Mechanical, vibration damping and acoustics characteristics of hybrid aloe vera /jute/polyester composites

被引:4
作者
Senthilrajan, S. [1 ]
Venkateshwaran, N. [2 ]
Giri, R. [1 ]
Ismail, Sikiru O. [3 ]
Nagarajan, Rajini [4 ]
Krishnan, Kumar [5 ]
Mohammad, Faruq [6 ]
机构
[1] Rajalakshmi Engn Coll, Dept Mech Engn, Chennai 602105, India
[2] Rajalakshmi Engn Coll, Ctr Excellence Digital Mfg, Dept Mech Engn, Chennai 602105, India
[3] Univ Hertfordshire, Ctr Engn Res, Sch Phys Engn & Comp Sci, Dept Engn, Hatfield AL10 9AB, England
[4] Kalasalingam Acad Res & Educ, Dept Mech Engn, Anand Nagar 626126, Krishnankoil, India
[5] INTI Int Univ, Fac Hlth & Life Sci, Nilai 71800, Negeri Sembilan, Malaysia
[6] King Saud Univ, Coll Sci, Dept Chem, POB 2455, Riyadh 11451, Saudi Arabia
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 31卷
关键词
Woven; Jute; Aloe vera; Hybrid; Vibration; Acoustic; Transmission loss; Energy efficiency; SOUND-ABSORPTION PROPERTIES; POLYMER COMPOSITES; NATURAL FIBERS; WOVEN; EPOXY; BEHAVIOR; POLYPROPYLENE; HYBRIDIZATION; TENSILE;
D O I
10.1016/j.jmrt.2024.06.158
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The development of biodegradable hybrid fibre composites is gaining pace in the automotive and construction industries due to their lightweight structural applications, which offer considerable benefits for the environment. In this present investigation, hybrid bio composites were fabricated using a compression molding machine with plain woven jute and aloe vera mats along with polyester resin as the matrix. Six types of hybrid biocomposite laminates were prepared by varying the stacking arrangement of jute and aloe-vera mats to analyse the impact of stacking arrangements on vibration damping and acoustic behaviour of these hybrid bio composites. From the results, it is concluded that the maximum value of natural frequency is obtained from the JJAJ type of composite. i.e., 157, 326, and 370 Hz for Modes I, II, and III respectively, due to good interlacing of fibres in the weft and warp directions. J/J/A/J (AJ3) hybrid bio composite has highest sound absorption coefficient of 0.47 at 3000 Hz, and a better transmission loss i.e 19.84 dB, according to the results of the acoustic research. The comparison of experimental and theoretical analysis was carried out, and found that experimental and theoretical values are closely related to each other.
引用
收藏
页码:2402 / 2413
页数:12
相关论文
共 70 条
[1]  
[Anonymous], 1998, ASTM E1050
[2]  
[Anonymous], 1998, ISO 10534-2
[3]  
ASTM, ASTM D790-03
[4]  
ASTM, ASTM E2611-17
[5]   Experimental investigations into sound transmission loss by different materials at aircraft noise [J].
Bahl, Shashi ;
Bagha, Ashok Kumar ;
Sehgal, Shankar .
MATERIALS TODAY-PROCEEDINGS, 2021, 44 :2048-2053
[6]   Characterization of alkali treated and untreated new cellulosic fiber from Saharan aloe vera cactus leaves [J].
Balaji, A. N. ;
Nagarajan, K. J. .
CARBOHYDRATE POLYMERS, 2017, 174 :200-208
[7]   The Acoustic Characterization of Broom Fibers [J].
Berardi, Umberto ;
Iannace, Gino ;
Di Gabriele, Maria .
JOURNAL OF NATURAL FIBERS, 2017, 14 (06) :858-863
[8]   Effect of nanoclay addition on vibration properties of glass fibre reinforced vinyl ester composites [J].
Chandradass, J. ;
Kumar, M. Ramesh ;
Velmurugan, R. .
MATERIALS LETTERS, 2007, 61 (22) :4385-4388
[9]  
Evran S, 2020, J POLYTECH, V23, P633
[10]   Acoustical and fire-retardant properties of jute composite materials [J].
Fatima, S. ;
Mohanty, A. R. .
APPLIED ACOUSTICS, 2011, 72 (2-3) :108-114