Effect of Hf addition on structural transformation and aging stability of Cu-15Ni-8Sn alloy

被引:1
|
作者
Zhang, Junjia [1 ]
Zheng, Jisen [1 ]
Chen, Xin [1 ]
Liao, Qiyu [1 ]
Wang, Ze [1 ]
Yin, Bingbing [1 ]
Dong, Yong [2 ]
Zou, Cunlei [3 ]
Fu, Ying [4 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Lightweight Struct Mat Liaoning Prov, Shenyang 110819, Peoples R China
[2] Guangdong Univ Technol, Sch Mat & Energy, Guangzhou 510006, Peoples R China
[3] Dalian Jiaotong Univ, Sch Mat Sci & Engn, Dalian 116028, Peoples R China
[4] Songshan Lake Mat Lab, Dongguan 523808, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 899卷
基金
中国国家自然科学基金;
关键词
Cu-15Ni-8Sn alloy; Microstructural evolution; Aging stability; Softening resistance; DISCONTINUOUS PRECIPITATION; CELLULAR PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURES; ELEMENTS; DEPENDENCE; BEHAVIOR; KINETICS; GROWTH; CERIUM;
D O I
10.1016/j.msea.2024.146434
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Cu-15Ni-8Sn-xHf (wt.%, x = 0-0.6) alloys were prepared by vacuum melting, and the effect of Hf on the micro -structure of as -cast, as -solution -treated and as -aged alloys was systematically investigated, as well as the alloy aging stability. The Hf addition provided a significant role on refining the solidification structure and reducing the micro -segregation degree, and it also made gamma- D0 3 phases more likely to form in needlelike-shape rather than lamellar -shape. With the presence of more Hf atoms, their existence form was accordingly changed from solid solute atoms to nano -scale precipitation phases and then to micron -scale segregation phase. A small content of Hf (0.1 wt%) could effectively improve the aging stability by inhibiting the growth of gamma- D0 3 . Once its content reached or exceeded 0.3 wt%, the harmful discontinuous precipitation was completely inhibited, and the common lamellar -shape gamma- D0 3 locating around the grain boundary was no longer formed. Even the alloy failed at higher temperatures, it could only be carried out through the continuous precipitation method, namely the generation of needlelike-shape gamma- D0 3 uniformly in the matrix. The appropriate Hf addition was capable of extending the alloy aging window, and the hardness of Cu-15Ni-8Sn-0.3Hf alloy could still exceed 360 HV even after 48 h aging.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Effects of nanoscale Sn segregation on corrosion behavior of laser powder b e d fusion Cu-15Ni-8Sn alloy
    Zuo, Pengcheng
    Zhang, Zequn
    Qi, Xiaohong
    Liu, Zhuangzhuang
    Xia, Jiuyang
    Wu, Junshen
    Li, Xiaogang
    Zhang, Bowei
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 158 : 96 - 110
  • [42] FEM and machine learning aided modelling of compressive deformation anisotropy in pressure-less sintered Cu-15Ni-8Sn alloy
    Kamal, Tafzeelul
    Gouthama
    Upadhyaya, Anish
    MATERIALIA, 2024, 34
  • [43] Pre-deformation aging strengthening mechanism of Cu-15Ni-8Sn alloys prepared by laser additive manufacturing
    Wang, Jibing
    Zhou, Xianglin
    Li, Jinghao
    Zhang, Mina
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 878
  • [44] Precipitation evolution and properties of Cu-15Ni-8Sn alloys via Al microalloying during ageing
    Luo, Wei
    Peng, Li-Jun
    Mi, Xu-Jun
    Xie, Hao-Feng
    Cao, Yi-Cheng
    Huang, Shu-Hui
    RARE METALS, 2024, 43 (10) : 5216 - 5228
  • [45] Revealing the influential mechanism of electromagnetic vibration on the bulk solidification and the upward continuous casting of Cu-15Ni-8Sn Alloy
    Tang, Ganpei
    Sun, Zhe
    Lin, Zhongze
    Zheng, Tianxiang
    Zhou, Bangfei
    Shi, Peijian
    Li, Qiang
    Liu, Chunmei
    Lu, Haibiao
    Shen, Zhe
    Ding, Biao
    Zhong, Yunbo
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 189 : 166 - 182
  • [46] Modulation of microstructure and properties of Cu-Ni-Sn alloy by addition of trace Ti
    Hu, Ying-lin
    Cheng, Zi-luo
    Li, Xiao-na
    Li, Zhu-min
    Hou, Yuan-di
    Li, Min
    Yang, Mian
    Zheng, Yue-hong
    Dong, Chuang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2024, 34 (12) : 3978 - 3991
  • [47] Evolution of microstructure and mechanical properties during hot forging and heat treatments of Cu-15Ni-8Sn alloy fabricated by hot isostatic pressing
    Hu, Meichen
    Zhang, Xianwei
    Liu, Chaoqiang
    Gan, Xueping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [48] Significantly enhancing the ductility of high-strength Cu-15Ni-8Sn alloy via an optimized combined process of deformation and heat treatment
    Chen, Mingying
    Liu, Xinhua
    Zhao, Fan
    Xiao, Xingyu
    Xie, Jianxin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 914
  • [49] Additive manufacturing of fine-structured copper alloy by selective laser melting of pre-alloyed Cu-15Ni-8Sn powder
    Zhang, Gengming
    Chen, Chao
    Wang, Xiaojun
    Wang, Pengwei
    Zhang, Xiaoyong
    Gan, Xueping
    Zhou, Kechao
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 96 (9-12) : 4223 - 4230
  • [50] Synergistic improvement of ultra-high strength and ductility of Cu-15Ni-8Sn alloy induced by multi-pass rotary swaging and aging treatment
    Zhou, Yanjun
    Jiang, Kaixuan
    Yang, Shaodan
    Yang, Ran
    Yue, Pengfei
    Zhou, Fei
    Yang, Wenhao
    Du, Juan
    Guo, Huiwen
    Peng, Xiaowen
    Yang, Jingzhao
    Song, Kexing
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1012