Low-temperature superplastic deformation mechanism of ultra-fine grain Ti-6Al-4V alloy by friction stir processing

被引:35
作者
Qiang, Fei [1 ]
Xin, Shewei [1 ]
Tu, Xingyang [1 ]
Wang, Huan [1 ]
Guo, Ping [1 ]
Hou, Hongmiao [1 ]
Lian, Zhiwei [1 ]
Zhang, Lei [1 ]
Hou, Wentao [2 ]
机构
[1] Northwest Inst Nonferrous Met Res, 96 Weiyang Rd, Xian 710016, Shaanxi, Peoples R China
[2] Zhejiang Univ Technol, Coll Mech Engn, Hangzhou 310023, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
基金
中国国家自然科学基金;
关键词
Ti-6Al-4V alloy; Ultra-fine grain; Superplastic deformation; Friction stir processing; MICROSTRUCTURE; SHEET;
D O I
10.1016/j.jmrt.2024.05.150
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The ultra-fine grain Ti-6Al-4V alloy sheet was successfully achieved by friction stir processing (FSP). The low- temperature superplastic deformation mechanism of Ti-6Al-4V alloy under the strain rate of 3 x 10-4-4 s- 1 at 600 degrees C was studied by scanning electron microscope, electron backscatter diffraction and superplastic tensile test. It is found that the grain size of Ti-6Al-4V alloy by FSP is refined from 7.48 mu m to 0.82 mu m, and there is no preferential crystallographic orientation of the uniform grain. After FSP, the (3 phase of the base material (BM) in the grain boundary is refined and homogenized. During the superplastic tensile processing, with the increase of strain, the grain is refined continuously, and the alpha ->(3 phase transition is induced by the dislocations pile-up at the (3 grain boundary, and the content of (3 phase increases. The grain near the fracture was refined to 0.35 mu m, and the stress concentration led to the formation of cavities near the (3 phase, which eventually caused the fracture. The dynamic recrystallization in superplastic tensile processing is mainly geometric dynamic recrystallization and discontinuous dynamic recrystallization. The elongation of superplastic tensile (1033%) is 19.7 times higher than that of BM (50%). The order of superplastic deformation mechanism in the low-temperature superplastic deformation of the ultra-fine grain Ti-6Al-4V alloy sheet is as follows: intragranular dislocation slip and diffusion, grain boundary sliding, and phase boundary sliding. Phase boundary sliding is the main deformation mechanism for low-temperature superplastic deformation.
引用
收藏
页码:7413 / 7419
页数:7
相关论文
共 30 条
[11]   Modeling the multiaxial fracture behavior of Ti-6Al-4V alloy sheets at a high temperature using improved damage modeling [J].
Lee, Jinwoo ;
Bong, Hyuk Jong ;
Kim, Daeyong ;
Ha, Jinjin .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 25 :1844-1859
[12]   Ultrafine-grained AZ61 alloy produced by high-pressure torsion: Advent of superplasticity and effect of anisotropy [J].
Masuda, Takahiro ;
Tang, Yongpeng ;
Mohamed, Intan Fadhlina ;
Horita, Zenji .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 879
[13]   Superplastic behavior of a fine-grained Mg-Gd-Y-Ag alloy processed by equal channel angular pressing [J].
Rezaei, A. ;
Mahmudi, R. ;
Loge, R. E. .
JOURNAL OF MAGNESIUM AND ALLOYS, 2023, 11 (10) :3815-3828
[14]   Effects of Working Temperature on Microstructure and Hardness of Ti-6Al-4V Alloy Subjected to Asymmetrical Rolling [J].
Sahoo, Partha Sarathi ;
Mahapatra, Manas Mohan ;
Vundavilli, Pandu Ranga ;
Pandey, Chandan .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (03) :1218-1228
[15]   Correlation between microstructure, tribology and corrosion behaviors of Mg-Al-Zn alloy via creating fine and uniform twins through submerged friction stir processing [J].
Sun, Tao ;
Cao, Fujun ;
Jiang, Jian ;
Hou, Wentao ;
Yang, Zhihui ;
Huang, Guoqiang ;
Shen, Yifu .
MATERIALS CHARACTERIZATION, 2023, 206
[16]   Manufacture-friendly nanostructured metals stabilized by dual-phase honeycomb shell [J].
Wang, Hai ;
Song, Wei ;
Liu, Mingfeng ;
Zhang, Shuyuan ;
Ren, Ling ;
Qiu, Dong ;
Chen, Xing-Qiu ;
Yang, Ke .
NATURE COMMUNICATIONS, 2022, 13 (01)
[17]   Intermetallic compound and martensitic transformation in Ag/Cu co-modified Ti6Al4V alloy [J].
Wang, Yingchen ;
Zhang, Yintao ;
Wang, Liqiang ;
Liu, Jia ;
Tang, Yujin ;
Ma, Xiaoli ;
Lu, Weijie .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 :8940-8954
[18]  
Wen Jing Zhang, 2018, Defect and Diffusion Forum, V385, P189, DOI 10.4028/www.scientific.net/DDF.385.189
[19]   Achieving superior superplasticity from lamellar microstructure of a nugget in a friction-stir-welded Ti-6Al-4V joint [J].
Wu, L. H. ;
Xiao, B. L. ;
Ni, D. R. ;
Ma, Z. Y. ;
Li, X. H. ;
Fu, M. J. ;
Zeng, Y. S. .
SCRIPTA MATERIALIA, 2015, 98 :44-47
[20]   DDRX and CDRX of an as-cast nickel-based superalloy during hot compression at γ′ sub-/super-solvus temperatures [J].
Xie, Bingchao ;
Yu, Hao ;
Sheng, Tao ;
Xiong, Yuhang ;
Ning, Yongquan ;
Fu, M. W. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 803 :16-29