Microstructure and properties of a HIP manufactured SiC p reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite

被引:4
作者
Yao, Hui [1 ]
Xu, Xiaojing [1 ]
Luo, Yuntian [1 ]
Han, Tian [1 ]
Zhou, Qingshan [1 ]
机构
[1] Jiangsu Univ, Inst Adv Mfg & Modern Equipment Technol, Zhenjiang, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
关键词
Aluminum matrix composites; SiC particles; Microstructure; Mechanical properties; Corrosion properties; MECHANICAL-PROPERTIES; STRENGTHENING MECHANISMS; CORROSION BEHAVIOR; LOCALIZED CORROSION; TENSILE PROPERTIES; HEAT-TREATMENT; DEFORMATION; RESISTANCE; SUSCEPTIBILITY; PARTICLES;
D O I
10.1016/j.jmrt.2024.04.190
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, a hot isostatic pressing (HIP) manufactured SiC particles (SiC p ) reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite was fabricated through ball-milling, HIP, homogenization, hot extrusion, solution treatment, and aging treatment. The results showed the presence of an interfacial reaction layer, MgAl 2 O 4 , around the SiC p , which enhanced the bonding between the particles and the matrix. The aging treatment resulted in the formation of different aging precipitates, which were featured by GP zone for T4, GP zone + eta ' (metastable MgZn 2 ) + eta (stable MgZn 2 ) for T6 and GP zone + eta ' (metastable MgZn 2 ) for T6I4. The composite samples of T4, T6, and T6I4 exhibited different mechanical properties. Specifically, the elastic modulus was measured as 102.9, 103.4, and 102.3 GPa, the yield strength was 685.3, 598.1, and 619.7 MPa, the ultimate tensile strength was 713.6, 618.9, and 633.3 MPa, and the elongation was 2.2%, 1.8%, and 2.8%, respectively. Furthermore, the corrosion behavior of the composite was evaluated through electrochemical, intergranular corrosion, and exfoliation corrosion. The corrosion current density was found to be 3.17 x 10 -7 , 4.97 x 10 -7 , and 3.67 x 10 -7 A cm -2 , the corrosion potential was measured as -0.70, -0.81, and -0.56 V, and the maximum intergranular corrosion depth was 139.9, 167.8, and 106.2 mu m for T4, T6, and T6I4, respectively. The severity of exfoliation corrosion varied, with T4 showing severe pitting, T6 exhibiting moderate pitting, and T6I4 displaying slight pitting. The strengthening mechanism and load transfer strengthening of the composites were discussed in detail based on theoretical calculations, and the anti-corrosion mechanisms were also analyzed.
引用
收藏
页码:4856 / 4867
页数:12
相关论文
共 47 条
  • [1] THE DETERMINATION OF PH, POTENTIAL AND CHLORIDE CONCENTRATION IN CORRODING CREVICES ON 304-STAINLESS STEEL AND 7475-ALUMINUM ALLOY
    ALAVI, A
    COTTIS, RA
    [J]. CORROSION SCIENCE, 1987, 27 (05) : 443 - 451
  • [2] Microstructure and mechanical properties of Al-nano/micro SiC composites produced by stir casting technique
    Amouri, K.
    Kazemi, Sh.
    Momeni, A.
    Kazazi, M.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 674 : 569 - 578
  • [3] Development and strengthening mechanisms of bulk ultrafine grained AA6063/SiC composite sheets with varying reinforcement size ranging from nano to micro domain
    Bembalge, O. B.
    Panigrahi, S. K.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 766 : 355 - 372
  • [4] The influence of the surface distribution of Al6(MnFe) intermetallic on the electrochemical response of AA5083 aluminium alloy in NaCl solutions
    Bethencourt, M
    Botana, FJ
    Calvino, JJ
    Marcos, M
    Pérez, J
    Rodríguez, MA
    [J]. ELECTROCHEMICAL METHODS IN CORROSION RESEARCH VI, PTS 1 AND 2, 1998, 289-2 : 567 - 573
  • [5] Electrochemical Performance of SiC Composite Anode in Aluminum-Air Battery
    Bing, Mingcheng
    Mo, Fan
    Hu, Zhengfei
    [J]. ELECTROCHEMISTRY, 2020, 88 (06) : 525 - 531
  • [6] Investigating localized corrosion susceptibility arising from Sc containing intermetallic Al3Sc in high strength Al-alloys
    Cavanaugh, M. K.
    Birbilis, N.
    Buchheit, R. G.
    Bovard, F.
    [J]. SCRIPTA MATERIALIA, 2007, 56 (11) : 995 - 998
  • [7] Preparation, microstructures and deformation behavior of SiCP/6066Al composites produced by PM route
    Chen, N. P.
    Zeng, S. M.
    Liu, Z. Y.
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 202 (1-3) : 27 - 40
  • [8] Effects of Sc and Zr microalloying additions and aging time at 120 °C on the corrosion behaviour of an Al-Zn-Mg alloy
    Deng, Ying
    Yin, Zhimin
    Zhao, Kai
    Duan, Jiaqi
    Hu, Jian
    He, Zhenbo
    [J]. CORROSION SCIENCE, 2012, 65 : 288 - 298
  • [9] SOLUTION HARDENING BY TETRAGONAL DISTORTIONS - APPLICATION TO IRRADIATION HARDENING IN FCC CRYSTALS
    FLEISCHER, RL
    [J]. ACTA METALLURGICA, 1962, 10 (SEP): : 835 - &
  • [10] Influence of trace Ti on the microstructure, age hardening behavior and mechanical properties of an Al-Zn-Mg-Cu-Zr alloy
    Gao, Tong
    Zhang, Yongrui
    Liu, Xiangfa
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 598 : 293 - 298