Intrinsic mechanism of Co/Mn elemental manipulation in enhancing the cycling stability of single-crystal ultrahigh-nickel layered cathodes

被引:1
|
作者
Han, Duzhao [1 ]
Chen, Jinniu [1 ]
Li, Weipeng [1 ]
Xie, Liang [1 ]
Yan, Zheng [2 ]
Tang, Zexun [3 ]
Wu, Hao [4 ]
Peng, Jiali [5 ]
Dolotko, Oleksandr [5 ]
Zhao, Yuxin [6 ]
Hua, Weibo [1 ]
Wu, Yuping [7 ]
Tang, Wei [1 ]
机构
[1] Xi An Jiao Tong Univ, Sch Chem Engn & Technol, Xian 710049, Peoples R China
[2] Shanghai Inst Space Power, State Key Lab Space Power Sources Technol, 2965 Dongchuan Rd, Shanghai 200245, Peoples R China
[3] Hunan Inst Engn, Coll Mat & Chem Engn, Xiangtan 411104, Peoples R China
[4] Guangdong Jiana Energy Technol Co Ltd, Guangzhou 511449, Guangdong, Peoples R China
[5] Inst Appl Mat IAM, Karlsruhe Inst Technol KIT, D-76344 Eggenstein Leopoldshafen, Germany
[6] CNPC Tubular Goods Res Inst TGRI, Xian 710077, Peoples R China
[7] Southeast Univ, Sch Energy & Environm, Nanjing 210096, Peoples R China
基金
国家重点研发计划; 中国国家自然科学基金;
关键词
LITHIUM-ION BATTERIES; NI-RICH; PERFORMANCE;
D O I
10.1039/d4ta01437e
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ultrahigh-nickel layers suffer from poor cycling stability. Ultrahigh-nickel single-crystal cathodes with Co/Mn elements doped in the transition metal layer are considered promising to overcome this challenge via effectively mitigating the microcrack issue. However, the intrinsic mechanism by which Co/Mn elements enhance the cycling stability of single-crystal ultrahigh-nickel cathodes, as well as the dominant role of structural evolution and surface side reactions in the cycling fading of single-crystal cathodes, remains unclear. Herein, the single-crystal LiNiO2 (SC-N) with manipulated Co/Mn doping as LiNi0.9Co0.1O2 (SC-NC) and LiNi0.9Mn0.1O2 (SC-NM) oxides are synthesized to reveal the correlation between crystal structural evolution and electrochemical performance. The alleviated intensity and delayed onset potential of H2/H3 phase transition in the SC-NM cathode effectively mitigate the abrupt anisotropic lattice collapse, thereby enhancing the morphology integrity of the particles. Despite a higher cation mixing degree, the excellent structural stability derived from the reversible H2/H3 phase transition also provides favorable kinetics for repeated lithiation/delithiation. As a result, the Co-free SC-NM cathode can exhibit unconventional cycling stability with a capacity retention of 93.8% after 100 cycles at 0.5C between 2.7 and 4.3 V compared to the SC-N and SC-NC cathodes with capacity retention values of 71.7% and 81.1%, respectively under the same condition. This study emphasizes the importance of regulating the crystal structure evolution via Co/Mn manipulation in constructing high-performance single-crystal ultrahigh-nickel layered cathodes. We synthesized single-crystal ultrahigh-nickel layered cathodes with manipulated Co/Mn doping to reveal the correlation between crystal structural evolution and performance. Our study emphasizes the importance of regulating the crystal structure evolution constructing high-performance cathodes.
