN and multilayered AlCrN/TiVN hard coatings [J].
Chang, Yin-Yu ;
Weng, Shi-Yao ;
Chen, Chun-Hsiao ;
Fu, Fu-Xing .
SURFACE & COATINGS TECHNOLOGY, 2017, 332 :494-503
[9]   Machinability Performance Investigation of TiAlN-, DLC-, and CNT-Coated Tools during Turning of Difficult-to-Cut Materials [J].
Chenrayan, Venkatesh ;
Manivannan, Chandru ;
Shahapurkar, Kiran ;
Krishna, Ankit ;
Tirth, Vineet ;
Algahtani, Ali ;
Alarifi, Ibrahim M. .
JOURNAL OF NANOMATERIALS, 2022, 2022
[10]   Thermal Stablility and Oxidation Resistance of CrAlSiN Nano-structured Coatings Deposited by Lateral Rotating Cathode Arc [J].
Cheong, Jhun Yew ;
Ding, X. Z. ;
Tay, Beng Kang ;
Zeng, X. T. .
ADVANCED PRECISION ENGINEERING, 2010, 447-448 :725-+