High Temperature Air and Steam Oxidation and Fireside Corrosion Behavior of 304HCu Stainless Steel: Dichotomous Role of Grain Boundary Engineering

被引:2
|
作者
Sanyal, S. [1 ]
Bhuyan, P. [2 ]
Karthikeyan, R. [3 ]
Alroy, R. [4 ]
Kumar, G. Siva [4 ]
Mandal, S. [2 ]
Kamaraj, M. [1 ]
Seshadri, S. [3 ]
Sarma, V. S. [1 ]
机构
[1] Indian Inst Technol Madras, Dept Met & Mat Engn, Chennai 600036, India
[2] Indian Inst Technol Kharagpur, Dept Met & Mat Engn, Kharagpur 721302, India
[3] Indian Inst Technol Madras, Dept Appl Mech, Chennai 600036, India
[4] Int Adv Res Ctr Powder Met & New Mat ARCI, Ctr Engn Coatings, Hyderabad 500005, India
关键词
304HCu stainless steel; Grain boundary engineering; Oxidation; Fireside corrosion; Grain boundaries; Oxide scale; IRON-CHROMIUM ALLOYS; WATER-VAPOR; INTERGRANULAR CORROSION; MATERIALS TECHNOLOGY; FE-CR; SCALE; OXYGEN; EVOLUTION; 304-STAINLESS-STEEL; ATMOSPHERES;
D O I
10.1007/s11085-024-10252-z
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The 304HCu stainless steel is a candidate material for superheater and reheater tubes in advanced ultra-supercritical power plants due to its excellent creep and oxidation resistance. However, these operating conditions involve exposure to steam at high pressure and temperature on the steam-side and hot coal-ash products on the fireside. In this study, the role of grain boundary character distribution (GBCD) on oxidation and fireside corrosion behavior of 304HCu steel is investigated. The GBCD was modified through grain boundary engineering (GBE) via optimized strain-annealing treatment on the as-received (AR) specimen. The air oxidation, steam oxidation (pressure similar to 243 bar) and fireside corrosion studies were conducted at 973 K for up to 1000 h, in custom-designed setups precisely simulating the operating conditions. Following GBE, the grain size (excluding twins) and coincident site lattice boundary (Sigma <= 29) fraction increased from 21 +/- 1 to 60 +/- 12 mu m and from 62 +/- 4 to 74 +/- 3%, respectively, resulting in disruption of the random high angle grain boundary networks through the introduction of twins. Evaluation of oxidation behavior revealed that the GBE specimens have lower oxidation resistance (i.e., higher weight gain and oxide scale thickness) in both air and steam, while the same specimen displayed improved fireside corrosion resistance (lower percolation depth) as compared to the AR specimen. From a detailed analysis of the oxidation/fireside corrosion products and cross-sectional microstructures of the oxide layers, the above responses could be correlated with the GBCD and grain size, and the possible mechanisms operative during the air/steam oxidation and fireside corrosion are also presented. [GRAPHICS] .
引用
收藏
页码:143 / 168
页数:26
相关论文
共 50 条
  • [41] Improvement of Transpassive Intergranular Corrosion Resistance of 304 Austenitic Stainless Steel by Thermomechanical Processing for Twin-induced Grain Boundary Engineering
    Jin, Wei Zhong
    Kokawa, Hiroyuki
    Wang, Zhan Jie
    Sato, Yutaka S.
    Hara, Nobuyoshi
    ISIJ INTERNATIONAL, 2010, 50 (03) : 476 - 481
  • [42] Corrosion behavior of low energy, high temperature nitrogen ion-implanted AISI 304 stainless steel
    M. Ghoranneviss
    A. Shokouhy
    M. M. Larijani
    S. H. Haji Hosseini
    M. Yari
    A. Anvari
    M. Gholipur Shahraki
    A. H. Sari
    M. R. Hantehzadeh
    Pramana, 2007, 68 : 135 - 140
  • [43] Study on corrosion behavior of type 304 stainless steel with electrochemical impedance spectroscopy in high temperature pure water
    Mabuchi, Katsumi
    Sakai, Masanori
    Ohnaka, Noriyuki
    Zairyo to Kankyo/ Corrosion Engineering, 1994, 43 (01): : 2 - 10
  • [44] Corrosion behavior of low energy, high temperature nitrogen ion-implanted AISI 304 stainless steel
    Ghoranneviss, M.
    Shokouhy, A.
    Larijani, M. M.
    Hosseini, S. H. Haji
    Yari, M.
    Anvari, A.
    Shahraki, M. Gholipur
    Sari, A. H.
    Hantehzadeh, M. R.
    PRAMANA-JOURNAL OF PHYSICS, 2007, 68 (01): : 135 - 140
  • [45] Three-dimensional study of grain boundary engineering effects on intergranular stress corrosion cracking of 316 stainless steel in high temperature water
    Liu, Tingguang
    Xia, Shuang
    Bai, Qin
    Zhou, Bangxin
    Zhang, Lefu
    Lu, Yonghao
    Shoji, Tetsuo
    JOURNAL OF NUCLEAR MATERIALS, 2018, 498 : 290 - 299
  • [46] Influence of pre-deformation, sensitization and oxidation in high temperature water on corrosion resistance of AISI 304 stainless steel
    Lv Jinlong
    Liang Tongxiang
    Luo Hongyun
    NUCLEAR ENGINEERING AND DESIGN, 2016, 309 : 1 - 7
  • [47] EFFECT OF Ni2+ IN OCCLUDED VOLUME ON THE OXIDATION BEHAVIOR OF 304 STAINLESS STEEL IN HIGH TEMPERATURE WATER
    Kuang Wenjun
    Wu Xinqiang
    Han En-Hou
    ACTA METALLURGICA SINICA, 2011, 47 (07) : 927 - 931
  • [48] Isothermal oxidation behavior of the AISI430 stainless steel at high temperature in static air
    Sun, Bin
    Wang, Shouren
    Wang, Yanjun
    Pan, Yongzhi
    EMERGING FOCUS ON ADVANCED MATERIALS, PTS 1 AND 2, 2011, 306-307 : 95 - 99
  • [49] EFFECT OF SEA-WATER ON CORROSION BEHAVIOR OF AUSTENITIC STAINLESS-STEEL (TYPE 304) AT HIGH-TEMPERATURE
    KOTHARI, NC
    JOURNAL OF THE AUSTRALASIAN INSTITUTE OF METALS, 1973, 18 (04): : 161 - 166
  • [50] CERIA COATING EFFECT ON THE HIGH-TEMPERATURE CORROSION BEHAVIOR OF THE CLASSICAL AISI-304 STAINLESS-STEEL
    AGUILAR, G
    COLSON, JC
    LARPIN, JP
    MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1992, 89 (7-8): : 447 - 458