Activity of Chromium Oxide in CaO-SiO2-MgO-Al2O3-MnO-CaF2-CrOx Slag for Chromium Reducing Process

被引:1
作者
Shi, Chonglin [1 ]
Li, Zhi [2 ,3 ]
Liu, Yuxing [1 ]
Kobayashi, Yoshinao [4 ]
机构
[1] Tokyo Inst Technol, Dept Mat Sci & Engn, N1-3,2-12-1 Ookayama,Meguro Ku, Tokyo 1528550, Japan
[2] Tokyo Inst Technol, Dept Mat Sci & Engn, Tokyo, Japan
[3] Toshiba Co Ltd, Battery Div, 8 Shinsugita Cho,Isogo Ku, Yokohama, Kanagawa 2358522, Japan
[4] Tokyo Inst Technol, Inst Innovat Res, Lab Zero Carbon Energy, N1-3,2-12-1 Ookayama,Meguro Ku, Tokyo 1528550, Japan
关键词
activity; chromium oxide; CaO-SiO2-MgO-Al2O3-MnO-CaF2-CrOx slag; stainless steel; reducing process; ELECTRIC FURNACE DUSTS; WASTE TREATMENT-PLANT; STAINLESS-STEEL SLAG; SILICATE-GLASSES; RAMAN-SPECTRA; FILTER CAKE; VISCOSITY; RECOVERY; MELTS; COEFFICIENTS;
D O I
10.2355/isijinternational.ISIJINT-2023-214
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Thermodynamic data of chromium oxide activities in molten slags are important for improvement of the reduction treatment process of chromium oxides in stainless steel slags. The chemical equilibrium experiments were conducted in the present work to measure the activity coefficients of chromium oxides in the CaO-CaF2-MgO-Al2O3-SiO2-MnO-CrOx slags at 1 823 K (1 550 degrees C) under oxygen partial pressure of 2.57x10(-11) atm with different chromium oxides contents. It is found that no solid phase appears in the slag when the initial CrO1.5 mole fraction of the slag is no more than 0.00390 (0.5 mass%), which could ensure the accuracy of the chromium valence analysis. The activity coefficient of CrO keeps almost constant with the increase of mole fraction of total chromium oxides, which indicates that CrO obeys Henry's law under the present conditions. The activity coefficient of CrO1.5 firstly levels off and then rises sharply when the mole fraction of total chromium oxides reaches 0.00198, beyond this point, activity coefficient of CrO1.5 keeps relatively constant again. Through the Raman spectroscopy analysis, the sharp increase of the activity coefficient of CrO1.5 is assumed to be caused by the transformation of CrO1.5 from network former to network modifier.
引用
收藏
页码:893 / 900
页数:8
相关论文
共 41 条
  • [21] MYSEN BO, 1980, AM MINERAL, V65, P690
  • [22] Understanding the Structure and Structural Effects on the Properties of Blast Furnace Slag (BFS)
    Sajid, Muhammad
    Bai, Chenguang
    Aamir, Muhammad
    You, Zhixiong
    Yan, Zhiming
    Lv, Xueming
    [J]. ISIJ INTERNATIONAL, 2019, 59 (07) : 1153 - 1166
  • [23] Sano N., 2004, 10 INT FERROALLOYS C, P670
  • [24] Reduction behavior of chromium oxide in molten slag using aluminum, ferrosilicon and graphite
    Shibata, E
    Egawa, S
    Nakamura, T
    [J]. ISIJ INTERNATIONAL, 2002, 42 (06) : 609 - 613
  • [25] In-situ chromium and vanadium recovery of landfilled ferrochromium and stainless steel slags
    Spooren, Jeroen
    Kim, Eunyoung
    Horckmans, Liesbeth
    Broos, Kris
    Nielsen, Peter
    Quaghebeur, Mieke
    [J]. CHEMICAL ENGINEERING JOURNAL, 2016, 303 : 359 - 368
  • [26] EFFECTS OF TEMPERATURE AND COMPOSITION ON SILICATE GLASS STRUCTURE AND DYNAMICS - SI-29 NMR RESULTS
    STEBBINS, JF
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1988, 106 (1-3) : 359 - 369
  • [27] Stubbe G, 2011, STAHL EISEN, V131, P45
  • [28] Turkdogan E.T., 1980, Physical Chemistry of High Temperature Technology, P10
  • [29] ANIONIC CONSTITUTION OF 1-ATMOSPHERE SILICATE MELTS - IMPLICATIONS FOR THE STRUCTURE OF IGNEOUS MELTS
    VIRGO, D
    MYSEN, BO
    KUSHIRO, I
    [J]. SCIENCE, 1980, 208 (4450) : 1371 - 1373
  • [30] Development of an analytical technique to quantify Cr2+ and Cr3+ in metallurgical slags
    Wang, Hui
    Xiao, Yiwu
    Jiang, Kaixi
    Du Sichen
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2008, 39 (02): : 390 - 393