Effects of Static Strain Aging on Mechanical Performance of Ductile Cast Iron

被引:0
|
作者
Bjorklund, Ville [1 ]
Haenninen, Hannu [1 ]
Bossuyt, Sven [1 ]
机构
[1] Aalto Univ, Dept Mech Engn, Sch Engn, POB 14200, FI-00076 Aalto, Finland
关键词
DIC; ductile cast iron; spent nuclear fuel; strain aging; strain localization; COTTRELL ATMOSPHERE FORMATION; RESIDUAL-STRESS; BEHAVIOR; TENSILE; STEEL; MICROSTRUCTURE; KINETICS; MODEL;
D O I
10.1007/s11665-024-09716-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
EN-GJS-400-15U nodular cast iron intended to be used as load-bearing element in long-term geological disposal canisters containing spent nuclear fuel in Finland and Sweden was studied for static strain aging (SSA). Tensile test specimens manufactured from the nodular cast iron were pre-strained to 1%, 2% and 3% nominal plastic strains. The pre-strained specimens were aged at different temperatures ranging from room temperature to 400 degrees C for varying times. The aged specimens were tested with conventional tensile testing using constant cross-head speed of 0.016 mm/s. Additionally, four specimens were studied with digital image correlation (DIC) during the tensile testing to obtain full-field strain measurements. SSA resulted in elevated pronounced yield point in all the conditions, while the as-received material showed continuous yielding behavior. SSA reduced the elongation to fracture. DIC tests showed more localized yielding behavior in the SSA specimens. Over-aging effect was observed at 400 degrees C where increasing pre-strain did not increase the yield stress more. For 1-day aging time, the highest yield stress increment was found after aging at 200 degrees C. The yield stress of the material was almost identical after aging in 100 degrees C and 200 degrees C.
引用
收藏
页码:10131 / 10148
页数:18
相关论文
共 50 条
  • [21] Effect of Alloying Elements and Technological Parameters of Austempering on the Structure and Mechanical Properties of Ductile Cast Iron (ADI)
    Keles, Ali
    Cengiz, Rabia
    Yildirim, Mehmet
    METAL SCIENCE AND HEAT TREATMENT, 2023, 65 (3-4) : 191 - 199
  • [22] Microstructure and tribological performance of boride layers on ductile cast iron under dry sliding conditions
    Zhang, Dongya
    Li, Yue
    Du, Xin
    Fan, Hongwei
    Gao, Feng
    ENGINEERING FAILURE ANALYSIS, 2022, 134
  • [23] Effect of Dynamic Strain Aging on Isothermal (473 K) Low Cycle Fatigue of Ferritic Ductile Cast Iron
    Mouri, Hayato
    Hayashi, Morihito
    Wunderlich, Wilfried
    MATERIALS TRANSACTIONS, 2009, 50 (08) : 1935 - 1940
  • [24] Ultrasonic and mechanical studies of some properties of ductile cast iron
    Abdel-Fattah, AM
    El-Gazery, M
    Abdel-Kader, H
    ASNT FALL CONFERENCE AND QUALITY TESTING SHOW: PAPER SUMMARIES, 1997, : 70 - 72
  • [25] Formation of Ultrafine Graphite Nodules in Ductile Iron and its Effects on Mechanical Properties
    Liu, Chen
    Du, Yuzhou
    Li, Pengchun
    Wang, Xin
    Sun, Wanting
    You, Caiyin
    Jiang, Bailing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (19) : 10485 - 10494
  • [26] A Study of Effect of Vanadium on Microstructure and Mechanical Properties of As-Cast and Austempered Ductile Iron
    Bakhshinezhad, H.
    Honarbakhshraouf, A.
    Abdollah-Pour, H.
    PHYSICS OF METALS AND METALLOGRAPHY, 2019, 120 (05): : 441 - 446
  • [27] Microstructural and mechanical properties (hardness) investigations of Al-alloyed ductile cast iron
    Shayesteh-Zeraati, A.
    Naser-Zoshki, H.
    Kiani-Rashid, A. R.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 500 (01) : 129 - 133
  • [28] Characterization of boride coatings on a ductile cast iron
    Azouani, Omar
    Keddam, Mourad
    Allaoui, Omar
    Sehisseh, Abdelaziz
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2017, 53 (02) : 306 - 311
  • [29] Effect of spheroidization of cementite in ductile cast iron
    Basavaraj
    Sondar, Pavankumar R.
    Hegde, Subray R.
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2021, 28 (03) : 404 - 411
  • [30] Effects of Tempering Temperature on Mechanical and Tribological Behavior of Ductile Iron
    Hu, Zhitao
    Liu, Chen
    Du, Yuzhou
    Wang, Xin
    Zhu, Xinyu
    Jiang, Bailing
    LUBRICANTS, 2022, 10 (12)