Mechanical strength and low-velocity impact behavior of glass fiber reinforced filament wound pipes with different number of layers after hydrothermal aging

被引:0
作者
Akin, Yasin [1 ,3 ]
Kara, Memduh [2 ]
机构
[1] Sakarya Univ Appl Sci, Technol Fac, Dept Mech Engn, Sakarya, Turkiye
[2] Mersin Univ, Engn Fac, Dept Mech Engn, Mersin, Turkiye
[3] Sakarya Univ Appl Sci, Dept Mech Engn, Technol Fac, TR-54050 Serdivan, Sakarya, Turkiye
关键词
Glass fiber; hydrothermal aging; tangential stress; low-velocity impact; damage mechanism; COMPOSITE RING; FAILURE; PREDICTION;
D O I
10.1177/00219983241260881
中图分类号
TB33 [复合材料];
学科分类号
摘要
Composite pipe is preferred over metal and other materials for water supply, liquid chemical transport, and fuel and gas transport. This is because composite pipes are more corrosion resistant, have a high strength/density ratio, high stiffness/density ratio, and more durable than metal pipes. The properties of the composite pipes employed may differ based on the operating environment. Therefore, determining the properties of the composite pipe according to the working environment is extremely important for its lifespan. The thickness of the samples is increased in line with different needs (such as increased strength). Increasing the thickness of samples, especially those exposed to different environmental conditions, and investigating the changes that will occur in the physical and mechanical properties of the samples are another important situation. In this investigation, glass fiber (GFRP) reinforced epoxy composite pipes have been examined, which were manufactured using the filament winding method with different layers [+/- 55 degrees]. To determine their properties in different working environments, the GFRP composite pipes were subjected to hydrothermal aging in pure water at 80 degrees C for several days (7, 14, 21, and 28). The changes in their mechanical properties under working conditions were determined through hoop tensile strength tests and low velocity impact tests applied at different energy levels. The experimental results show that the tangential stress values increased by 10.59% as the number of layers increased. As the aging time increased, the durability of the 6-layer composite pipe decreased by 17.69%. Furthermore, the ability of the aged pipes to withstand damage was evaluated, revealing that the aging process exacerbated the damage within the pipes.
引用
收藏
页码:2111 / 2129
页数:19
相关论文
共 43 条
[1]   Hydrothermal effects on the burst strength of impacted glass fiber/epoxy composite pipes [J].
Ahmad, Hawa ;
Majid, Mohd Shukry Abdul ;
Rojan, Mohd Afendi ;
Mat, Fauziah ;
Dan-Mallam, Yakubu .
MATERIALS TESTING, 2016, 58 (04) :333-336
[2]   Effect of hydrothermal ageing on the thermal and delamination fracture behaviour of CFRP composites [J].
Alessi, Sabina ;
Pitarresi, Giuseppe ;
Spadaro, Giuseppe .
COMPOSITES PART B-ENGINEERING, 2014, 67 :145-153
[3]  
[Anonymous], 2015, STANDARD TEST METHOD
[4]   Hydrothermal ageing of graphene/carbon nanotubes/epoxy hybrid nanocomposites [J].
Arribas, C. ;
Prolongo, M. G. ;
Sanchez-Cabezudo, M. ;
Moriche, R. ;
Prolongo, S. G. .
POLYMER DEGRADATION AND STABILITY, 2019, 170
[5]   Impact response of filament-wound structure with polymeric liner: Experimental and numerical investigation (Part-A) [J].
Azeem, Mohammad ;
Ya, Hamdan H. ;
Alam, Mohammad Azad ;
Muhammad, Masdi ;
Sapuan, Salit M. ;
Kumar, Mukesh ;
Gemi, Lokman ;
Maziz, Ammar ;
Ismail, Ahmad Rasdan ;
Khan, Sanan H. .
RESULTS IN ENGINEERING, 2024, 21
[6]   Damage investigation and assessment due to low-velocity impact on flax/glass hybrid composite plates [J].
Barouni, Antigoni K. ;
Dhakal, Horn N. .
COMPOSITE STRUCTURES, 2019, 226
[7]   Prediction of notched strength for cylindrical composites pipes under tensile loading conditions [J].
Benyahia, H. ;
Tarfaoui, M. ;
El Moumen, A. ;
Ouinas, D. .
COMPOSITES PART B-ENGINEERING, 2018, 150 :104-114
[8]   Fracture toughness (Mode I) characterization of SiO2 nanoparticle filled basalt/epoxy filament wound composite ring with split-disk test method [J].
Demirci, Mehmet Turan ;
Tarakcioglu, Necmettin ;
Avci, Ahmet ;
Akdemir, Ahmet ;
Demirci, Ibrahim .
COMPOSITES PART B-ENGINEERING, 2017, 119 :114-124
[9]   Failure pressure and impact response of glass-epoxy pipes exposed to seawater [J].
Deniz, Mehmet Emin ;
Ozdemir, Okan ;
Ozen, Mustafa ;
Karakuzu, Ramazan .
COMPOSITES PART B-ENGINEERING, 2013, 53 :355-361
[10]   Seawater effect on impact behavior of glass-epoxy composite pipes [J].
Deniz, Mehmet Emin ;
Karakuzu, Ramazan .
COMPOSITES PART B-ENGINEERING, 2012, 43 (03) :1130-1138