Constructing Near-Network Microstructure via Heat Treatment for Synergistic Enhancement of Strength and Toughness in (TiB + TiC + La2O3)/TC4 Composite

被引:0
作者
He, Tiantao [1 ]
Yue, Chunyu [1 ]
Zheng, Bowen [1 ]
Gu, Feng [1 ]
Lin, Xuejian [1 ]
Zuo, Xiaojiao [1 ]
Wang, Yinxiao [1 ]
Huang, Hongjun [1 ]
Yuan, Xiaoguang [1 ]
机构
[1] Shenyang Univ Technol, Sch Mat Sci & Engn, Shenyang 110870, Peoples R China
关键词
(TiB + TiC + La2O3)/TC4 composite; double heat treatment; strengthening and toughening mechanisms; wear behaviour; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; COMPOSITES; TEMPERATURE; ALLOY; BEHAVIOR; ARCHITECTURE;
D O I
10.1007/s11665-024-09597-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To further improve the mechanical properties and wear resistance of 3 vol.% TiB + 3 vol.% TiC + 0.4 vol.% La2O3/TC4 composites, the TMCs were prepared in-situ by melting cast method and then heat treated by different processes. The effects of different heat treatment processes on the microstructure evolution, mechanical properties and tribological properties of composites were comprehensively studied. The results indicated that heat treatment can effectively decrease the size of alpha-Ti and reinforced phase and increase the proportion of HAGBs. After different heat treatment, the grain orientation is more random and the distribution of reinforced phase is more uniform. The compressive strength and toughness are significantly improved, and the strength-toughness synergy is effectively realized (as-cast: 1890 MPa, 17.52%, HT2: 2010 MPa, 20.65%). Compared with as-cast TMCs, the average COF and specific wear rate of TMCs after different heat treatments are decreased to varying degrees. The average COF were 0.343, 0.262, 0.215, 0.236, respectively. The specific wear rates were 2.36 x 10(-7), 2.32 x 10(-7), 2.28 x 10(-7), 2.29 x 10(-7)mm(3)/N mm, respectively. The worn degree of the grinding surface is reduced, and the wear surface has a small amount of spalling and furrows. The wear mechanisms were three-body abrasive wear, slight adhesive wear and oxidative wear. In short, the strengthening and toughening mechanisms are ascribed to the grain refinement, load transfer effect and Zener pinning effect after heat treatment.
引用
收藏
页码:5961 / 5973
页数:13
相关论文
共 47 条
  • [31] Characteristics of interfacial reactions between Ti-6Al-4V alloy and ZrO2 ceramic mold
    Sun, Shi-chen
    Zhao, Er-tuan
    Hu, Chen
    Yu, Jin-rui
    An, Yu-kun
    Guan, Ren-guo
    [J]. CHINA FOUNDRY, 2020, 17 (06) : 409 - 415
  • [32] Reinforcing effect of in situ grown TiB fibers on Ti-22Al-11Nb-4Mo alloy
    Tang, F
    Emura, S
    Hagiwara, M
    [J]. SCRIPTA MATERIALIA, 2000, 43 (06) : 573 - 578
  • [33] The influences of anneal temperature and cooling rate on microstructure and tensile properties of laser deposited Ti-4Al-1.5Mn titanium alloy
    Tian, X. J.
    Zhang, S. Q.
    Wang, H. M.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 608 : 95 - 101
  • [34] Heat Treatment Behaviour of SLM-Built Titanium Matrix Composite: Microstructure and Tribological Performance
    Verma, Pankaj Kumar
    Warghane, Sameer
    Nichul, Unissa
    Mehtani, Hitesh
    Kumar, Pawan
    Hiwarkar, Vijay
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 9586 - 9595
  • [35] Hardness and Oxidation Resistance of In Situ Synthesized Multi-phase (TiB + TiC + Ti5Si3) Hybrid-Reinforced Ti555-Type Titanium Matrix Composites
    Wang, Hao
    Xu, Xiaojing
    Liu, Yangguang
    Wang, Saifu
    Sun, Zhiwei
    Han, Mengnan
    Sha, Shaohui
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (01) : 471 - 482
  • [36] Effect of SiC Content on Hot Corrosion Resistance of TiC and Ti5Si3 Reinforced Ti-Al-Sn-Zr Titanium Matrix Composites
    Wang, Hao
    Xu, Xiaojing
    Liu, Yangguang
    Cai, Chengbin
    Sun, Zhiwei
    Han, Mengnan
    Sha, Shaohui
    Tabie, Vitus Mwinterbo
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (04) : 2439 - 2448
  • [37] Effect of precipitation phase on microstructure and superelasticity of cold-rolled beta titanium alloy during heat treatment
    Wang, Liqiang
    Lu, Weijie
    Qin, Jining
    Zhang, Fan
    Zhang, Di
    [J]. MATERIALS & DESIGN, 2009, 30 (09) : 3873 - 3878
  • [38] High temperature deformation behavior of melt hydrogenated (TiB + TiC)/Ti-6Al-4V composites
    Wang, Xuan
    Wang, Liang
    Luo, LiangShun
    Yan, Hui
    Li, XinZhong
    Chen, RuiRun
    Su, YanQing
    Guo, JingJie
    Fu, HengZhi
    [J]. MATERIALS & DESIGN, 2017, 121 : 335 - 344
  • [39] Microstructure and Mechanical Behavior of Heat-Treated and Thermomechanically Processed TA15 Ti Alloy Composites
    Wu, Huili
    Sun, Zhichao
    Cao, Jing
    Yin, Zhikun
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (02) : 788 - 799
  • [40] A novel heterogeneous network structure titanium matrix composite with a combination of strength and ductility
    Yu, Jiashi
    Zhao, Yongqing
    Zhang, Wei
    Zhao, Qinyang
    Lu, Jinwen
    Huo, Wangtu
    Zhang, Yusheng
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 840