Wear Resistance Evaluation of Self-Fluxing Nickel-Based Coating Deposited on AISI 4340 Steel by Atmospheric Plasma Spray

被引:2
|
作者
Moncao, Francisco C. [1 ]
Caliari, Felipe R. [2 ]
Freitas, Filipe E. [3 ]
Couto, Antonio A. [1 ]
Augusto, Arnaldo [1 ]
Lima, Carlos R. C. [1 ]
Massi, Marcos [1 ]
机构
[1] Univ Prebiteriana Mackenzie, Sch Engn, BR-01302907 Sao Paulo, Brazil
[2] SUNY Stony Brook, Ctr Thermal Spray Res, Stony Brook, NY 11794 USA
[3] Anton Paar Brasil Ltda, BR-04026090 Sao Paulo, Brazil
关键词
atmospheric plasma spray; nickel-based self-fluxing coating; post-process coating remelting; hardness; wear resistance; TEMPERATURE; BEHAVIOR;
D O I
10.3390/met14050532
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Materials with enhanced wear resistance are constantly in high demand. Nickel-based self-fluxing materials deposited by atmospheric plasma spraying (APS) have feasible wear resistance performance. This study aimed to evaluate the results of a nickel-based self-fluxing alloy coating deposited on AISI 4340 steel substrate using APS. Additionally, the temperature at which the remelting process achieved optimal results was investigated. The AISI 4340 steel substrate samples were coated with a self-fluxing NiCrBSiCFe powder by APS. The post-coating remelting process was performed in a controlled atmosphere tube furnace at 900, 1000, and 1100 degrees C. Microstructural analysis was carried out by Scanning Electron Microscopy (SEM) before and after remelting. The estimated porosity of the as-sprayed sample was 3.28%, while the remelted coating sample at 1100 degrees C had only 0.22% porosity. Furthermore, a microhardness measurement was conducted, and the best condition yielded an average value of 750 HV0.5. Tribological tests were performed to evaluate the coefficient of friction and wear rates, revealing that at 1100 degrees C, the as-sprayed coating had a wear rate of 9.16 x 10-5 [mm3/(N*m] and the remelted coating had 4.106 x 10-5 [mm3/(N*m]. The wear-loss volume was determined to be 14.1 mm3 for the as-sprayed coating sample and 3.6 mm3 for the remelted coating at 1100 degrees C.
引用
收藏
页数:14
相关论文
共 44 条
  • [41] Melt pool evolution, microstructure and fracture toughness analysis of nickel-based composite coating deposited by laser-based directed energy deposition on 316L stainless steel
    Li, Wanyang
    Liu, Weiwei
    Ma, Zongyu
    Liu, Huanqiang
    Song, Jianrong
    Li, Tao
    Liu, Shujie
    Zhao, Yue
    Peng, Shitong
    Wang, Fengtao
    Zhang, Hongchao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1020
  • [42] ELEVATION OF THE WEAR RESISTANCE OF LOW-ALLOY STRUCTURAL STEEL BY PLASMA-POWDER SURFACING WITH ALLOYS BASED ON IRON, CHROMIUM, AND NICKEL
    Perepl'otchikov, E. F.
    Vasyliv, Kh. B.
    Vynar, V. A.
    Ryabtsev, I. O.
    Zakiev, V. I.
    MATERIALS SCIENCE, 2018, 54 (03) : 378 - 386
  • [43] Elevation of the Wear Resistance of Low-Alloy Structural Steel by Plasma-Powder Surfacing with Alloys Based on Iron, Chromium, and Nickel
    E. F. Perepl’otchikov
    Kh. B. Vasyliv
    V. A. Vynar
    I. O. Ryabtsev
    V. I. Zakiev
    Materials Science, 2018, 54 : 378 - 386
  • [44] Matrix Composite Coatings Deposited on AISI 4715 Steel by Powder Plasma-Transferred Arc Welding. Part 3. Comparison of the Brittle Fracture Resistance of Wear-Resistant Composite Layers Surfaced Using the PPTAW Method
    Czuprynski, Artur
    Zuk, Marcin
    MATERIALS, 2021, 14 (20)