Microstructure and properties of a HIP manufactured SiC p reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite

被引:4
作者
Yao, Hui [1 ]
Xu, Xiaojing [1 ]
Luo, Yuntian [1 ]
Han, Tian [1 ]
Zhou, Qingshan [1 ]
机构
[1] Jiangsu Univ, Inst Adv Mfg & Modern Equipment Technol, Zhenjiang, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
关键词
Aluminum matrix composites; SiC particles; Microstructure; Mechanical properties; Corrosion properties; MECHANICAL-PROPERTIES; STRENGTHENING MECHANISMS; CORROSION BEHAVIOR; LOCALIZED CORROSION; TENSILE PROPERTIES; HEAT-TREATMENT; DEFORMATION; RESISTANCE; SUSCEPTIBILITY; PARTICLES;
D O I
10.1016/j.jmrt.2024.04.190
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, a hot isostatic pressing (HIP) manufactured SiC particles (SiC p ) reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite was fabricated through ball-milling, HIP, homogenization, hot extrusion, solution treatment, and aging treatment. The results showed the presence of an interfacial reaction layer, MgAl 2 O 4 , around the SiC p , which enhanced the bonding between the particles and the matrix. The aging treatment resulted in the formation of different aging precipitates, which were featured by GP zone for T4, GP zone + eta ' (metastable MgZn 2 ) + eta (stable MgZn 2 ) for T6 and GP zone + eta ' (metastable MgZn 2 ) for T6I4. The composite samples of T4, T6, and T6I4 exhibited different mechanical properties. Specifically, the elastic modulus was measured as 102.9, 103.4, and 102.3 GPa, the yield strength was 685.3, 598.1, and 619.7 MPa, the ultimate tensile strength was 713.6, 618.9, and 633.3 MPa, and the elongation was 2.2%, 1.8%, and 2.8%, respectively. Furthermore, the corrosion behavior of the composite was evaluated through electrochemical, intergranular corrosion, and exfoliation corrosion. The corrosion current density was found to be 3.17 x 10 -7 , 4.97 x 10 -7 , and 3.67 x 10 -7 A cm -2 , the corrosion potential was measured as -0.70, -0.81, and -0.56 V, and the maximum intergranular corrosion depth was 139.9, 167.8, and 106.2 mu m for T4, T6, and T6I4, respectively. The severity of exfoliation corrosion varied, with T4 showing severe pitting, T6 exhibiting moderate pitting, and T6I4 displaying slight pitting. The strengthening mechanism and load transfer strengthening of the composites were discussed in detail based on theoretical calculations, and the anti-corrosion mechanisms were also analyzed.
引用
收藏
页码:4856 / 4867
页数:12
相关论文
共 47 条
  • [21] Effect of Particle Size on Mechanical Properties and Fracture Behaviors of Age-Hardening SiC/Al-Zn-Mg-Cu Composites
    Ma, Guonan
    Wang, Dong
    Xiao, Bolv
    Ma, Zongyi
    [J]. ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 34 (10) : 1447 - 1459
  • [22] Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy
    Ma, Kaka
    Wen, Haiming
    Hu, Tao
    Topping, Troy D.
    Isheim, Dieter
    Seidman, David N.
    Lavernia, Enrique J.
    Schoenung, Julie M.
    [J]. ACTA MATERIALIA, 2014, 62 : 141 - 155
  • [23] Ma WC, 1997, J MATER SCI LETT, V16, P1867, DOI 10.1023/A:1018501709583
  • [24] Effect of heat treatment on microstructure and interface of SiC particle reinforced 2124 Al matrix composite
    Mandal, Durbadal
    Viswanathan, Srinath
    [J]. MATERIALS CHARACTERIZATION, 2013, 85 : 73 - 81
  • [25] Mechanical properties of sintered 7xxx series AI/SiCp composites
    Min, Kyung Ho
    Lee, Baek-Hee
    Chang, Si-Young
    Kim, Young Do
    [J]. MATERIALS LETTERS, 2007, 61 (11-12) : 2544 - 2546
  • [26] The oxidation of SiC particles and its interfacial characteristics in Al-matrix composite
    Shi, ZL
    Ochiai, S
    Hojo, M
    Lee, J
    Gu, MY
    Lee, H
    Wu, RJ
    [J]. JOURNAL OF MATERIALS SCIENCE, 2001, 36 (10) : 2441 - 2449
  • [27] Properties of P/M processed particle reinforced metal matrix composites specified by reinforcement concentration and matrix-to-reinforcement particle size ratio
    Slipenyuk, A
    Kuprin, V
    Milman, Y
    Goncharuk, V
    Eckert, J
    [J]. ACTA MATERIALIA, 2006, 54 (01) : 157 - 166
  • [28] SEGREGATION TO SIC/AL INTERFACES IN AL BASED METAL MATRIX COMPOSITES
    STRANGWOOD, M
    HIPPSLEY, CA
    LEWANDOWSKI, JJ
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (08): : 1483 - 1487
  • [29] Annealing of Al-Zn-Mg-Cu Alloy at High Pressures: Evolution of Microstructure and the Corrosion Behavior
    Suo, Chuanjun
    Ma, Pan
    Jia, Yandong
    Liu, Xiao
    Shi, Xuerong
    Yu, Zhishui
    Prashanth, Konda Gokuldoss
    [J]. MATERIALS, 2021, 14 (08)
  • [30] Pure Al matrix composites produced by vacuum hot pressing: tensile properties and strengthening mechanisms
    Tang, F
    Anderson, IE
    Gnaupel-Herold, T
    Prask, H
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 383 (02): : 362 - 373