Effect of Inorganic Fillers on Electrical and Mechanical Properties of Ceramizable Silicone Rubber

被引:0
作者
Yang, Mingyuan [1 ]
Qiao, Jingqi [1 ]
Su, Bolin [2 ]
Xiao, Yongjian [1 ]
Kang, Shenglin [1 ]
Li, Yuchen [1 ]
Cao, Hanzhong [1 ]
Tang, Hongchuan [3 ]
Zhao, Xuetong [1 ]
机构
[1] Chongqing Univ, Sch Elect Engn, State Key Lab Power Transmiss Equipment Technol, Chongqing 400044, Peoples R China
[2] Liaoning Tech Univ, Fac Elect & Control Engn, Fuxin 123032, Peoples R China
[3] State Grid Chongqing Elect Power Res Inst, Chongqing 401121, Peoples R China
基金
中国国家自然科学基金;
关键词
ceramizable silicone rubber; inorganic fillers; ceramic samples; fire-resistant cable; electrical and mechanical properties; PERCOLATION; COMPOSITES; PYROLYSIS; HYBRID; MICA;
D O I
10.3390/polym16121695
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Ceramizable silicone rubber (CSR) composed of silicone rubber matrix and inorganic fillers can be transformed into a dense flame-retardant ceramic upon encountering high temperatures or flames. Conventionally, CSR can be sintered into a dense ceramic at temperatures above 1000 degrees C, which is higher than the melting point of a copper conductor used in a power cable. In this study, the vulcanization process and mass ratio of inorganic fillers of CSR were studied to lower its ceramization temperature to 950 degrees C. The electrical and mechanical properties of CSRs and their ceramic bulks were studied with various ratios of wollastonite and muscovite. It was found that the CSR samples could be successfully fabricated using a two-step vulcanization technique (at 120 degrees C and 150 degrees C, respectively). As a high ratio of muscovite filler was introduced into the CSR, the sample presented a high dc electrical resistivity of 6.713 x 1014 Omega<middle dot>cm, and a low dielectric constant of 4.3 and dielectric loss of 0.025 at 50 Hz. After the thermal sintering (at 950 degrees C for 1 h) of the CSR sample with a high ratio of muscovite, the ceramic sample exhibits a dense microstructure without any pores. The ceramic also demonstrates excellent insulating properties, with a volume resistivity of 8.69 x 1011 Omega<middle dot>cm, and a low dielectric loss of 0.01 at 50 Hz. Meanwhile, the three-point bending strength of the ceramic sample reaches a value of 110.03 MPa. This study provides a potential route to fabricate CSR used for fire-resistant cables.
引用
收藏
页数:15
相关论文
共 50 条
[21]   Effect of Inorganic Components on Properties of Ceramizable Phenolic Resin Matrix Composites [J].
He, Dongpei ;
Shi, Minxian ;
Yang, Yuqing ;
Huang, Zhixiong .
6TH ANNUAL INTERNATIONAL CONFERENCE ON MATERIAL SCIENCE AND ENVIRONMENTAL ENGINEERING, 2019, 472
[22]   Preparation, characterization and fire resistance evaluation of a novel ceramizable silicone rubber composite [J].
Yu, Jiangjiang ;
Qu, Linlin ;
Min, Yuanyuan ;
Hong, Ling ;
Chen, Dongliang .
JOURNAL OF APPLIED POLYMER SCIENCE, 2022, 139 (20)
[23]   Effect of hollow glass beads on density and mechanical properties of silicone rubber composites [J].
Quan, Xudong ;
Han, Ruijie ;
Shao, Yuanrui ;
Niu, Kangmin .
JOURNAL OF APPLIED POLYMER SCIENCE, 2021, 138 (07)
[24]   Effects of graded porous structures on the mechanical and electrical properties of Ketjenblack/silicone-rubber composites [J].
Yoshimura, Keijiro ;
Nakano, Kazunori ;
Nishiwaki, Takeshi ;
Iwama, Yuki ;
Murata, Masanobu .
SENSORS AND ACTUATORS A-PHYSICAL, 2021, 332
[25]   Optimisation of the Ceramic Phase for Ceramizable Silicone Rubber Based Composites - microstructural aspect [J].
Pedzich, Zbigniew ;
Bielinski, Dariusz M. ;
Dul, Jan ;
Zarzecka-Napierala, Magdalena .
ADVANCED ENGINEERING CERAMICS AND COMPOSITES, 2011, 484 :226-+
[26]   BORON OXIDE AS A FLUXING AGENT FOR SILICONE RUBBER-BASED CERAMIZABLE COMPOSITES [J].
Anyszka, R. ;
Bielinski, D. M. ;
Pedzich, Z. .
HIGH PERFORMANCE ELASTOMER MATERIALS: AN ENGINEERING APPROACH (ELASTOMERS), 2015, :91-107
[27]   Comparative Properties of HTV Silicone Rubber for Composite Insulators - ATH and Silica Fillers [J].
Ilhan, S. ;
Tuzun, D. ;
Ozdemir, A. .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2021, 28 (02) :414-422
[28]   Effect of Fluorosilicone Rubber on Mechanical Properties, Dielectric Breakdown Strength and Hydrophobicity of Methyl Vinyl Silicone Rubber [J].
Wang, Zhaoyang ;
Lin, Yankai ;
Li, Zhanxu ;
Yang, Yumeng ;
Lin, Jun ;
He, Shaojian .
POLYMERS, 2023, 15 (16)
[29]   Effect of inorganic powder fillers on the polypropylene properties [J].
Stasiek, Andrzej ;
Raszkowska-Kaczor, Aneta ;
Formela, Krzysztof .
PRZEMYSL CHEMICZNY, 2014, 93 (06) :888-892
[30]   SYNERGIC EFFECT OF TWO INORGANIC FILLERS ON THE MECHANICAL AND THERMAL PROPERTIES OF HYBRID POLYPROPYLENE COMPOSITES [J].
Aguilar, Hector ;
Yazdani-Pedram, Mehrdad ;
Toro, Patricio ;
Quijada, Raul ;
Miguel Angel, Lopez-Manchado .
JOURNAL OF THE CHILEAN CHEMICAL SOCIETY, 2014, 59 (02) :2468-2473