引用
收藏
页码:13724 / 13732
页数:9
相关论文
共 50 条
  • [31] Probing the thermal degradation mechanism of polycrystalline and single-crystal Li(Ni0.8Co0.1Mn0.1)O2 cathodes from the perspective of oxygen vacancy diffusion
    Wei, Zesen
    Liang, Chen
    Jiang, Lihua
    Sun, Mei
    Cheng, Siyuan
    Wang, Linjun
    Chen, Shiyao
    Fang, Zheng
    Li, Yuxuan
    Zhang, Ningjie
    Peng, Qingkui
    Meng, Xiangdong
    Zhang, Wenhua
    Sun, Jinhua
    Wang, Qingsong
    ENERGY STORAGE MATERIALS, 2023, 56 : 495 - 505
  • [32] Radially Oriented Single-Crystal Primary Nanosheets Enable Ultrahigh Rate and Cycling Properties of LiNi0.8Co0.1Mn0.1O2 Cathode Material for Lithium-Ion Batteries
    Xu, Xing
    Huo, Hua
    Jian, Jiyuan
    Wang, Liguang
    Zhu, He
    Xu, Sheng
    He, Xiaoshu
    Yin, Geping
    Du, Chunyu
    Sun, Xueliang
    ADVANCED ENERGY MATERIALS, 2019, 9 (15)
  • [33] Enhancing the electrochemical performance of single-crystal LiNi0.8Co0.1Mn0.1O2 cathode material by phosphorus doping
    Liu, Zhaofeng
    Zheng, Shuang
    Zhou, Yingke
    Tian, Xiaohui
    CHEMICAL ENGINEERING SCIENCE, 2024, 285
  • [34] Upcycling of Spent LiNi0.33Co0.33Mn0.33O2 to Single-Crystal Ni-Rich Cathodes Using Lean Precursors
    Gao, Hongpeng
    Yan, Qizhang
    Tran, Duc
    Yu, Xiaolu
    Liu, Haodong
    Li, Mingqian
    Li, Weikang
    Wu, Junlin
    Tang, Wei
    Gupta, Varun
    Luo, Jian
    Chen, Zheng
    ACS ENERGY LETTERS, 2023, 8 (10) : 4136 - 4144
  • [35] In situ co-doping strategy for achieving long-term cycle stability of single-crystal Ni-rich cathodes at high voltage
    Zhang, Zhi
    Hong, Bo
    Yi, Maoyi
    Fan, Xinming
    Zhang, Zhian
    Huang, Xiaobing
    Lai, Yanqing
    CHEMICAL ENGINEERING JOURNAL, 2022, 445
  • [36] Enhancing structure and cycling stability of single crystal LiNi0.5Mn1.5O4 cathode via multifunctional MXene surface modification
    Liu, Jingjun
    Yuan, Mingliang
    Li, Zhen
    Wang, Lianghua
    Yan, Junqing
    Peng, Jing
    Ou, Shengwen
    Xu, Jingyue
    JOURNAL OF ENERGY STORAGE, 2024, 76
  • [37] Unveiling the enhancing mechanism of cycling stability of Li1.2Mn0.54Ni0.13Co0.13O2-xFx cathode materials
    Chen Liang
    Panpan Zhang
    Hui Huang
    Chao Gao
    Jun Guo
    Yapeng He
    Ionics, 2023, 29 : 2573 - 2586
  • [38] Unveiling the enhancing mechanism of cycling stability of Li1.2Mn0.54Ni0.13Co0.13O2-xFx cathode materials
    Liang, Chen
    Zhang, Panpan
    Huang, Hui
    Gao, Chao
    Guo, Jun
    He, Yapeng
    IONICS, 2023, 29 (07) : 2573 - 2586
  • [39] Effects of Co/Mn Content Variation on Structural and Electrochemical Properties of Single-Crystal Ni-Rich Layered Oxide Materials for Lithium Ion Batteries
    You, Longzhen
    Wen, Ya
    Chu, Binbin
    Li, Guangxin
    Huang, Ben
    Wu, Jianhua
    Huang, Tao
    Yu, Aishui
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (21) : 24620 - 24635
  • [40] Enhanced rate capability and high-voltage cycling stability of single-crystal nickel-rich cathode by surface anchoring dielectric BaTiO3
    Jin, Feng
    Xue, Xiaoyin
    Zhao, Yin
    Shi, Liyi
    Wang, Zhuyi
    Zhang, Meihong
    Wang, Yi
    Zhu, Jiefang
    Yuan, Shuai
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2022, 619 : 65 - 74